| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Talc Filler |
| Manufacturer | Aclo Compounders |
| Trade Name | Accutech |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Aclo Accutech Polypropylene Homopolymer HP0336T20L Talc Reinforced.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.011 cm/cm | 0.011 in/in | MD; ASTM D955 |
| Melt Flow | 12 g/10 min | 12 g/10 min | ASTM D1238 |
| Ash | 20 % | 20 % | ASTM D2584 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 92 | 92 | ASTM D785 |
| Tensile Strength at Break | 24.0 MPa | 3480 psi | ASTM D638 |
| Tensile Strength, Yield | 34.0 MPa | 4930 psi | ASTM D638 |
| Elongation at Break | 20 % | 20 % | ASTM D638 |
| Elongation at Yield | 6.0 % | 6.0 % | ASTM D638 |
| Tensile Modulus | 1.60 GPa | 232 ksi | ASTM D638 |
| Flexural Strength | 42.0 MPa | 6090 psi | ASTM D790 |
| Flexural Modulus | 2.299 GPa | 333.5 ksi | ASTM D790 |
| Izod Impact, Notched | 0.299 J/cm | 0.560 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 115 °C | 239 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 62.8 °C | 145 °F |