Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 48.0 MPa | 6960 psi | STN EN ISO 178 |
Plastcom PLASTALEN® PH 51 T 40 Polypropylene reinforced with mineral filler Modified homopolymer PP for injection molding with the content of 40% mineral filler. General application. Delivered in black color.Information Provided by Plastcom spol. s r.o. |
|||
Flexural Strength | <= 48.0 MPa | <= 6960 psi | ISO 178 |
Polykemi AB POLYfill PP CCP20020 UV Polypropylene, Mineral Reinforced, UV stabilized Information provided by Polykemi AB |
|||
Flexural Strength | 48.0 MPa | 6960 psi | ASTM D790 |
Proto3000 Duraform® PA Selective Laser Sintering (SLS®) Prototyping Polymer Description: Durable polyamide (nylon) material for real-world physical testing and functional useFeatures: Excellent surface resolution and feature detailEasy-to-processCompliant with USP Class VI .. |
|||
Flexural Strength | <= 48.0 MPa | <= 6960 psi | ISO 178 |
Polykemi AB POLYfill PPH BK901213 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 48.0 MPa | 6960 psi | 0.1 in/min; ASTM D790 |
Ineos Nova 271 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Excellent balance of stiffness, heat resistance, and impact properties, Custom colorsApplications: Injection molding and extrusion, Applications requiring strength and durability where custom colori.. |
|||
Flexural Strength | 48.0 MPa | 6960 psi | 0.1 in/min; ASTM D790 |
Ineos Nova 474 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Custom ColorsApplications: Injection molding, Alternative to engineering resinsPerformance grades of polystyrene are engineered to have specific properties. These products can be custom colored. N.. |
|||
Flexural Strength | 48.0 MPa | 6960 psi | at 3.5% strain; ISO 178 |
FKuR Kunststoff Bio-Flex® A 4100 CL Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Flexural Strength | 48.0 MPa | 6960 psi | ISO 178 |
SABIC Innovative Plastics LNP Lubricomp KX99792 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KX99792 is a compound based on Acetal Copolymer resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the .. |
|||
Flexural Strength | 48.0 MPa | 6960 psi | ASTM D790 |
SABIC Innovative Plastics ULTEM STM1600 PEI Copolymer Siltem 1600 is a flexible copolymer designed for wire and cable applications. It offers a halogen free (according VDE 0472) flame retardant solution that also offers low smoke emission and toxicity... |
|||
Flexural Strength | 48.0 MPa | 6960 psi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp FF004 PE LNP THERMOCOMP* FF004 is a compound based on Polyethylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Strength | 48.0 MPa | 6960 psi | ISO Data |
Styrolution Styrolux 656C SBC Styrolux 656C is a high flow thermoplastic injection molding styrene-butadiene block copolymer. It has crystal clarity, good toughness, good stiffness, and warpage resistance for general molding ap.. |
|||
Flexural Strength | 48.0 MPa | 6960 psi | ISO 178 |
Styrolution Styrolux® 656 C SBC Description: Styrolux® 656 C is a clear styrene-butadiene copolymer (SBC) with enhanced flow properties. It is used almost exclusively for injection molding of rigid, tough parts requiring highes.. |
|||
Flexural Strength | 48.0 MPa | 6960 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly LNP* STAT-LOY* K3000SZ is a compound based on Acetal Copolymer resin. Added feature of this material is: AntiSstatic. |
|||
Flexural Strength | 48.0 MPa | 6960 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly (Asia Pacific) LNP* Stat-loy* K3000SZ is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat. |
|||
Flexural Strength | 48.0 MPa @Temperature 260 °C |
6960 psi @Temperature 500 °F |
ASTM D790 |
Saint-Gobain Meldin® 7001 Direct Formed Polyimide Finished parts and basic shapes made from unfilled polyimide material for structural applications requiring requiring high electrical insulative properties, high purity and low outgassing, and high .. |
|||
Flexural Strength | 48.0 MPa | 6960 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP WX02869H Polyester, TP LNP THERMOCOMP* WX02869H is a compound based on Polyester, TP resin containing High Specific Gravity. Added features of this material include: High Impact. |
|||
Flexural Strength | 48.0 MPa | 6960 psi | ASTM D790 |
A. Schulman POLYFLAM™ E-15937B High Strength Impact Modified Polypropylene DescriptionPolyfort® E-15937B is a high strength impact modified polypropylene.Information provided by A. Schulman. |
|||
Flexural Strength | 48.0 MPa | 6960 psi | ASTM D790 |
A. Schulman POLYFLAM™ E-15937B High Strength Impact Modified Polypropylene DescriptionPolyfort® E-15937B is a high strength impact modified polypropylene.Information provided by A. Schulman. |
|||
Flexural Strength | 48.0 MPa | 6960 psi | ASTM D790 |
A. Schulman POLYFLAM™ E-15937B High Strength Impact Modified Polypropylene DescriptionPolyfort® E-15937B is a high strength impact modified polypropylene.Information provided by A. Schulman. |
|||
Flexural Strength | 48.0 MPa | 6960 psi | ASTM D790 |
A. Schulman POLYFLAM™ E-15937B High Strength Impact Modified Polypropylene DescriptionPolyfort® E-15937B is a high strength impact modified polypropylene.Information provided by A. Schulman. |
|||
Flexural Strength | 48.0 MPa | 6960 psi | ASTM F417 |
CoorsTek Nitrogen Bonded Silicon Carbide, SCNB Thermal Shock Delta Tc = 400°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Flexural Strength | 48.0 - 55.2 MPa | 6960 - 8000 psi | ASTM D790 |
CPC - Vycom FLAMETEC™ KYTEC® PVDF Kytec® PVDF, the homopolymer of 1, 1-difluoroethene, is a tough engineering thermoplastic that offers a unique balance of properties. Kytec has the characteristic stability of fluoropolymers when e.. |
|||
Flexural Strength | 48.0 MPa | 6960 psi | ASTM D790 |
Entec Hypro™ PPH-T30 Homopolymer Polypropylene, 30% Talc Reinforced Information provided by Entec |
|||
Flexural Strength | 48.0 MPa | 6960 psi | ASTM D790 |
3D Systems DuraForm® PA Nylon for SLS® Systems For use with all selective laser sintering (SLS®) systems.ApplicationsComplex, thin-wall ductworkMotorsportsAerospaceHousings and enclosuresImpellers and connectorsConsumer sporting goodsVehicle da.. |
|||
Flexural Strength | 48.0 MPa | 6960 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0334M30CL Mica Reinforced Coupled |
|||
Flexural Strength | 48.0 MPa | 6960 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0339M10CL Mica Reinforced Coupled |
|||
Flexural Strength | 48.0 MPa | 6960 psi | ASTM D790 |
A. Schulman ComAlloy Comshield® 104 Homopolymer Polypropylene, Electrically Conductive - Carbon Black Filled Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Strength | 48.0 MPa | 6960 psi | ASTM D790 |
A. Schulman ComAlloy Voloy® 100 Polypropylene, Mineral Reinforced, Flame Retardant, UL, CSA Data provided by the manufacturer, ComAlloy International Company.15% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Strength | 48.0 MPa | 6960 psi | |
Plastcom SLOVALEN PH 21 T 20 PP, 20% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shr.. |
|||
Flexural Strength | 48.0 MPa | 6960 psi | ISO 178 |
Polyplastics Duracon® TD-20 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |