Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 4.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
4.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycolac® FR15 ABS Flame retardant ABS (non-PBBE additive). Good property/toughness. Excellent moldability. UL94 V-0/5VA rated. |
|||
Melt Flow | 4.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers SAN 280 Water Clear Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 300 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 572 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PC 1431 PRE-ELEC PC 1431 is a conductive thermoplastic compound based on polycarbonate. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Melt Flow | 4.0 g/10 min @Load 5.00 kg, Temperature 230 °C |
4.0 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PP 1386 PRE-ELEC PP 1386 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Melt Flow | 4.0 - 6.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.0 - 6.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4435S (35405) Medium Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
PolyOne Dynaflex™ G6703-0001 Thermoplastic Elastomer (TPE) Dynaflex™ G6703-0001 is an easy processing compound designed for use in injection molding applications where extremely soft feel properties are desired. - Excellent Colorability - Good Ozone and UV.. |
|||
Melt Flow | 4.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
4.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® ML3513 PC (Europe-Africa-Middle East) LEXAN ML3513 is a high viscosity, 30% short fibre glass reinforced, flame retardant grade, especially designed for connectors and relay separators.This data was supplied by SABIC-IP for the Europe-A.. |
|||
Melt Flow | 4.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
4.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Geloy XTPM309 ASA+PC (Europe-Africa-Middle East) XTPM309 is a modified HRA170 with improved processing stability.Typical properties measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 4.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
4.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Geloy XTPM309E ASA+PC (Europe-Africa-Middle East) XTPM309E is a high heat resistant ASA+PC. It shows high impact retention, which can be positioned for various outdoor and indoor applications requiring superior heat aging properties and colour stab.. |
|||
Melt Flow | 4.0 - 6.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.0 - 6.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4431S (30405) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 4.0 - 6.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.0 - 6.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4436S (35405) Medium Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 4.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
4.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Polimeri Europa SINKRAL B532 ABS, Very High Impact
(discontinued **) Very high impact; injection/extrusion grade.Information provided by EnichemPolimeri Europa now has Enichem's plastics businesses. This grade is no longer in the product line. |
|||
Melt Flow | 4.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
4.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
Cond I; ASTM D1238 |
Ravago Manufacturing Americas Hylac® GP48 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Melt Flow | 4.0 - 7.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.0 - 7.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
±15% |
Kazanorgsintez PE2NT21-13 High Density Polyethylene Composite Production Method: Copolymerization of eythylene at low pressure in presence of complex catalysts using gaseous-phase method. Application: Composition is intended for injection molding processin.. |
|||
Melt Flow | 4.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 (G) |
LG Chemical HIPS MI750L PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Melt Flow | 4.0 g/10 min @Load 10.0 kg, Temperature 200 °C |
4.0 g/10 min @Load 22.0 lb, Temperature 392 °F |
ISO 1133 |
Kuraray SEPTON® S2007 Thermoplastic Rubber SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi.. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 265 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 509 °F |
ASTM D 1238 |
SABIC Innovative Plastics Xenoy® EXXY0113 PBT (Europe-Africa-Middle East) Blow Moldable Impact modified XENOYThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 250 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 482 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Europe-Africa-Middle East) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 265 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 509 °F |
ASTM D 1238 |
SABIC Innovative Plastics Xenoy® X6800BM PBT Blow moldable, impact modifed XENOYThis data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 4.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
4.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Techmer ES Plastiblend® ABS 8003 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Impact ModifierFeatures: Heat Stabilized and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Comp.. |
|||
Melt Flow | 4.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
4.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM Test |
Styrolution Luran® S 776 SE ASA Luran S 776 SE is a general purpose extrusion ASA grade with good toughness and strength, used for sheet and profile extrusions.Information provided by STYROLUTION, which is a joint venture between .. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 250 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® WP-1041 PC/ABS, Unreinforced Metal Plating Grade High flow PC/ABS material that can be used for automobile R/G door handleInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 250 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® WP-1041 PC/ABS, Unreinforced Metal Plating Grade High flow PC/ABS material that can be used for automobile R/G door handleInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 260 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 500 °F |
ISO 1133 |
Polyplastics TOPAS® 6015 Cyclic Olefin Copolymer (COC) (Asia/Pacific Grade) A similar grade to 6013. However, heat deflection temperature is (HDT/B) = 150°C. This is a temperature that cannot be achieved with many other amorphous polymers.Information provided by PolyPlasti.. |
|||
Melt Flow | 4.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133H |
Total PS CPDS 856 Flame Retardant Polystyrene POLYSTYRENE (PS) COMPOUND (CPDS) 856 is a high impact halogen free polystyrene which offers a good balance of rheological and mechanical properties.Main Characteristics:Bromine and Chlorine free,UL9.. |
|||
Melt Flow | 4.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
4.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D 1238 |
Cossa Polimeri ESTADIENE 1030 HT V0 Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, high thermal resistance, good light resistance, good processability and surface appearanceInformation provided by Cossa Polimeri S.. |
|||
Melt Flow | 4.0 g/10 min @Load 10.0 kg, Temperature 190 °C |
4.0 g/10 min @Load 22.0 lb, Temperature 374 °F |
ExxonMobil Method |
ExxonMobil Pax-Plus™ 3201 Blown Film Resin Pax-Plus 3201 is a rubber modified high density polyethylene film resin that exhibits excellent impact strength and stress crack resistance. It is used primarily in film where its good tear resista.. |
|||
Melt Flow | 4.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers ABS 9500P Injection Molding Grade, Ultra High Impact Powder Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 4.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
4.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
Procedure A; ASTM D1238 |
Diamond Polymers ASA 5946 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High HeatInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 4.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
4.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Hytrel® HTR237BG BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 45 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR237BG is designed for blow molding or processing techniques requiring high viscosity. It has nominal dur.. |