Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO179/3C DIN.53453 |
Omnia Plastica PPS GF40 Polyphenylenesulphide Crystalline polymer based on polyphenylene sulfide with the addition of 40% glass-fibre. Very high rigidity, stiffness and flexural strength. The temperature resistance is very high: up to 240° C. .. |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 W-GV30 Nylon 6.6, std. viscosity for injection molding, 30% glass fiber reinforced Nylon 6.6, std. viscosity for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.800 J/cm² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EX2079X PC (Europe-Africa-Middle East) Lexan* EX2079X polycarbonate resin, MVR (300°C/1.2kg) 3 cm3/10min, high viscosity, branched, extrusion, flame retardant, halogen free per DIN VDE 0472 Part 815, mold release, UV stabilized, translu.. |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO Data, Low Temp |
Americas Styrenics Styron® 482 High Impact Polystyrene
(discontinued **) STYRON® 482 high impact polystyrene resin is a high flow resin typically used in toys. When used unmodified for the manufacture of food contact articles STYRON 482 complies with the US Food, Drug a.. |
|||
Charpy Impact, Notched | 0.800 J/cm² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYform POM C M20 Polyoxymethylene Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO 179 |
Nilit Nilamid B G6 FR C4 30% Glass Fiber Reinforced, Flame Retardant PA6 Description: Nilamid B G6 FR C4 combines excellent mechanical performance with flame retardancy. The halogenated flame retardant system used in this product allows a wide range of colors. This produ.. |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL A63 CV-CU 0550 Nylon 6.6 for injection molding, 5% carbon fiber reinforced, 50% copper filled Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | DIN 53453 |
Nilit FRIANYL B63 GV10 Nylon 6 for injection molding, 10% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO 179 1eA |
Lehmann & Voss LUVOCOM® 1105-7944 PEEK, with PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Emergency running property.High chemical resistance parts, hydrolysis resistance, non flam.. |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | |
LATI Larpeek 50 PEEK Polyetheretherketone (PEEK). Unfilled. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe;.. |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO 179 1eA |
Lehmann & Voss LUVOCOM® 1-3260/schwarz Polyamide 66, with PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | |
LATI Latamid 6 H2 G/30-V0AF PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia .. |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | |
LATI Latilub 87/28-17ST K/15 PC, 15% Carbon Fiber Reinforced, Silicone/PTFE Filled Self-lubricating product based on Polycarbonate (PC). Silicone / PTFE. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat.. |
|||
Charpy Impact, Notched | 0.800 J/cm² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL SE100 PPE+HIPS (Europe-Africa-Middle East) NORYL® SE100 is an unfilled, flame retardant material with a Vicat B/120 of 120°C. It has a UL-94 flammability rating V1 @ 1.47 mm, and is halogen free according to VDE/DIN 472 part 815. |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® A 21T2 V25 PA66, 25% glass fiber, DRY Description: Flame retardant polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Appl.. |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Valox® 310SE0 PBT (Asia Pacific) VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO 179/1eA |
Polyplastics Tepcon M25 Acetal-copolymer (POM), High Viscosity Information provided by PolyPlastics. |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO 179 |
Total PPR 10222 Random Copolymer Polypropylene, Injection Molding Total Petrochemicals PPR 10222 is a nucleated and antistatic random copolymer polypropylene with a melt flow index of 40 g/10min for the injection molding of articles with high transparency and exce.. |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® EBGM-20 HX PA666-GF15 Product description: Grilon EBGM-20 HX black 9992 is a high viscosity, high heat stabilized PA66 + PA6 extrusion blow molding grade with 15% glass fibers. The special features of Grilon EBGM-20 HX b.. |
|||
Charpy Impact, Notched | 0.800 J/cm² @Temperature 30.0 °C |
3.81 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® EBV-2H PA6-GF20 Product description: Grilon EBV-2H is a high viscosity, heat stabilized PA6 extrusion blow molding grade with 20% glass fibers. Grilon EBV-2H has the following important properties: High melt streng.. |
|||
Charpy Impact, Notched | 0.800 J/cm² @Temperature -40.0 °C |
3.81 ft-lb/in² @Temperature -40.0 °F |
ISO 179/1eA |
DuPont Performance Polymers Rynite® 530 BK503 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Polyethylene Terephthalate Rynite 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength stiffness and toughness excellent .. |
|||
Charpy Impact, Notched | 0.800 J/cm² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® RS LC1201 BK040A Nylon 1010
(Unverified Data**) Toughened Renewably Sourced Medium Viscosity Polyamide 1010 Developed for Extrusion Zytel RS LC1201 BK040A is a renewably sourced polyamide 1010 resin containing a minimum of 85% renewably sourced i.. |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO179 |
Beijing Chemical Industry KAIFA® 301-G10F PBT Resin 10% glass fiber reinforced, flame retardant, good flow, low bleedingInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Charpy Impact, Notched | 0.800 J/cm² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
BASF Ultramid® 1503-2 BK ND3007 33% Glass Filled PA66 (Dry) Ultramid 1503-2 BK ND3007 is a 33% glass reinforced, heat stabilized, pigmented black injection molding PA6/6. |
|||
Charpy Impact, Notched | 0.800 J/cm² @Temperature 30.0 °C |
3.81 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® HT1V-4 FWA nat PA6T/6I-GF40 Product description: Grivory HT1V-4 FWA natural is a 40 wt.-% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6.. |
|||
Charpy Impact, Notched | 0.800 J/cm² @Temperature 30.0 °C |
3.81 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® HT1V-4 HY black 9205 PA6T/6I-GF40 Product description: Grivory HT1V-4 HY black 9205 is a 40% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-4 HY bl.. |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |