Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 7.47 J/cm @Temperature -28.9 °C |
14.0 ft-lb/in @Temperature -20.0 °F |
ASTM D256 |
Polymer Resources TP-IM1 Polybutylene Terephthalate, Low Temperature Impact Modified Polybutylene Terephthalate, Low Temperature Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Izod Impact, Notched | 7.47 J/cm @Temperature 22.8 °C |
14.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Ravago Manufacturing Americas Hybrid B2026IU Polycarbonate + PBT Alloy Available in North America UV Stabilizer Good Impact Resistance RoHS Compliant Form: Pellets Processing Method: Injection Molding Information provided by Ravago |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 6.35 mm, Temperature 22.8 °C |
14.0 ft-lb/in @Thickness 0.250 in, Temperature 73.0 °F |
ASTM-D256 |
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (DAM) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 6.35 mm, Temperature 22.8 °C |
14.0 ft-lb/in @Thickness 0.250 in, Temperature 73.0 °F |
ASTM-D256 |
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (Conditioned) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Izod Impact, Notched | 7.47 J/cm @Temperature 23.0 °C |
14.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Asia Pacific) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 7.47 J/cm @Temperature 23.0 °C |
14.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Europe-Africa-Middle East) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
14.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® PC/PBT IM 1799 BK Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
14.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® PC/PBT IM 5720 A BK Availability: North AmericaForms: PelletsAdditive: Impact Modifier and UV StabilizerFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
14.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® PC/PBT IM 6200 BK Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
14.0 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Plastiblend® PC/PBT IM 6600 Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
14.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® PC/PBT IM 6600 Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 7.47 J/cm @Temperature 23.0 °C |
14.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Valox® 364 PBT Designed for outdoor telecommunications enclosure applications.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 7.47 J/cm @Temperature 23.0 °C |
14.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Formosa Plastics Formolene® 2706N Impact Copolymer Polypropylene Copolymer for Heavy Duty Injection Molded Applications Formolene® 2706N is a copolymer of polypropylene designed and formulated for injection molding applications. It contains a unique combination .. |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
14.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D-256 |
Axiall SP-7221 Rigid PVC, Molding Georgia Gulf SP-7221 is a high impact rigid vinyl compound designed for water distribution systems. The product is NSF listed under Standard 14.Information provided by Georgia GulfGeorgia Gulf beca.. |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 3.17 mm |
14.0 ft-lb/in @Thickness 0.125 in |
ASTM D-256 |
Axiall 9017 Rigid PVC, Molding Georgia Gulf 9017 is for food packaging applications requiring optimum taste and odor properties such as water and mouthwash.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporatio.. |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
14.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D-256 |
Axiall UV-7160 Rigid PVC, Molding Georgia Gulf UV-7160 is a rigid vinyl injection molding compound characterized by excellent flow, toughness, heat stability, color hold and surface appearance. This combination of outstanding attri.. |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
14.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D-256 |
Axiall 6509 Rigid PVC, Molding Georgia Gulf 6509 is a non-regulated, high flow, injection molding compound that has been specifically designed for outdoor applications that require an added degree of static resistance.Information.. |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 3.17 mm |
14.0 ft-lb/in @Thickness 0.125 in |
ASTM D-256 |
Axiall 9017J Clear 06 Rigid PVC, Molding, Clear Georgia Gulf 9017J Clear 06 is for food packaging and personal care applications requiring optimum taste and odor properties. The compound contains an ultraviolet light stabilizer, which protects l.. |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 6.35 mm |
14.0 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Axiall 9202J Rigid PVC, Molding Georgia Gulf 9202J is suitable for all types of food packaging. The compound provides low taste and odor properties and contains an ultraviolet light stabilizer which protects light sensitive produ.. |