Axiall SP-7221 Rigid PVC, Molding

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall SP-7221 Rigid PVC, Molding.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Georgia Gulf SP-7221 is a high impact rigid vinyl compound designed for water distribution systems. The product is NSF listed under Standard 14.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D-792
Linear Mold Shrinkage 0.0040 - 0.0050 cm/cm
0.0040 - 0.0050 in/in
ASTM D-955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 97
97
ASTM D-785
Tensile Strength, Yield 42.7 MPa
6200 psi
ASTM D-638
Tensile Modulus 2.41 GPa
350 ksi
ASTM D-638
Flexural Strength 68.9 MPa
10000 psi
ASTM D-790
Flexural Modulus 2.59 GPa
375 ksi
ASTM D-790
Izod Impact, Notched 0.694 J/cm

@Thickness 3.17 mm,
Temperature -20.0 °C
1.30 ft-lb/in

@Thickness 0.125 in,
Temperature -4.00 °F
ASTM D-256
7.47 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
14.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Gardner Impact 36.2 J

@Temperature 23.0 °C
26.7 ft-lb

@Temperature 73.4 °F
1/2" R Tup, 123 mil
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 74.00 °C
165.2 °F
ASTM D-648
Deflection Temperature at 1.8 MPa (264 psi) 71.00 °C
159.8 °F
ASTM D-648
Oxygen Index 36 %
36 %
ASTM D-2863
Descriptive Properties Value Comments
Cell Classification, ASTM D-1784 14333-D
NSF std. 14
Flow Ratio (Distance/Wall Thickness, 390-400°F) 130
Georgia Gulf Test