Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
Polymer Resources PC/TP-GP3-G10 PC/Polyester Alloy, 10% Glass Reinforced Superior Chemical Resistance, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
Polymer Resources PPX-G5 Modified-PPO, 5% Glass Reinforced Modified-Polyphenylene Oxide, 5% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pro.. |
|||
Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
Ravago Manufacturing Americas Hylex® P1010FRVNH Polycarbonate, Unreinforced Information provided by Ravago. |
|||
Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
Ravago Manufacturing Americas Hylex® P1018FRVNHE Polycarbonate Polycarbonate, 18 Melt Flow, Flame Retardant, Non HalogenatedInformation provided by Ravago. |
|||
Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
Solvay Specialty Polymers Amodel® AT-1001L Polyphthalamide (PPA) Amodel® AT-1001L is an unreinforced, impact modified polyphthalamide (PPA) resin that exhibits exceptional impact strength at temperatures ranging from room temperature to as low as -40°F (-40.. |
|||
Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF8 IM4 HS L 8% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 8% Filler by WeightAdditive: LubricantFeatures: Lubricated Appearance: BlackInformation provided by TP Compo.. |
|||
Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
Techmer ES Luriblend® HTN 05007 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, High Heat Resistance and LubricatedAppearance: BlackInformation provided by TP Composites, .. |
|||
Flexural Strength | 96.5 MPa | 14000 psi | Method I (3 point load), 2.0 mm/min; ASTM D790 |
Styron CALIBREâ„¢ 200-14 Polycarbonate Resin Overview: CALIBREâ„¢ 200-14 polycarbonate resin is a natural, FDA compliant, 14 melt flow rate general purpose polycarbonate resin with no mold release or UV stabilizer.Govt. and Industry Standar.. |
|||
Flexural Strength | 96.5 MPa | 14000 psi | Method I (3 point load), 2.0 mm/min; ASTM D790 |
Styron CALIBREâ„¢ 201-22 Polycarbonate Resin Overview: CALIBREâ„¢ 201-22 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc.. |
|||
Flexural Strength | 96.5 MPa | 14000 psi | Method I (3 point load), 2.0 mm/min; ASTM D790 |
Styron CALIBREâ„¢ 203-22 Polycarbonate Resin Overview: CALIBREâ„¢ 200-22 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc.. |
|||
Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
Styron CALIBREâ„¢ 301-10 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Flexural Strength | 96.5 MPa | 14000 psi | Method I (3 point load), 2.0 mm/min; ASTM D790 |
Styron CALIBREâ„¢ 301V-6 Polycarbonate Resin Overview: CALIBREâ„¢ 301V-6 Polycarbonate resins offer exceptional impact resistance and heat distortion resistance, and meets UL94 V-2 rating. CALIBRE 301V-6 contains a mold release agent and is.. |
|||
Flexural Strength | 96.5 MPa | 14000 psi | 3-points, 2 mm/min; ASTM D790 |
Styron CALIBREâ„¢ 2060-6 Polycarbonate CALIBREâ„¢ 2060-6 resin is designed for medical applications which use steam or ethylene oxide for sterilization. This material has excellent retention of physical properties and optical clarity.. |
|||
Flexural Strength | 96.5 MPa | 14000 psi | Method I (3 point load), 2.0 mm/min; ASTM D790 |
Styron CALIBREâ„¢ 302V-6 Polycarbonate Resin Overview: CALIBREâ„¢ 302V-6 Polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity (for tinted/transparent colors), and is available in both tint.. |
|||
Flexural Strength | 96.5 MPa | 14000 psi | 0.125 in, injection molded, unannealed; ASTM D790 |
Styron EMERGEâ„¢ 4530-15 Polycarbonate EMERGEâ„¢ PC 4530-15 advanced resin is a general purpose polycarbonate resin offering ultraviolet light stability, ignition resistance, heat resistance and excellent toughness. Applications: Co.. |
|||
Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
Lubrizol ISOPLAST™ 302EZ Engineering Thermoplastic Polyurethane Resin NSF Standard 61 CertifiedInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
Chase Plastics CP Pryme® NN100HL (Dry) Nylon 66, Heat Stabilized, Lubricated Features: Heat StabilizedLubricatedForm: PelletsInformation provided by Chase Plastics. |
|||
Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
Chase Plastics CP Pryme® NN300HL (Dry) Nylon 66, Heat Stabilized, Lubricated Features: General purposeHeat stabilizedLubricatedForm: PelletsInformation provided by Chase Plastics. |
|||
Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
Chase Plastics CP Pryme® PC300RHF Polycarbonate, Recycled Content Features: Good flowHigh rigidityGood toughnessHigh strengthLow viscosityGood mold releaseRecycled contentForm: PelletsInformation provided by Chase Plastics. |
|||
Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
A. Schulman COMTUF® 5011 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman. |
|||
Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
A. Schulman COMTUF® 5011 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman. |
|||
Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
Entec Hylex® P1017FR Polycarbonate Information provided by Ravago. |
|||
Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
Entec Hylex® P1317FR Polycarbonate Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
Entec Hypro™ PPC-GF40 Natural Impact Polypropylene, 40% Glass Reinforced Information provided by Entec |
|||
Flexural Strength | 96.5 - 110 MPa | 14000 - 16000 psi | |
Bulk Molding Compounds BMC 102 Glass Filled Thermoset Polyester BMC 102 is a medium strength, glass fiber reinforced molding compound that meets Ford Specification ESF-M3D56-A. It can be supplied in bulk or extruded in pre-weighed slugs and is well suited for in.. |
|||
Flexural Strength | 96.5 - 124 MPa | 14000 - 18000 psi | |
Bulk Molding Compounds BMC 610 Mineral Filled, Glass Reinforced Polyester Compound BMC 610 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is set a part form other medium impact el.. |
|||
Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
Solvay Specialty Polymers Amodel® AT-1001L Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1001L is an unreinforced, impact modified polyphthalamide (PPA) resin that exhibits exceptional impact strength at temperatures ranging from room temperature to as low as -40°F (-40°C), .. |