Material Notes:
KYDEX® 331 is a co-extruded high impact fire rated thermoplastic sheet with a weatherable cap that offers superior performance for thermoforming. It can also be used as an impact resistant surface material.KYDEX® 331d offers the same benefits as KYDEX® 331 but with a decorative cap (black/white, granite).Features:Weatherable formulaHigh impact resistanceFire retardant, self-extinguishingLow moisture absorption, resistance to chipping and cracking, great fabrication and machining properties and flexibilityExcellent forming properties, uniform wall thickness and crisp detailCan be drilled, punched and cut using standard woodworking or metal working toolsSuggested Applications:Kiosk HousingsEquipment HousingsMedical ProductsInformation provided by Kydex, LLC.
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength 42.0 MPa
6090 psi
ASTM D638
Flexural Strength 66.0 MPa
9570 psi
ASTM D790
Flexural Modulus 2.482 GPa
360.0 ksi
ASTM D790
Izod Impact, Notched 6.40 J/cm
12.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 66.7 °C
152 °F
unannealed; ASTM D648
75.5 °C
168 °F
annealed; ASTM D648
Flammability, UL94 V-0
V-0
5VA
5VA