Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 42.0 MPa | 6090 psi | STN EN ISO 178 |
Plastcom PLASTALEN® PH 91 T 20 Polypropylene reinforced with mineral filler Modified homopolymer PP for injection molding with the content of 20 % mineral filler. General application in all industry branches. Delivered in natural mode and in the full RAL color scale.Informa.. |
|||
Flexural Strength | <= 42.0 MPa | <= 6090 psi | ISO 178 |
Polykemi AB POLYfill PPH K20040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 42.0 MPa | 6090 psi | at 5% strain; ASTM D790 |
Ineos Nova FX550 (ASTM) Advanced Styrenic Polymer
(discontinued **) Extremely high glossHigh Izod impact strengthUL Classification 94 HBPractical toughnessHigh flow for injection moldingScuff resistanceApplications: Replacement resin for selected ABS applicationsRef.. |
|||
Flexural Strength | 42.0 MPa | 6090 psi | ASTM D790 |
LG Chemical LUPOL GP-1000FA General Purpose Polypropylene, High Impact, Flame Retardant, Non-Bleed LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Flexural Strength | 42.0 MPa | 6090 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY A3000T ABS (Asia Pacific) LNP* Stat-loy* A3000T is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat. |
|||
Flexural Strength | 42.0 MPa | 6090 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP AH0230A ABS (Asia Pacific) LNP THERMOCOMP* AH0230A is a compound based on Acrylonitrile Butadiene Styrene resin. Added features of this material include: High Specific Gravity. |
|||
Flexural Strength | 42.0 MPa | 6090 psi | ISO 178 |
Styrolution PS 456EB HIPS Styrolution PS 456EB is a high flow, high impact polystyrene with a good heat resistance and a high stiffness, developed for injection blow molding applications, especially for bottle of yot.High fl.. |
|||
Flexural Strength | 42.0 MPa | 6090 psi | 2 mm/min; ISO 178 |
Sax Polymers SAXALEN PPH335T20 Polypropylene Homopolymer, 20% Talc Filled SAXALEN PPH335T20 is a 20% mineral filled Polypropylene - Homopolymer intended for injection molding with very good flow properties and higher stiffness by low warpage and good surface appearance.In.. |
|||
Flexural Strength | 42.0 MPa | 6090 psi | ASTM D790 |
UBE UBESTA® P3014UMX Powder Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Flexural Strength | 42.0 MPa | 6090 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1908E Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 1908E is a 20% talc filled impact copolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Strength | 42.0 MPa | 6090 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1908E Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 1908E is a 20% talc filled impact copolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Strength | 42.0 MPa | 6090 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1908E Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 1908E is a 20% talc filled impact copolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Strength | 42.0 MPa | 6090 psi | ISO 178 |
Polyplastics Duracon® TD-25 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Flexural Strength | 42.0 MPa | 6090 psi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer HP0334W10L Wollastonite Reinforced |
|||
Flexural Strength | 42.0 MPa | 6090 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0334M30L Mica Reinforced |
|||
Flexural Strength | 42.0 MPa | 6090 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0336M20L Mica Reinforced |
|||
Flexural Strength | 42.0 MPa | 6090 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0336T20L Talc Reinforced |
|||
Flexural Strength | 42.0 MPa | 6090 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0336T30L Talc Reinforced |
|||
Flexural Strength | 42.0 MPa | 6090 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0336T40L Talc Reinforced |
|||
Flexural Strength | 42.0 MPa | 6090 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0336W10L Wollastonite Reinforced |
|||
Flexural Strength | 42.0 MPa | 6090 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0336W30L Wollastonite Reinforced |
|||
Flexural Strength | 42.0 MPa | 6090 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0339W30L1 Wollastonite Reinforced |
|||
Flexural Strength | 42.0 MPa | 6090 psi | ISO 178 |
Azoty Tarnow™ TARNOFORM 500 HI4 POM Easy flow high impact grade, possessing also high damping capacityInformation provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Flexural Strength | 42.0 MPa | 6090 psi | ASTM Test |
BASF Ultramid® 8202C HS PA6 (Conditioned) Ultramid 8202C HS is a heat stabilized, low viscosity, PA6 injection molding homopolymer possessing a modified crystalline structure for increased property performance and faster cycles. It is also.. |
|||
Flexural Strength | 42.0 MPa | 6090 psi | ASTM D790 |
Aclo Accucomp Polypropylene HPO306L Homopolymer |
|||
Flexural Strength | 42.0 MPa | 6090 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0339M20L Mica Reinforced |
|||
Flexural Strength | 42.0 MPa | 6090 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0339W10L Wollastonite Reinforced |
|||
Flexural Strength | 42.0 MPa | 6090 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0339W30L Wollastonite Reinforced |
|||
Flexural Strength | <= 42.0 MPa | <= 6090 psi | ISO 178 |
Polykemi AB POLYfill PPH TS15010 H VTUV1 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |