Polymer Property : Charpy Impact, Notched = 2.14 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
dry; ISO 179-1/1eA
Murtfeldt Murylon® A Nylon 66
This material combines the excellent properties of the Murylon® range with additional high tensile and compressive strength, increased wear resistance, and a lower level of moisture absorption than..
Charpy Impact, Notched 0.450 J/cm²

@Temperature -30.0 °C
2.14 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Nilit FRIANYL A63 GV20 Nylon 6.6 for injection molding, 20% glass fiber reinforced
Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
ISO 179/1eA
Nilit FRIANYL A63 W-KV30 Nylon 6.6 for injection molding, 30% glass ball reinforced
Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
DIN 53453
Nilit FRIANYL B63 CV10 Nylon 6.6 for injection molding, 10% carbon fiber reinforced
Nylon 6.6 for injection molding, good conductive and electrostatic properties.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
ISO 179/1eA
Radici Radilon® CST (dry) Copolyamide 6 semiaromatic
Transparent gradeInformation provided by Radici group.
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
ISO 179/1eA
Radici Raditer® B RV 100 Polybutylene Terephthalate with 10% Glass fiber
Raditer® B RV 100 is a glass fiber reinforced thermoplastic polyester based on polybutylene terephthalate. The PBT compounds combine excellent thermal, mechanical, electrical and chemical properti..
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
ISO 179/1eA
Nilit FRIANYL A63 KV25 Nylon 6.6 for injection molding, 25% glass ball reinforced
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact, Notched 0.450 J/cm²

@Temperature -20.0 °C
2.14 ft-lb/in²

@Temperature -4.00 °F
DIN 53453
IRPC Polimaxx Polene 2346S Polypropylene Block Copolymer
CHARACTERISTICS: HIGH STIFFNESS, HIGH FLOW, GOOD IMPACT, HEAT STABILITY CONTAIN ANTISTATIC AND UV STABILIZER ADDITIVEAPPLICATIONS: INJECTION MOLDING FOR ELECTRICAL APPLIANCES, AUTOPARTS
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
LATI Latamid 66 H2 G/25-V0CT4 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Lat..
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
ISO 179
Sumitomo Bakelite North America RX® 630 Fiberglass Reinforced Phenolic
RXÂ 630 is a fiberglass reinforced phenolic molding compound, with good dimensional stability and good strength at elevated temperatures. Information supplied by Sumitomo Bak North America.
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
ISO 179/1eA
Solvay TECHNYL® A 208F PA66, DRY
Description: Unreinforced polyamide PA66, heat stabilized, high fluidity, fast cycling grade, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 208F offers three main advanta..
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
ISO 179/1EA-1993
Solvay Technyl® A 205F Nylon 66, EH0
Unreinforced polyamide 66, high fluidity, fast cycling grade, for injection molding.Technyl A 205F offers two main advantages: excellent filling qualities and UL 94 V2 under 0.4 mm. It is particula..
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
ISO 179
Total PPH 7069 Polypropylene, Homopolymer
ATOFINA Polypropylene PPH 7069 is homopolymer.ApplicationATOFINA Polypropylene PPH 7069 is characterized by medium fluidity for extrusion of continuous filament (CF) and bulk continuous filament (BC..
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
ISO 179/1eA
DuPont Performance Polymers Crastin® S620F20 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S620F20 NC010 is an unreinforced nucleated lubricated medium viscosity polybutylene terephthalate resin for fast injection molding.In..
Charpy Impact, Notched 0.450 J/cm²

@Temperature -40.0 °C
2.14 ft-lb/in²

@Temperature -40.0 °F
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® 70G13HS1L BK031 Nylon 66  (Unverified Data**)
13% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G13HS1L BK031 is a 13% glass fiber reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont ..
Charpy Impact, Notched 0.450 J/cm²

@Temperature -30.0 °C
2.14 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® 103FHS NC010 Nylon 66  (Unverified Data**)
Unreinforced Heat Stabilized Polyamide 66 Zytel 103FHS NC010 is a heat stabilized internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivi..
Charpy Impact, Notched 0.450 J/cm²

@Temperature -40.0 °C
2.14 ft-lb/in²

@Temperature -40.0 °F
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® 70G13HS1L NC010 Nylon 66  (Unverified Data**)
13% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G13HS1L NC010 is a 13% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor..
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
ISO 179/IeA
Addiplast Addinyl A2 V15 Nylon 66, 15% Glass Filled
Glass fiber reinforced, high strengthInformation provided by Addiplast.
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
ISO 179/1eA
BASF Ultradur® S 4090 GM11 5/5% Glass/Mineral Filled PBT
Description: Is a PBT + ASA, injection-molding grades reinforced with 5% glass fiber/mineral, for laminar parts with high demands on dimensional stability and low warpage, e.g. lids, ventilation gri..
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
ISO 179/1eU
DSM Stanyl® TW200F3 (DAM) Nylon 46 15% Glass Reinforced, Heat Stabilized (North America)
Information provided by DSM Engineering Plastics.
Charpy Impact, Notched 0.450 J/cm²

@Temperature -30.0 °C
2.14 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66  (Unverified Data**)
Unreinforced Polyamide 66Zytel 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers