Proto3000 Duraform® PA Selective Laser Sintering (SLS®) Prototyping Polymer

Category Polymer , Rapid Prototyping Polymer , Thermoplastic , Nylon
Manufacturer Proto3000
Trade Name Duraform®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Proto3000 Duraform® PA Selective Laser Sintering (SLS®) Prototyping Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Durable polyamide (nylon) material for real-world physical testing and functional useFeatures: Excellent surface resolution and feature detailEasy-to-processCompliant with USP Class VI testingCompatible with autoclave sterilizationGood chemical resistance and low moisture absorptionBenefits:Nicely balanced mechanical properties and processabilityBuild prototypes that withstand functional testingProduce durable end-use parts without toolingCreate accurate and repeatable parts as demanded by manufacturersMachinable and paintable for demonstration partsApplications: Complex, thin-wall ductwork- Motorsports- AerospaceHousings and enclosuresImpellers and connectorsConsumer sporting goodsVehicle dashboards and grillesFunctional prototypes that approach end-use performance propertiesAppropriate for low- to mid-volume rapid manufacturingMedical applications requiring USP Class VI compliance, or biocompatibilityParts requiring machining or joining with adhesivesComplex production and prototype plastic partsForm, fit, or functional prototypesInformation provided by Proto3000 for their protoyping engineering services.
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
ASTM D792
Water Absorption 0.070 %

@Time 86400 sec
0.070 %

@Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Shore D 73
73
ASTM D2240
Tensile Strength, Ultimate 43.0 MPa
6240 psi
ASTM D638
Elongation at Break 14 %
14 %
ASTM D638
Tensile Modulus 1.586 GPa
230.0 ksi
ASTM D638
Flexural Strength 48.0 MPa
6960 psi
ASTM D790
Flexural Modulus 1.387 GPa
201.2 ksi
ASTM D790
Izod Impact, Notched 0.320 J/cm
0.599 ft-lb/in
ASTM D256
Izod Impact, Unnotched 3.36 J/cm
6.29 ft-lb/in
ASTM D256
Gardner Impact 2.70 J
1.99 ft-lb
ASTM D5420
Thermal Properties Metric English Comments
CTE, linear 62.3 µm/m-°C

@Temperature 0.000 - 50.0 °C
34.6 µin/in-°F

@Temperature 32.0 - 122 °F
ASTM E831
124.6 µm/m-°C

@Temperature 85.0 - 145 °C
69.22 µin/in-°F

@Temperature 185 - 293 °F
ASTM E831
Specific Heat Capacity 1.64 J/g-°C
0.392 BTU/lb-°F
ASTM E1269
Thermal Conductivity 0.700 W/m-K
4.86 BTU-in/hr-ft²-°F
ASTM E1225
Deflection Temperature at 0.46 MPa (66 psi) 180 °C
356 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
203 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 5.90e+13 ohm-cm
5.90e+13 ohm-cm
ASTM D257
Surface Resistance 7.00e+13 ohm
7.00e+13 ohm
ASTM D257
Dielectric Constant 2.73

@Frequency 1.00e+6 Hz
2.73

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 17.3 kV/mm
439 kV/in
ASTM D149
Dissipation Factor 0.044

@Frequency 1000 Hz
0.044

@Frequency 1000 Hz
ASTM D150