Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 CV-CM 0830 9005/Z Powder-coatable nylon 6.6 for injection molding, 8% carbon fiber reinforced, 30% ceramic filled Powder-coatable nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL A63 TF20 Nylon 6.6 for injection molding, 20% PTFE lubricated Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.400 - 0.700 J/cm² @Temperature 23.0 °C |
1.90 - 3.33 ft-lb/in² @Temperature 73.4 °F |
Injection and Compression; ISO 179/ 1eA |
Raschig Group EPOXIDUR® 3582 EP Epoxy Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Moldi.. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -40.0 °C |
1.90 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL B63 W-GV15 Nylon 6 for injection molding, 15% glass fiber reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | |
Arkema Group Oroglas® HFI-7 Acrylic
(discontinued **) OROGLAS HFI-7 is a medium impact grade that in addition to the improvement in impact resistance provides superior flow which contribute to reduce the cycle time and improve demolding.Key features :.. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | ISO 179 1eA |
Lehmann & Voss LUVOCOM® 1105-8135/VI PEEK, unreinforced, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | |
LATI Kelon® B H CETG/300 PA 6, Glass/Mineral Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | |
LATI Latiohm 36/07 PD01 G/20 ABS, 20% Glass Fiber Reinforced Semiconductive/dissipative product based on Acrylonitrile-Butadiene-Styrene copolymer (ABS). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInfor.. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics ULTEM 1000R PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0, V2 and 5VA listing. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics ULTEM 2312EPR PEI 30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Valox® 815 PBT (Europe-Africa-Middle East) VALOX 815 is a 15% glass reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housings assemblies, industrial glue guns, appliance housings and handles. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
ISO 179/2C |
SABIC Innovative Plastics Valox® 815F PBT+PET (Europe-Africa-Middle East) PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | ISO 179 |
SIDPEC EGYPTENE® HD 5226 EA HDPE Injection Molding Applications:House waresThin-walled food containersPET bottle base cupInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature 23.0 °C |
1.90 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA |
DSM Stanyl® TS250FK33 PA46-(GF+MF)30 FR 30% Glass/Mineral Reinforced, Flame Retardant, Low Warpage |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature 30.0 °C |
1.90 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® GM-4H PA*-MD40 Product description: Grivory GM-4H natural is a 40 % mineral reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyamide. G.. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Crastin® S610SF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin S610SF is an unreinforced low viscosity polybutylene terephthalate for injection molding. It has hig.. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature 30.0 °C |
1.90 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® L 25 W 20 PA12 Product Description: Grilamid L 25 W 20 is a semi-flexible plasticized high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 20 is UV and heat stabilized. The main features of Grila.. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Orgalloy® RS 66M25 Nylon 66 Alloy, 25% Mineral Filled (Conditioned) RS 66 series, rigid polyamide 66 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional propertie.. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | 1eA; ISO 179 |
Azoty Tarnow™ TARNOFORM 700 POM Easy flowing grade for injection molding of thin-walled parts or in case of long flow path.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | ISO 179 / 1eA |
Asahi Kasei Tenac®-C MT754 Copolymer Acetal Resin 20% Mineral filled, high stiffness, low warp gradeInformation provided by Asahi Kasei Corporation. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
BASF Ultramid® 1003-2 NF2002 PA66 (Conditioned) Ultramid 1003-2 NF2002 is a general purpose, heat stabilized nylon 6/6. |
|||
Charpy Impact, Notched | 0.400 - 3.00 J/cm² | 1.90 - 14.3 ft-lb/in² | Average value: 1.42 J/cm² Grade Count:69 |
Overview of materials for Nylon 46, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values .. |
|||
Charpy Impact, Notched | 0.400 - 0.650 J/cm² | 1.90 - 3.09 ft-lb/in² | Average value: 0.575 J/cm² Grade Count:4 |
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | ISO 179 1eA |
Lehmann & Voss LUVOCOM® 1-0865 Polyamide 66, with aramid reinforcement, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Low warpage.Improved heat resistance.Control disks, cams, sliding elements and other duty parts.. |