Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem RP 347 Injection Molding Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem RP 347 Injection Molding Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: RP 347 is a medium melt flow rate random copolymer designed for injection moulding. This product offers excellent transparency and gloss, very good stiffness/impact strength balance, excellent processability and also provides very low odor/taste. Applications: Cosmetic packaging; Containers for freezer; Containers with high transparency. Information provided by Braskem
Physical Properties Metric English Comments
Density 0.902 g/cc
0.0326 lb/in³
ASTM D792A
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238L
Mechanical Properties Metric English Comments
Hardness, Rockwell R 83
83
ASTM D785
Tensile Strength, Yield 30.0 MPa
4350 psi
ASTM D638
Elongation at Yield 14 %
14 %
ASTM D638
Flexural Modulus 0.950 GPa
138 ksi
1% secant; ASTM D790
Izod Impact, Notched 0.200 J/cm

@Temperature -20.0 °C
0.375 ft-lb/in

@Temperature -4.00 °F
ASTM D256A
1.20 J/cm

@Temperature 23.0 °C
2.25 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 51.0 °C
124 °F
ASTM D648
Vicat Softening Point 128 °C
262 °F
10 N; ASTM D1525
Optical Properties Metric English Comments
Haze 16 %
16 %
ASTM D1003