Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Cycoloy® CX7110 PC+ABS (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Cycoloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Cycoloy® CX7110 PC+ABS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Cycoloy* resin grade CX7110 is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant systems. Excellent impact/flow balance together with a UL-94 V0 rating at 1.2mm makes it an ideal candidate for various applications including thin wall designs.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D 792
Density 1.19 g/cc
0.0430 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.10 %
0.10 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.20 %

@Temperature 23.0 °C
0.20 %

@Temperature 73.4 °F
ISO 62
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm

@Thickness 3.20 mm
0.0040 - 0.0060 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 21 g/10 min

@Load 2.16 kg,
Temperature 260 °C
21 g/10 min

@Load 4.76 lb,
Temperature 500 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
22 g/10 min

@Load 2.16 kg,
Temperature 260 °C
22 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 51.0 MPa
7400 psi
50 mm/min; ISO 527
54.0 MPa
7830 psi
Type I, 50 mm/min; ASTM D 638
Tensile Strength, Yield 61.0 MPa
8850 psi
50 mm/min; ISO 527
64.0 MPa
9280 psi
Type I, 50 mm/min; ASTM D 638
Elongation at Break 90 %
90 %
Type I, 50 mm/min; ASTM D 638
90 %
90 %
50 mm/min; ISO 527
Elongation at Yield 4.0 %
4.0 %
Type I, 50 mm/min; ASTM D 638
4.0 %
4.0 %
50 mm/min; ISO 527
Tensile Modulus 2.70 GPa
392 ksi
1 mm/min; ISO 527
2.90 GPa
421 ksi
50 mm/min; ASTM D 638
Flexural Yield Strength 100 MPa
14500 psi
1.3 mm/min, 50 mm span; ASTM D 790
100 MPa
14500 psi
2 mm/min; ISO 178
Flexural Modulus 2.50 GPa
363 ksi
2 mm/min; ISO 178
2.70 GPa
392 ksi
1.3 mm/min, 50 mm span; ASTM D 790
Izod Impact, Notched 1.20 J/cm

@Temperature -30.0 °C
2.25 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
6.00 J/cm

@Temperature 23.0 °C
11.2 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Notched (ISO) 10.0 kJ/m²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
15.0 kJ/m²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
80*10*3; ISO 180/1A
Charpy Impact, Notched 1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA
1.50 J/cm²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA
Impact Test 63.0 J

@Temperature 23.0 °C
46.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 75.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
75.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 75.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
75.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Thermal Conductivity 0.200 W/m-K
1.39 BTU-in/hr-ft²-°F
ISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C

@Thickness 3.20 mm
201 °F

@Thickness 0.126 in
unannealed; ASTM D 648
98.0 °C

@Thickness 6.40 mm
208 °F

@Thickness 0.252 in
unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C
183 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
84.0 °C

@Thickness 3.20 mm
183 °F

@Thickness 0.126 in
unannealed; ASTM D 648
90.0 °C

@Thickness 6.40 mm
194 °F

@Thickness 0.252 in
unannealed; ASTM D 648
Vicat Softening Point 102 °C
216 °F
Rate B/50; ASTM D 1525
102 °C
216 °F
Rate B/50; ISO 306
103 °C
217 °F
Rate B/120; ISO 306
Flammability, UL94 V-2

@Thickness 0.750 mm
V-2

@Thickness 0.0295 in
UL 94
V-1

@Thickness 1.00 mm
V-1

@Thickness 0.0394 in
UL 94
V-0

@Thickness 1.20 mm
V-0

@Thickness 0.0472 in
UL 94
5VB

@Thickness 1.80 mm
5VB

@Thickness 0.0709 in
UL 94
Descriptive Properties Value Comments
Ball Pressure Test, 75°C +/- 2°C Pass
IEC 60695-10-2