Material Notes:
Kytec® PVDF, the homopolymer of 1, 1-difluoroethene, is a tough engineering thermoplastic that offers a unique balance of properties. Kytec has the characteristic stability of fluoropolymers when exposed to harsh thermal, chemical, and ultraviolet environments. Kytec has a continuous use temperature of 235º F. Kytec is chemically resistant to most acids, bases, and organic solvents and is ideally suited for handling wet or dry chlorine, bromine and other halogens.FEATURES AND BENEFITS Weldability- Easy to fabricate and thermoplastically weldable. Strength- Good tensile strength and mechanical abrasion resistance. Purity- An ultra-pure material. Chemical Resistance- Resistance to a broad range of chemistries. Fire Safe- Meets FM4910 criteria and is FM listed.Information provided by Compression Polymers Corp - Vycom
Physical Properties Metric English Comments
Density 1.77 - 1.79 g/cc
0.0639 - 0.0647 lb/in³
ASTM D792
Water Absorption 0.020 %
0.020 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Shore D 76 - 80
76 - 80
ASTM D2240
Tensile Strength, Ultimate 41.4 MPa
6000 psi
ASTM D638
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D638
Elongation at Break 50 - 250 %
50 - 250 %
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Tensile Modulus 1.55 GPa
225 ksi
ASTM D638
Flexural Strength 48.0 - 55.2 MPa
6960 - 8000 psi
ASTM D790
Flexural Modulus 1.72 GPa
250 ksi
ASTM D790
Compressive Strength >= 61.0 MPa
>= 8850 psi
ASTM D695
Izod Impact, Unnotched 0.801 - 1.33 J/cm
1.50 - 2.50 ft-lb/in
ASTM D256
Coefficient of Friction 0.10 - 0.25
0.10 - 0.25
ASTM D1894
Coefficient of Friction, Static 0.15 - 0.25
0.15 - 0.25
ASTM D1894
Thermal Properties Metric English Comments
CTE, linear 101 - 121 µm/m-°C
<br>@Temperature 20.0 °C
56.0 - 67.0 µin/in-°F
<br>@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.190 - 0.220 W/m-K
1.32 - 1.53 BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 125 - 140 °C
257 - 284 °F
Deflection Temperature at 1.8 MPa (264 psi) 105 - 116 °C
221 - 240 °F
Brittleness Temperature -43.3 °C
-46.0 °F
ASTM D2236
Oxygen Index 43 %
43 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 1.40e+15 ohm-cm
1.40e+15 ohm-cm
ASTM D257
Dielectric Constant 6.0
<br>@Frequency 1e+6 Hz
6.0
<br>@Frequency 1e+6 Hz
ASTM D150
6.8
<br>@Frequency 60 Hz
6.8
<br>@Frequency 60 Hz
ASTM D150
6.9
<br>@Frequency 1000 Hz
6.9
<br>@Frequency 1000 Hz
ASTM D150
Dielectric Strength 12.2 kV/mm
<br>@Thickness 3.17 mm
310 kV/in
<br>@Thickness 0.125 in
ASTM D149
Dissipation Factor 0.013
<br>@Frequency 1000 Hz
0.013
<br>@Frequency 1000 Hz
ASTM D150
0.032
<br>@Frequency 60 Hz
0.032
<br>@Frequency 60 Hz
ASTM D150
0.153
<br>@Frequency 1e+6 Hz
0.153
<br>@Frequency 1e+6 Hz
ASTM D150
Arc Resistance >= 50 sec
>= 50 sec
ASTM D495
Descriptive Properties Value Comments
Factory Mutual 4910 Listed
File #3D1Q5.AM