| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.146 g/cc | 0.04140 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | MD; ASTM D955 |
| Melt Flow | 10 g/10 min | 10 g/10 min | ASTM D1238 |
| Ash | 30 % | 30 % | ASTM D2584 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 86 | 86 | ASTM D785 |
| Tensile Strength at Break | 30.0 MPa | 4350 psi | ASTM D638 |
| Tensile Strength, Yield | 32.0 MPa | 4640 psi | ASTM D638 |
| Elongation at Break | 14 % | 14 % | ASTM D638 |
| Elongation at Yield | 5.0 % | 5.0 % | ASTM D638 |
| Tensile Modulus | 2.899 GPa | 420.5 ksi | ASTM D638 |
| Flexural Strength | 42.0 MPa | 6090 psi | ASTM D790 |
| Flexural Modulus | 3.00 GPa | 435 ksi | ASTM D790 |
| Izod Impact, Notched | 0.352 J/cm | 0.660 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 122 °C | 252 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C | 163 °F |