Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.981 J/cm @Temperature 23.0 °C |
1.84 ft-lb/in @Temperature 73.4 °F |
|
PolyMirae Moplen EP300K Injection Molding Grade Polypropylene Moplen EP300K is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP300K is a block copolymer particularly suitable for injection.. |
|||
Izod Impact, Notched | 0.981 J/cm @Temperature 23.0 °C |
1.84 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
PolyMirae Moplen EP500N Injection Molding Grade Polypropylene Moplen EP500N is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP500N is a block copolymer particularly suitable for injection.. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 6.50 mm, Temperature 23.0 °C |
1.84 ft-lb/in @Thickness 0.256 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical ALPHALAC SF510 HIPS Super flow, High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include TV cabinets, thin pa.. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 6.50 mm, Temperature 23.0 °C |
1.84 ft-lb/in @Thickness 0.256 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical ALPHALAC SG960 HIPS Description: Injection Molding, General Purpose, Good ProcessabilityApplication: Washer Cover, Air-conditioner Panel, Refrigerator PartsCAS No. 9003-55-8Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.84 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HIPS 405AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 158725-44-1 and 1309-64-4Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.84 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical KEYFLEX BT 1072D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 6.40 mm, Temperature -40.0 °C |
1.84 ft-lb/in @Thickness 0.252 in, Temperature -40.0 °F |
ASTM D256 |
LG Chemical KEYFLEX BT 1163D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.84 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical MA210 ABS, Low Gloss Feature: Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.84 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical XR440 ABS, Low Emission High Heat ABS Feature: Injection Molding Grade, Low Emission High Heat ABSApplication: Automotives Interior housingCAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.84 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical XR474F ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Exterior Housing (Lamp Housing Etc)CAS No. 25120-20-1, 9003-56-9, 31621-07-5, and 9003-54-7Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 6.50 mm, Temperature 23.0 °C |
1.84 ft-lb/in @Thickness 0.256 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical ALPHALAC SG970NSU HIPS Description: Injection Molding, General Purpose, Good Processability, High gloss, antistatic and UV stabilizedApplication: Air Conditioner Panel, Washer CoverCAS No. 9003-55-8Information provided by.. |
|||
Izod Impact, Notched | >= 0.981 J/cm @Thickness 6.40 mm, Temperature -10.0 °C |
>= 1.84 ft-lb/in @Thickness 0.252 in, Temperature 14.0 °F |
ASTM D256 |
LG Chemical LUPOL TE5007B PP+Rubber, High Impact Description: Injection Molding, PP+Rubber, Low Density, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia , Rear Bumper Step)Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.84 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical XG569C MABS, Anti-Scratch, High Gloss Feature: Injection Molding, Anti-Scratch, High GlossApplication: LCD TV Front Cabinet, Bezel, Audio/Video HousingCSA No. 9011-14-7 and 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 6.35 mm |
1.84 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® FD-1122 PC, FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | >= 0.981 J/cm @Thickness 3.17 mm |
>= 1.84 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® FD-1122 PC, FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 3.17 mm |
1.84 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® HN-3104 PC, 10% Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 6.35 mm |
1.84 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® BC-0130 X ABS, Unreinforced General Purpose Stiff ABS material that is used for battery casesInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 6.35 mm |
1.84 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® SF-0505H MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 6.35 mm |
1.84 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® WX-9700 ASA, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 3.17 mm |
1.84 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® FD-1112 PC, FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 6.35 mm |
1.84 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® FD-1122 PC, FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 3.17 mm |
1.84 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® HN-3104 PC, 10% Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 6.35 mm |
1.84 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® BC-0130 X ABS, Unreinforced General Purpose Stiff ABS material that is used for battery casesInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 6.35 mm |
1.84 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® LH-0300 ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 6.35 mm |
1.84 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® FD-1112 PC, FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 3.17 mm |
1.84 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® FD-1112 PC, FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.981 J/cm @Temperature 23.0 °C |
1.84 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
SCG Chemicals EL-Proâ„¢ P640J Polypropylene Injection Molding Key Characteristics:Good flowabilityHigh stiffnessHigh impact strengthRecommended Applications:High impact electrical appliance parts, automotive and motorcycle parts such as fan stand, washing tubI.. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 6.40 mm |
1.84 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron KU670M ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Izod Impact, Notched | 0.981 - 1.27 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.84 - 2.39 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Samyang Triel® 5722EM Thermoplastics Polyetherester Elastomer, Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5722EM is an extrusion grade.Information provided by Samyang. |
|||
Izod Impact, Notched | 0.981 - 1.18 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.84 - 2.20 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Samyang Triel® 5700 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5700 is an extrusion grade.Information provided by Samyang. |