Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
SABIC PS 155 General Purpose Polystyrene for Foam Extrusion Product Description: General purpose Polystyrene PS 155 is manufactured by continuous mass polymerization of styrene monomer. It is a crystal-like, hard and brittle polymer with medium flow and go.. |
|||
Flexural Strength | <= 66.0 MPa | <= 9570 psi | ISO 178 |
Polykemi AB POLYabs N00 LG ABS, Low Gloss Information provided by Polykemi AB |
|||
Flexural Strength | <= 66.0 MPa | <= 9570 psi | ISO 178 |
Polykemi AB POLYabs XX0 ABS, Extrusion Grade Information provided by Polykemi AB |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ISO 178 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding... |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ISO 178 |
SABIC Innovative Plastics LNP FARADEX AS003 ABS (Asia Pacific) LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ISO 178 |
SABIC Innovative Plastics LNP FARADEX AS003 ABS (Europe-Africa-Middle East) LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
Eastman Eastar 5445 PCTG Copolyester, Injection Molded
(discontinued **) Eastar PCTG 5445 is an amorphous copolyester. Because of its clarity, toughness and good melt strength, Eastar PCTG Copolyester 5445 is useful in a number of applications. It has high gloss and is t.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | 2mm/min; ASTM D790 |
Kingfa HF-606 Flame Retardant ABS Features:UL 94 V-0 @ 1.6-3.0mm, 5VB @ 2.0mmHigh flowModerate UV stabilityHigh stiffnessApplications:Injection moldingMonitor cabinetCD-ROMPower switchInformation Provided by Kingfa Sci. & Tech. Co.,.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | 2mm/min; ASTM D790 |
Kingfa HP-126 Modified ABS Features:UL94 HB @ 1.6-3.0mmHigh impact resistanceHigh flowApplications:LCD cabinetLarge thin-wall partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ISO 178 |
Ineos ABS Lustran® 288 ABS, Injection Molding Grade Lustran® ABS 288 is a very high-flow injection molding grade of ABS (acrylonitrile butadiene styrene) with good impact strength and high gloss. It is intended for use in a wide range of applicati.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
KYDEX® 311 Co-Extruded High Impact Fire-Rated Thermoplastic Sheet Features:Color-matched cap, black or off-white substrateThickness ranging from 1.5 mm to 8.9 mmToughness and durabilityEasy to form with good part definitionChemical resistantFire retardantExcellent.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
KYDEX® 311 MB Co-Extruded High Impact Fire-Rated Thermoplastic Sheet with Microban® Antimicrobial Features:Color-matched cap, black or off-white substrateThickness ranging from 1.5 mm to 8.9 mmToughness and durabilityEasy to form with good part definitionChemical resistantFire retardantExcellent.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
KYDEX® XD 3D Laminate Thermoplastic 3D Laminate for Flat Lamination and Membrane Pressed Uses Features:Tough and durableResistant to cracking and chippingSolid, integral color3500+ custom colorsResistant to a wide range of chemicalsAbrasion resistantFire retardantExcellent fabrication qualit.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
KYDEX® 321 Co-Extruded High Impact Fire Rated Sheet Features:Metallic cap, black, gray or off-white substrateThickness ranging from 3.18 mm to 8.9 mmTextures: P-3 Velour Matte and P-C Level HaircellImpact resistantEasy to form with good part definiti.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
KYDEX® 331/331d Co-Extruded High Impact Fire Rated Thermoplastic Sheet with Weatherable Acrylic Film Cap KYDEX® 331 is a co-extruded high impact fire rated thermoplastic sheet with a weatherable cap that offers superior performance for thermoforming. It can also be used as an impact resistant surfa.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
KYDEX® T MB High Impact Fire Rated Thermoforming Sheet with Microban® Antimicrobial Product Features:Substitute for FR-ABS sheet with competitive pricing but superior cost/performanceHigher breakage resistanceStandard thicknesses from 0.71 mm to 2.36 mmAmong the most rigid of thermoforming.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
Plenco 1500 Polyester, Granular, Compression Molded PLENCO 01500 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance, and low post shrinkage characteristics. UL recognized under compon.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | |
Zeon Chemicals Zeonex® 330R Cyclo-Olefin Polymer Zeonex®330R has a lower birefringence than other Zeonex® products. This grade can satisfy market demands in the optical area where low birefringence and high dimensional stability in precision opt.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ISO 178 |
Unitika M1030DH PA6, Conditioned Nano composite nylonInformation provided by Unitika Ltd. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ISO 178 |
Polyplastics Duranex® CA7200NX Polybutylene Terephthalate (PBT), Antistatic DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
Eastman Tritan MX810 Copolyester Applications:Blood TherapyDialyzer HousingsIV ComponentsKey Attributes:Ease of processingExcellent clarityExcellent hydrolytic stabilityFast drying timesGood chemical resistanceOutstanding impact re.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
Entec Hypro™ PPH-GF10 Natural Homopolymer Polypropylene, 10% Glass Reinforced Information provided by Entec |
|||
Flexural Strength | 66.0 MPa | 9570 psi | 2 mm/min; ISO 178 |
Chi Mei Polylac® PA-747F ABS - Extrusion Refrigerator |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ISO 178 |
Azoty Tarnow™ TARNOFORM 300 K POM Tribological modified grade with addition of special chalk, which causes decrease of wear.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
BASF Ultramid® 8351 HS BK 102 PA6 (Dry) Description: Ultramid 8351 HS BK-102 is a heat stabilized, pigmented black, impact modified type 6 nylon graft copolymer developed for injection molding applications requiring a high level of toughn.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
BASF Ultramid® 8351 HS BK 106 PA6 (Dry) Description: Ultramid 8351 HS BK-106 is a heat stabilized, pigmented black, impact modified type 6 nylon graft copolymer developed for injection molding applications requiring a high level of toughn.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D-790 |
Axiall 3020 Rigid PVC, Extrusion Georgia Gulf 3020 is a base for use of wood flour up to 40 percent. Impact strength and toughnessFlame retardantChemical resistanceDimensional stabilityInformation provided by Georgia GulfGeorgia G.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
Ashley Polymers Ashlene® ABS Resin F-221 High gloss, high impact, extrusion grade.Data provided by the manufacturer |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ISO 178 |
Unitika BV2120 PA66, Flame Retardant, Conditioned Information provided by Unitika Ltd. |