Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 11 g/10 min @Load 21.6 kg, Temperature 190 °C |
11 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
SABIC FI1157 Bimodal High Density Polyethylene for Blown Film Product Description: FI1157 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh.. |
|||
Melt Flow | 11 g/10 min @Load 5.00 kg, Temperature 260 °C |
11 g/10 min @Load 11.0 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycoloy® C4220K PC+ABS (Asia Pacific) Cycoloy* C4220K resin is an injection moldable 20% glass reinforced non FR PC-ABS.
Key features include improved Knit Line strength, good flow, excellent strength & rigidity, heat resistance & hyd.. |
|||
Melt Flow | 11 g/10 min @Load 5.00 kg, Temperature 260 °C |
11 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D 1238 |
SABIC Innovative Plastics Cycoloy® CY100FC PC+ABS (Europe-Africa-Middle East) High impact PC+ABS material designed for local Pacific Automotive applicationsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 11 g/10 min @Load 1.20 kg, Temperature 300 °C |
11 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Cycoloy® EFX810ME PC Modified PC blend offering metallic / sparkle look with minimal flowline visibility.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 11 g/10 min @Load 5.00 kg, Temperature 260 °C |
11 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics GELOY CR8510 ASA ASA with outstanding UV exposure performance for both exterior and interior applications. F1 Rated. |
|||
Melt Flow | 11 g/10 min @Load 1.20 kg, Temperature 300 °C |
11 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® FXE144H PC (Asia Pacific) FXE144H is a Lexan PC Translucent Grade in our VisualFX Portfolio. It is part of Energy family, which includes Illuminate, Glass, and Flame effects. Grade was developed to meet the Aesthetic Differe.. |
|||
Melt Flow | 11 g/10 min @Load 1.20 kg, Temperature 300 °C |
11 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® FXM141R PC FXM141R is a Lexan PC grade in Metallic or Pearlescent effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color .. |
|||
Melt Flow | 11 g/10 min @Load 2.16 kg, Temperature 230 °C |
11 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1183 |
LyondellBasell Moplen HP400N Polypropylene Homopolymer Description: HP400N is a high flow homopolymer with a conventional molecular weight distribution and is formulated with a general-purpose additive package. HP400N is designed for injection molding a.. |
|||
Melt Flow | 11 g/10 min @Load 5.00 kg, Temperature 190 °C |
11 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) I4 HD 7255 High Density Polyethylene HD7255 is a HDPE grade with high impact strength and low warpage.Applications: thick walled, highly stressed transport containers, injection molding.Information provided by Iran Petrochemical Commer.. |
|||
Melt Flow | 11 g/10 min @Load 5.00 kg, Temperature 250 °C |
11 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® ENH8560 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 30% Glass fiber reinforced PBT/PET blend |
|||
Melt Flow | 11 g/10 min @Load 5.00 kg, Temperature 200 °C |
11 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM Test |
Styrolution Styrolux 3G33 SBC Styrolux 3G33 is a thermoplastic styrene-butadiene block copolymer which is suitable for injection molding, extrusion and thermoforming. It offers an outstanding combination of crystal clarity and .. |
|||
Melt Flow | 11 g/10 min @Load 5.00 kg, Temperature 200 °C |
11 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM Test |
Styrolution Styrolux 684D SBC Styrolux 684D is a thermoplastic styrene-butadiene block copolymer which is suitable for injection molding, extrusion, and thermoforming. It offers an outstanding combination of crystal clarity and.. |
|||
Melt Flow | 11 g/10 min @Load 3.80 kg, Temperature 230 °C |
11 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM Test |
Styrolution Terluran® GP-35 ABS Terluran GP-35 is a very high flow grade of ABS for injection molding with good resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF an.. |
|||
Melt Flow | 11 g/10 min @Load 2.16 kg, Temperature 230 °C |
11 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Samyang Triel® 5450 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5450 is an extrusion grade.Information provided by Samyang. |
|||
Melt Flow | 11 g/10 min @Load 2.16 kg, Temperature 240 °C |
11 g/10 min @Load 4.76 lb, Temperature 464 °F |
ASTM D1238 |
Samyang Triel® 5450 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5450 is an extrusion grade.Information provided by Samyang. |
|||
Melt Flow | 11 g/10 min @Load 5.00 kg, Temperature 280 °C |
11 g/10 min @Load 11.0 lb, Temperature 536 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 (Asia Pacific) Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie.. |
|||
Melt Flow | 11 g/10 min @Load 5.00 kg, Temperature 280 °C |
11 g/10 min @Load 11.0 lb, Temperature 536 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 (Europe-Africa-Middle East) Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie.. |
|||
Melt Flow | 11 g/10 min @Load 5.00 kg, Temperature 280 °C |
11 g/10 min @Load 11.0 lb, Temperature 536 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq.. |
|||
Melt Flow | 11 g/10 min @Load 5.00 kg, Temperature 280 °C |
11 g/10 min @Load 11.0 lb, Temperature 536 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Europe-Africa-Middle East) NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq.. |
|||
Melt Flow | 11 g/10 min @Load 5.00 kg, Temperature 220 °C |
11 g/10 min @Load 11.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem HU2410 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications.
Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
Melt Flow | 11 g/10 min @Load 2.16 kg, Temperature 265 °C |
11 g/10 min @Load 4.76 lb, Temperature 509 °F |
ASTM D 1238 |
SABIC Innovative Plastics Xylex FXY391DF PC+POLYESTER (Asia Pacific) PC+Polyester alloy in Diffusion Visual fx. This grade is compliant with US FDA/European food contact regulations. Color package may influence performance.This data was supplied by SABIC-IP for the A.. |
|||
Melt Flow | 11 g/10 min @Load 2.16 kg, Temperature 265 °C |
11 g/10 min @Load 4.76 lb, Temperature 509 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Xylex X7529 PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical quality. UV 400nm block.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
Melt Flow | 11 g/10 min @Load 3.80 kg, Temperature 230 °C |
11 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Diamond Polymers ABS 2100 P Compounding Grade Powder Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 11 g/10 min @Load 3.80 kg, Temperature 230 °C |
11 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Diamond Polymers ABS 3500 HF Injection Molding Grade, High Flow, Medium Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 11 g/10 min @Load 2.16 kg, Temperature 230 °C |
11 g/10 min @Load 4.76 lb, Temperature 446 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Hytrel® G4774 Polyester Elastomer TPC-ET
(Unverified Data**) 47 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4774 is a medium modulus grade with nominal hardness of 47D. It contains discoloring stabilizer. It can be proc.. |
|||
Melt Flow | 11 g/10 min @Load 2.16 kg, Temperature 230 °C |
11 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
DuPont Performance Polymers Hytrel® G4774 Polyester Elastomer TPC-ET
(Unverified Data**) 47 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4774 is a medium modulus grade with nominal hardness of 47D. It contains discoloring stabilizer. It can be proc.. |
|||
Melt Flow | 11 g/10 min @Load 21.6 kg, Temperature 190 °C |
11 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Total XSene® HD55110 High Density Polyethylene - Blown Film HDPE HD55110 is a bimodal high density polyethylene with a particular molecular design developed with Total Petrochemicals Double Loop Technology™.HDPE HD55110 has been especially designed for appl.. |
|||
Melt Flow | 11 g/10 min @Load 1.20 kg, Temperature 300 °C |
11 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® FXE144H PC (Europe-Africa-Middle East) FXE144H is a Lexan PC Translucent Grade in our VisualFX Portfolio. It is part of Energy family, which includes Illuminate, Glass, and Flame effects. Grade was developed to meet the Aesthetic Differe.. |
|||
Melt Flow | 11 g/10 min @Load 2.16 kg, Temperature 265 °C |
11 g/10 min @Load 4.76 lb, Temperature 509 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Xylex X7529OQ PC+POLYESTER (Asia Pacific) PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical qualityThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 11 g/10 min @Load 5.00 kg, Temperature 260 °C |
11 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics GELOY CR7500 ASA High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only. |