Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Strength = 13000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 89.6 MPa
13000 psi
ASTM D790
PolyOne Geon™ Vinyl Rigid Extrusion 87624 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Flexural Strength 89.6 MPa
13000 psi
Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Network Polymers PC-1029
Description: Natural PolycarbonateInformation provided by Network Polymers Inc.
Flexural Strength 89.6 MPa
13000 psi
ASTM D790
Polymer Resources AC-GP2-TFE5 Acetal Copolymer, 5% PTFE
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Flexural Strength 89.6 MPa
13000 psi
ASTM D790
Polymer Resources PPX/NY GP2 PPO/Nylon 66 Alloy, Medium Heat
Polyphenylene Oxide/Nylon 66 Alloy , General Purpose, Medium HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
Flexural Strength 89.6 MPa
13000 psi
ASTM D790
Polymer Resources PPX-EN-FR3 Modified-PPO, V-1 Flame Retardant, Extrusion Grade
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte..
Flexural Strength 89.6 MPa
13000 psi
ASTM D790
Polymer Resources PPX-GP1-[color]EN Modified PPO, Extrusion Grade with HDT of 265 F
Process: Extrusion Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Flexural Strength 89.6 MPa
13000 psi
ASTM D790
Ravago Manufacturing Americas Hylex® P1010FRMA Polycarbonate
Polycarbonate, General Purpose, Flame RetardantInformation provided by Ravago.
Flexural Strength 89.6 MPa
13000 psi
ASTM D790
Ravago Manufacturing Americas Hylex® P1310FRMA Polycarbonate
Polycarbonate, General Purpose, Flame Retardant, UV StabilizedInformation provided by Ravago.
Flexural Strength 89.6 MPa
13000 psi
ASTM D790
Polymer Resources PC-FR1A-D-[color]-3 Polycarbonate, Flame Retardant, Low Flow, UV-stabilized
Polycarbonate, Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Flexural Strength 89.6 MPa
13000 psi
ASTM D790
Polymer Resources PC-FR3A-D-[color]-3 Polycarbonate, Flame Retardant, High Flow, UV-stabilized
Polycarbonate, Flame Retardant, High Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat..
Flexural Strength 89.6 MPa
13000 psi
Parallel to pressing direction
Momentive Performance Materials HBN Hot-Pressed Boron Nitride
Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom..
Flexural Strength 89.6 MPa
13000 psi
ASTM D790
Techmer ES Electrablend® ABS SS5 5% Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 5% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Information provided by TP Composites, Inc.
Flexural Strength 89.6 MPa
13000 psi
ASTM D790
Techmer ES HiFill® HIPS GF30 30% Glass Filled
Availability: North AmericaForms: PelletsGlass Fiber Reinforcement, 30% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc.
Flexural Strength 89.6 MPa
13000 psi
ASTM D790
Techmer ES Luriblend® PA6 TS18 Nylon 6
Availability: North AmericaForms: PelletsAdditive: PTFE+ Silicone Lubricant(18%)Features: LubricatedInformation provided by TP Composites, Inc.
Flexural Strength 89.6 MPa
13000 psi
ASTM D790
Chase Plastics CP Pryme® PC300RUV Polycarbonate (Utility Grade), UV Stabilizer, Mold Release
Information provided by Chase Plastics.
Flexural Strength 89.6 MPa
13000 psi
ASTM D790
Westlake Plastics Pomalux® CN-SS Acetal Copolymer (conductive)
Stainless-steel-fiber-filled, non-sloughing, dimensionally stable material HDT @ 264 psi of 225F. This material has relatively high chemical resistance, is extremely strong and stiff, and is an exc..
Flexural Strength 89.6 MPa
13000 psi
ASTM D790
A. Schulman ComAlloy® E-14756 Flame Retardant Easy Flow Polycarbonate Alloy
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Flexural Strength 89.6 MPa
13000 psi
ASTM D-790
Axiall HR-5009 Rigid PVC, Molding
Georgia Gulf HR-5009 is a rigid, fitting-grade PVC compound designed for hot runner molds, large parts and multi-cavity molds. This compound is characterized by excellent processability, which incl..
Flexural Strength 89.6 MPa
13000 psi
ASTM D-790
Axiall NR-5009 Rigid PVC, Molding
Georgia Gulf NR-5009 is an economical high flow rigid PVC fittings compound designed for multi-cavity molds and large diameter fittings. This compound is characterized by excellent processability, ..
Flexural Strength 89.6 MPa
13000 psi
ASTM D790
Asahi Kasei Thermylene® P6-16FG-0801 16% Fiber Glass Reinforced, UV Stabilized
Information provided by Asahi Thermofil
Flexural Strength 89.6 MPa
13000 psi
ASTM D790
Americas Styrenics STYRON® 685DL High Heat Crystal Polystyrene
Product CharacteristicsHigh heat resistanceHigh tensile strengthBlue tintFood Contact CompliantTypical ApplicationsFoamOPSMedicalInformation provided by AmericasStyrenics LLC.
Flexural Strength 89.6 MPa
13000 psi
ISO 178
BASF Ultramid® B3ZG6 30% Glass Filled PA6 (Conditioned)
Ultramid B3ZG6 is an impact-modified, 30% glass fiber reinforced injection molding PA6 grade for industrial items having very high impact strength and rigidity.
Flexural Strength 89.6 MPa
13000 psi
ASTM D-790
Axiall 3217 Rigid PVC, Extrusion
Georgia Gulf 3217 is a powder blend designed for the extrusion of window, door, fence and marine profiles where weatherability is of primary consideration.Information provided by Georgia GulfGeorgia..
Flexural Strength 89.6 MPa
13000 psi
ASTM D790
Asahi Kasei Thermylene® P-30FG-0812 30% Glass Fiber Reinforced, UV Stabilized
Information provided by Asahi Thermofil
Flexural Strength 89.6 MPa
13000 psi
ASTM D790
Americas Styrenics STYRON® 695 High Heat Crystal Polystyrene
Product CharacteristicsReduced residualsHigh heat resistancehigh strengthFood Contact CompliantTypical ApplicationsOPSInformation provided by AmericasStyrenics LLC.
Copyright © lookpolymers.com All Rights Reserved