Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.40 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M3500 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 6.40 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M3800 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 6.40 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M3890 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 6.40 J/cm @Thickness 3.18 mm, Temperature 0.000 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
Injection Molded; ASTM D256A |
PolyOne Novablend™ 9562 Polyvinyl Chloride Alloy (PVC Alloy) Custom MoldingInformation provided by PolyOne |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo.. |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo.. |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CY9640 PC+ABS (Europe-Africa-Middle East) PC+ ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® LG8002 PC+ABS Automotive. Low gloss, high impact and ductility at 73F and -22F. UV-stable colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® LG8002 PC+ABS (Asia Pacific) Automotive. Low gloss, high impact and ductility at 73F and -22F. UV-stable colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® MC9000 PC+ABS AUTOMOTIVE. PC+ABS; high heat resistant. Ductile at room temperature. Excellent flow.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® MC9000 PC+ABS (Asia Pacific) AUTOMOTIVE. PC+ABS; high heat resistant. Ductile at room temperature. Excellent flow.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® XCY620 PC+ABS (Europe-Africa-Middle East) PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Eur.. |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® EM3110R PC Automotive interiors. Optimizes flow/processability for cost effective thinner wall design uses. Internal mold release.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 6.40 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
12.0 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in .. |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature -30.0 °C |
12.0 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer (Europe-Africa-Middle East) Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul.. |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® HPH4504 PPC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® HPH4504H PPC (Europe-Africa-Middle East) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Izod Impact, Notched | 6.40 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ HC 8210 Polyvinyl Chloride, Rigid (PVC, Rigid) Geon HC 8210 is a high flow, high impact resistance rigid grade offering enhanced chemical resistance for medical device housing applications. It is RoHS compliant with UL V0 and 5VA ratings.Informa.. |
|||
Izod Impact, Notched | 6.40 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ SF M7000 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 6.40 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ SF M7010 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 6.40 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ SF M7020 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Geloy XTPM307 ASA+PC (Europe-Africa-Middle East) XTPM307 is a high heat resistant PC/ASA with improved processing stability over HRA150. Typical values measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® ML5472 PC Gamma sterilization resistant. High heat (PPC). Available in natural color only. Internal mold release.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
50%RH; ASTM D256 |
DuPont Performance Polymers Zytel® 7304 NC010 Nylon 6
(Unverified Data**) Zytel® 7304 NC010 is a medium viscosity, unlubricated polyamide 6 resin for extrusion applications.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Valox® 365 PET Unreinforced, opaque, provides chemical resistance and dimensional stability, UL94V-0 rated at 0.031".This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 6.40 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
12.0 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
Injection Molded; ASTM D256 |
Styron PULSEâ„¢ 2100 LG PC/ABS Engineering Resin Overview: PULSE 2100LG Engineering Resin is designed to provide top performance in tough applications, from single piece items to intricate components. Ideal for energy management solutions, it can .. |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Styron PULSEâ„¢ 2300 PT PC/ABS Engineering Resin Information provided by Styron |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature -40.0 °C |
12.0 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Styron PULSEâ„¢ 6000 BG PC/ABS Engineering Resin Overview: PULSE 6000 BG is a PC/ABS resin offering an interesting combination of heat ageing characteristics, low temperature impact performance and high melt strength. Its low MFR enables manufactu.. |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Lubrizol Estaloc® 59020 Reinforced Thermoplastic Polyurethane Type: Estaloc® 59020 RETPU is a polyester-type reinforced engineered thermoplastic polyurethane (RETPU).Features: Fast cycling, dimensional stability, durability, aesthetics, low temperature impact.. |
|||
Izod Impact, Notched | 6.40 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
12.0 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
0.25 mm Notch Depth, Injection Molded; ASTM D256 |
Styron PULSE™ EXT 100 PC/ABS Engineering Resin Overview: PULSE EXT 100 engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at both room and low temperatures. PULSE EXT 100 engin.. |