Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | <= 92.0 MPa | <= 13300 psi | ISO 178 |
Polykemi AB POLYfill PPH GF5015 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Flexural Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CY6012 PC+ABS (Asia Pacific) Cycoloy* resin grade CY6012 is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant systems. Excellent impact/flow balance together with a UL-94 V0 & 5VB rating.. |
|||
Flexural Strength | <= 92.0 MPa | <= 13300 psi | ISO 178 |
Polykemi AB POLYshine PBT D201 T20 PBT, Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 92.0 MPa | 13300 psi | ASTM D790 |
Kolon KOCETAL® DS500 Acid Resistant Acetal Resin Improved acid resistance. Applications: Products for improved chemical resistance. Information provided by API-Kolon. |
|||
Flexural Strength | 92.0 MPa | 13300 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP KZL16 Acetal Copolymer LNP LUBRICOMP* KZL16 is a compound based on Acetal Copolymer resin containing Glass Fiber, Milled Glass, PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Strength | 92.0 MPa | 13300 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP KZL16 Acetal Copolymer LNP LUBRICOMP* KZL16 is a compound based on Acetal Copolymer resin containing Glass Fiber, Milled Glass, PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Strength | 92.0 MPa | 13300 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP LL003 PEEK LNP* LUBRICOMP* LL003 is a compond based on Polyetheretherketone resin containing 15% PTFE Lubricant. Added feature of this material is: Wear Resistant. |
|||
Flexural Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics XYLEX HX7509HP PC+POLYESTER (Europe-Africa-Middle East) Medium flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), fo.. |
|||
Flexural Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics XYLEX X7509HP PC+POLYESTER PC+Polyester alloy. Houseware applications. USA/Europe Food contact. this grade will no longer be supported with biocompatibility information and should not be used for medical applications which r.. |
|||
Flexural Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics XYLEX X7509HP PC+POLYESTER (Asia Pacific) PC+Polyester alloy. Houseware applications. USA/Europe Food contact. this grade will no longer be supported with biocompatibility information and should not be used for medical applications which r.. |
|||
Flexural Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics XYLEX X7509HP PC+POLYESTER (Europe-Africa-Middle East) PC+Polyester alloy. Houseware applications. USA/Europe Food contact. this grade will no longer be supported with biocompatibility information and should not be used for medical applications which r.. |
|||
Flexural Strength | 92.0 MPa | 13300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP AX08306 ABS LNP* THERMOCOMP* AX08306 is a compound based on ABS resin containing Proprietary Filler(s). Added feature of this grade is: Platable. |
|||
Flexural Strength | 92.0 MPa | 13300 psi | 2mm/min; ISO 178 |
Teijin Panlite® LN-2250Y Flame Resistant, Translucent Polycarbonate Resin Flame retardant and mold release grade with normal fluidity, while maintaining intrinsic transparency of polycarbonate resin. It is suitable for injection molding applications.Applications:Electric,.. |
|||
Flexural Strength | 92.0 MPa | 13300 psi | 2mm/min; ISO 178 |
Teijin Panlite® LV-2225Y Standard (mold release/ice color grade) Polycarbonate Resin Flame retardant and mold release grade, while maintaining intrinsic transparency of polycarbonate resin. It is suitable for injection molding applications, required to be slightly high fluidity.Appl.. |
|||
Flexural Strength | 92.0 MPa | 13300 psi | ASTM D790 |
SABIC Innovative Plastics NORYL N300 PPE (Asia Pacific) High Heat 150deg.C, FR V-0 |
|||
Flexural Strength | 92.0 MPa | 13300 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP EP003 PEI LNP* Lubricomp EP003 is a Polyetherimide containing 15% PTFE/Silicone. Added features include: Internally Lubricated. |
|||
Flexural Strength | 92.0 MPa | 13300 psi | ISO 178 |
SABIC Innovative Plastics LNP Lubricomp LL003E PEEK LNP* Lubricomp* LL003E is a compound based on Polyetheretherketone (PEEK) containing PTFE. Characteristics of this grade are: Easy Molding and Internally Lubricated.This data was supplied by SABIC.. |
|||
Flexural Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xylex X7529 PC+POLYESTER (Asia Pacific) PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical quality. UV 400nm block.This data was supplied by SABIC-IP for the Asia Pacif.. |
|||
Flexural Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xylex X7529OQ PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical qualityThis data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |
|||
Flexural Strength | 92.0 MPa | 13300 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP MF004AS PP LNP THERMOCOMP* MF004AS is a compound based on Polypropylene resin containing 20% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Strength | 92.0 MPa | 13300 psi | ASTM D790 |
Plenco 1501 Polyester, Briquette, Transfer Molded PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va.. |
|||
Flexural Strength | 92.0 MPa | 13300 psi | ASTM D790 |
Plenco 2000 Phenolic, Granular, Compression Molded PLENCO 02000 is a versatile general purpose, organic filled phenolic molding compound, offering optimum cure characteristics and an excellent balance of molding properties. UL recognized under compo.. |
|||
Flexural Strength | 92.0 MPa | 13300 psi | ASTM D790 |
Plenco 2311 Phenolic, Granular, Compression Molded PLENCO 02311 is a versatile general purpose organic filled phenolic molding compound offering excellent mold processability and optimized cure cycles. PLENCO 02311 is also granulated to provide impr.. |
|||
Flexural Strength | 92.0 MPa | 13300 psi | ASTM D790 |
Plenco 4300 Phenolic, Granular, Transfer Molded PLENCO 04300 is a heat resistant, mineral filled phenolic molding compound offering optimum cure characteristics and excellent dimensional stability. It is formulated for wiring devices and electric.. |
|||
Flexural Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
Chi Mei Kibisan® PN-106 L150 SAN High Clarity |
|||
Flexural Strength | 92.0 MPa | 13300 psi | ISO 178 |
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri.. |
|||
Flexural Strength | 92.0 MPa | 13300 psi | ASTM D790 |
A. Schulman ComAlloy Lubrilon® 606 Nylon 6/6, PTFE Filled, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Flexural Strength | 92.0 MPa | 13300 psi | 2.6 mm/min; ASTM D790 |
BLUESTAR LXS 115 PPE-PS Typical Applications: Auto connect partsFire RatedInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Strength | 92.0 MPa | 13300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xylex X7529OQ PC+POLYESTER (Asia Pacific) PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical qualityThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Strength | 92.0 MPa | 13300 psi | ISO 178 |
Polyplastics Duracon® HP25X Acetal Co-polymer (POM), High stiffness, High viscosity DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |