Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DSM Stanyl® TS250FK33 PA46-(GF+MF)30 FR

Category Polymer , Thermoplastic , Nylon , Nylon 46 , Nylon 46, Flame Retarded + Glass Fiber Reinforced
Manufacturer DSM Engineering Plastics
Trade Name Stanyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Stanyl® TS250FK33 PA46-(GF+MF)30 FR.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
30% Glass/Mineral Reinforced, Flame Retardant, Low Warpage
Physical Properties Metric English Comments
Density 1.66 g/cc
0.0600 lb/in³
dry; ISO 1183
Moisture Absorption 1.60 %
1.60 %
Sim. To ISO 62
Linear Mold Shrinkage, Flow 0.0080 cm/cm
0.0080 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.017 cm/cm
0.017 in/in
Sim. To ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 120 MPa
17400 psi
dry; ISO 527-1/-2
Elongation at Break 2.0 %
2.0 %
dry; ISO 527-1/-2
Tensile Modulus 8.00 GPa
1160 ksi
dry; ISO 527-1/-2
Flexural Modulus 7.60 GPa
1100 ksi
dry; ISO 178
Charpy Impact, Notched 0.400 J/cm²

@Temperature 23.0 °C
1.90 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
11.1 µin/in-°F
dry; ISO 11359-1/-2
CTE, linear, Transverse to Flow 55.0 µm/m-°C
30.6 µin/in-°F
dry; ISO 11359-1/-2
Melting Point 295 °C
563 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 280 °C
536 °F
dry; ISO 75-1/-2
Flammability, UL94 V-0

@Thickness 0.750 mm
V-0

@Thickness 0.0295 in
dry; IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
dry; IEC 60093
Dielectric Strength 30.0 kV/mm
762 kV/in
dry; IEC 60243-1