Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.020 - 0.0219 cm/cm @Time 86400 sec |
0.020 - 0.0219 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP KL004A Acetal Homopolymer LNP LUBRICOMP* KL004A is a compound based on Acetal Homopolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.022 cm/cm @Time 86400 sec |
0.020 - 0.022 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP KL004A Acetal Homopolymer LNP LUBRICOMP* KL004A is a compound based on Acetal Homopolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.0219 cm/cm @Time 86400 sec |
0.020 - 0.0219 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP KL004AXC Acetal Homopolymer LNP* LUBRICOMP* KL004AXC is a compound based on Acetal Homopolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.022 cm/cm @Time 86400 sec |
0.020 - 0.022 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP KL004AXC Acetal Homopolymer LNP* LUBRICOMP* KL004AXC is a compound based on Acetal Homopolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.025 cm/cm @Time 86400 sec |
0.020 - 0.025 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP KL004U Acetal Copolymer LNP LUBRICOMP* KL004U is a compound based on Acetal Copolymer resin containing 20% PTFE. Added features of this material include: Wear Resistant, UV Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.025 cm/cm @Time 86400 sec |
0.020 - 0.025 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP KL004U Acetal Copolymer (Asia Pacific) LNP Lubricomp* KL004U is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated. This grade was previously found under the LNP* F.. |
|||
Linear Mold Shrinkage, Flow | 0.020 cm/cm @Time 86400 sec |
0.020 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Lubricomp QP003 PA 6/10 LNP* Lubricomp* QP003 is a compound based on Nylon 6/10 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Am.. |
|||
Linear Mold Shrinkage, Flow | 0.020 cm/cm @Time 86400 sec |
0.020 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Lubricomp QP003 PA 6/10 (Asia Pacific) LNP* Lubricomp* QP003 is a compound based on Nylon 6/10 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the As.. |
|||
Linear Mold Shrinkage, Flow | 0.020 cm/cm @Time 86400 sec |
0.020 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Lubricomp RP0049 PA 66 LNP LUBRICOMP* RP0049 is a compound based on Nylon 66 resin containing Flame Retardant, PTFE, Silicone. Added features of this material include: Flame Retardant.This data was supplied by SABIC-IP f.. |
|||
Linear Mold Shrinkage, Flow | 0.020 cm/cm @Time 86400 sec |
0.020 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Lubricomp RP0049 PA 66 LNP LUBRICOMP* RP0049 is a compound based on Nylon 66 resin containing Flame Retardant, PTFE, Silicone. Added features of this material include: Flame Retardant.This data was supplied by SABIC-IP f.. |
|||
Linear Mold Shrinkage, Flow | >= 0.020 cm/cm @Time 86400 sec |
>= 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP WL003 PBT LNP* LUBRICOMP* WL003 is a compound based on PBT resin containing 15% PTFE. Added feature of th is grade is: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | >= 0.020 cm/cm @Time 86400 sec |
>= 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON FX98500C PE (Asia Pacific) LNP* Stat-kon* FX98500C is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | >= 0.020 cm/cm @Time 86400 sec |
>= 0.020 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON FX98500C PE (Asia Pacific) LNP* Stat-kon* FX98500C is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.030 cm/cm @Time 86400 sec |
0.020 - 0.030 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Stat-kon KS302 Acetal Copoly LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | >= 0.020 cm/cm @Time 86400 sec |
>= 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON KS302 Acetal Copoly (Asia Pacific) LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel. |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.024 cm/cm @Time 86400 sec |
0.020 - 0.024 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Stat-loy K3000 Acetal Copoly LNP* Stat-loy* K3000 is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Americas regi.. |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.024 cm/cm @Time 86400 sec |
0.020 - 0.024 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Stat-loy K3000 Acetal Copoly (Asia Pacific) LNP* Stat-loy* K3000 is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Asia Pacific .. |
|||
Linear Mold Shrinkage, Flow | >= 0.020 cm/cm @Time 86400 sec |
>= 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP KFB11 Acetal Copoly LNP* THERMOCOMP* KFB11 is a compound based on Acetal Copolymer resin containing 5% Glass Fiber, 5% Glass Bead. Added features of this material include: Low Warpage, Chemically Coupled. |
|||
Linear Mold Shrinkage, Flow | >= 0.020 cm/cm @Time 86400 sec |
>= 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP KZ001L Acetal Copoly LNP* THERMOCOMP* KZ001L is a compound based on Acetal Copolymer resin containing 5% Milled Glass. Added features of this material include: Low Extractible. |
|||
Linear Mold Shrinkage, Flow | >= 0.020 cm/cm @Time 86400 sec |
>= 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP KZ001L Acetal Copoly (Asia Pacific) LNP* Thermocomp* KZ001L is a compound based on Acetal Copolymer resin containing Glass Fiber. Added features of this material include: Low Extractible. |
|||
Linear Mold Shrinkage, Flow | >= 0.020 cm/cm @Time 86400 sec |
>= 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT LNP* LUBRICOMP* WBL36L is a compound based on PBT resin containing 30% Glass Bead, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible. |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Stat-kon FX97333 PE LNP* Stat-kon* FX97333 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th.. |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Stat-kon FX97333 PE LNP* Stat-kon* FX97333 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th.. |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Stat-kon FX97333 PE (Asia Pacific) LNP* Stat-kon* FX97333 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th.. |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Stat-kon FX97333 PE (Asia Pacific) LNP* Stat-kon* FX97333 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th.. |
|||
Linear Mold Shrinkage, Flow | >= 0.020 cm/cm @Time 86400 sec |
>= 0.020 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON FX98500 PE (Asia Pacific) LNP* Stat-kon* FX98500 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | >= 0.020 cm/cm @Time 86400 sec |
>= 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON RD000IXP PA 66 LNP STAT-KON* RD000IXP is a compound based on Nylon 66 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Linear Mold Shrinkage, Flow | >= 0.020 cm/cm @Time 86400 sec |
>= 0.020 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON QD000I PA 6/10 LNP* STAT-KON* QD000I is a compound based on Nylon 6/10 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Linear Mold Shrinkage, Flow | >= 0.020 cm/cm @Time 86400 sec |
>= 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP KFB11 Acetal Copoly (Asia Pacific) LNP* Thermocomp* KFB11 is a compound based on Acetal Copolymer resin containing Glass Fiber, Milled Glass. Added features of this material include: Low Warpage, Chemically Coupled. |
|||
Linear Mold Shrinkage, Flow | 0.020 cm/cm @Thickness 3.00 mm |
0.020 in/in @Thickness 0.118 in |
ISO 294-4 |
DuPont Performance Polymers Sorona® MT3401 NC010 Polytrimethylene Terephthalate (PTT)