Material Notes:
Georgia Gulf 9202J is suitable for all types of food packaging. The compound provides low taste and odor properties and contains an ultraviolet light stabilizer which protects light sensitive products.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D-638
Tensile Modulus 2.41 GPa
350 ksi
ASTM D-638
Flexural Strength 69.6 MPa
10100 psi
ASTM D-790
Flexural Modulus 2.24 GPa
325 ksi
ASTM D-790
Izod Impact, Notched 7.47 J/cm

@Thickness 6.35 mm
14.0 ft-lb/in

@Thickness 0.250 in
ASTM D-256
10.7 J/cm

@Thickness 3.17 mm
20.0 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Tensile Impact Strength 178 kJ/m²
85.0 ft-lb/in²
ASTM D-1822
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ASTM D-648
Optical Properties Metric English Comments
Haze 6.0 %

@Thickness 3.17 mm
6.0 %

@Thickness 0.125 in
pressed plaque; ASTM D-1003-61
Transmission, Visible 76 %

@Thickness 3.17 mm
76 %

@Thickness 0.125 in
pressed plaque; ASTM D-1003-61
Descriptive Properties Value Comments
Bottle Means Failure Height, ft 15+
Vertical Free Fall; 30-g., 16-oz. cylinders
Equilibrium Torque, meter-grams 1450
Brabender Plastograph, No. 6 Roller Head, 190°C Bath, 57-g. Charge; 60/43 rpm
Stability Time, minutes 22