Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.20 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.25 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87775 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 1.20 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.25 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding 87546 Polyvinyl Chloride, Rigid (PVC, Rigid) Provisional Data SheetInformation provided by PolyOne |
|||
Izod Impact, Notched | 1.20 J/cm @Temperature -30.0 °C |
2.25 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CE1821 PC+ABS (Europe-Africa-Middle East) High stiffness PC/ABS blend offering high impact, high heat, low CTE, good surface quality and excellent extrusion and thermoforming characteristics.This data was supplied by SABIC-IP for the Europe.. |
|||
Izod Impact, Notched | 1.20 J/cm @Temperature -30.0 °C |
2.25 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CX7110 PC+ABS (Europe-Africa-Middle East) Cycoloy* resin grade CX7110 is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant systems. Excellent impact/flow balance together with a UL-94 V0 rating at 1... |
|||
Izod Impact, Notched | 1.20 J/cm @Temperature 23.0 °C |
2.25 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
SABIC PP 57MNK10 Polypropylene Impact Copolymer for Injection Molding Product Description: PP 57MNK10 is a controlled rheology PP grade of medium molecular weight distribution specially developed for producing injection molded articles. This grade has an excellent i.. |
|||
Izod Impact, Notched | 1.20 J/cm @Thickness 6.35 mm |
2.25 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
LG Chemical SG-910 Alphalac Polystyrene
(Unverified Data**) High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include housing of electric appliances |
|||
Izod Impact, Notched | 1.20 J/cm @Temperature 23.0 °C |
2.25 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Micropol Microstat ML21 Linear medium density static dissipative polyethylene Information provided by Micropol Limited |
|||
Izod Impact, Notched | 1.20 J/cm @Temperature -30.0 °C |
2.25 ft-lb/in @Temperature -22.0 °F |
ASTM Test |
Styrolution Terluran® HI-10 ABS Terluran HI-10 is an injection molding and extrusion grade of ABS with very high toughness and medium flow.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Izod Impact, Notched | 1.20 J/cm @Temperature 23.0 °C |
2.25 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl NH3060 PPE+HIPS NH3060 resin is a modified PPE + PS blend with an excellent balance of non-chlorinated non-brominated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific .. |
|||
Izod Impact, Notched | 1.20 J/cm @Temperature 23.0 °C |
2.25 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl PX0003 PPE+HIPS PX0003 resin is a modified PPE+PS blend with an excellent balance of non-chlorinated non-brominated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific gr.. |
|||
Izod Impact, Notched | 1.20 J/cm @Temperature 23.0 °C |
2.25 ft-lb/in @Temperature 73.4 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® T-402 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 1.20 J/cm @Temperature -40.0 °C |
2.25 ft-lb/in @Temperature -40.0 °F |
Practical Use (Water Absorption 1.25%); ASTM-D256 |
Toyobo GLAMIDE® T-663G50 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 1.20 J/cm @Temperature 23.0 °C |
2.25 ft-lb/in @Temperature 73.4 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® T-665C30 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 1.20 J/cm @Temperature 23.0 °C |
2.25 ft-lb/in @Temperature 73.4 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® TY-502NZ 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 1.20 J/cm @Temperature 23.0 °C |
2.25 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTABLEND 0820 GF Polycarbonate ABS Blend, 10% Glass Filled Polycarbonate and Acrylonitrile Butadiene Styrene blend with 10% glass fiber reinforcementGood impact resistance, good thermal resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 1.20 J/cm @Temperature 23.0 °C |
2.25 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTACARB 0820 GF Polycarbonate, 10% Glass Filled Polycarbonate with 10% glass fiber reinforcementHigh stiffness, good impact resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 1.20 J/cm @Temperature 23.0 °C |
2.25 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTACARB 1601 OPALE Polycarbonate Polycarbonate for injection moldingOpal, light diffusiveInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 1.20 J/cm @Temperature 23.0 °C |
2.25 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTADIENE 1030 V0/F Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, high melt flow rate, good impact resistance, high gloss, good light resistance, excellent processabilityInformation provided by Co.. |
|||
Izod Impact, Notched | 1.20 J/cm @Temperature 23.0 °C |
2.25 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTADIENE 1218 V0/B Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, good impact resistance, excellent processability, good surface appearanceInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 1.20 J/cm @Temperature 23.0 °C |
2.25 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTASTIR HI 0412 Polystyrene Polystyrene for injection molding or extrusionHigh impact resistance, good thermal resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 1.20 - 1.50 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.25 - 2.81 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilac T ABS Acrylonitrile Butadiene Styrene |
|||
Izod Impact, Notched | 1.20 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.25 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilon G2-PC 10% GF Polycarbonate, 10% Glass Fiber Characteristics: 10% glass fibre filled, good mechanical properties |
|||
Izod Impact, Notched | 1.20 J/cm @Temperature 23.0 °C |
2.25 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Braskem RP 347 Injection Molding Polypropylene Description: RP 347 is a medium melt flow rate random copolymer designed for injection moulding. This product offers excellent transparency and gloss, very good stiffness/impact strength balance, ex.. |
|||
Izod Impact, Notched | 1.20 J/cm @Temperature 23.0 °C |
2.25 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Carmel Olefins CAPILENE® SL 50 Polypropylene Impact Copolymer Description: CAPILENE® SL 50 is a medium melt flow rate impact copolymer for injection molding applications. This grade combines good stiffness and impact properties.Applications: CAPILENE® SL .. |
|||
Izod Impact, Notched | 1.20 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.25 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® X5402 PPE/PA Oil ResistantInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.20 J/cm @Thickness 3.18 mm, Temperature -18.0 °C |
2.25 ft-lb/in @Thickness 0.125 in, Temperature -0.400 °F |
Compression Molded, all complete breaks; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L6256 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |