Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 25.4 microns | 1.00 mil | |
NOVA Chemicals Novapol® HF-Y450-A Hexene HDPE Film Resin Film Properties. Features: High strength and stiffness, excellent drawdown, used in blends with LDPE/LLDPE for improved film stiffness.Applications: Grease barrier, lamination films, blending resin.. |
|||
Thickness | 25.4 microns | 1.00 mil | |
ExxonMobil Exceed™ 1518EC Tough Premium Film Resin
(discontinued **) Exceed 1518EC resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1518EC resin have outstanding tensile, impact strength and puncture. These superi.. |
|||
Thickness | 25.4 microns | 1.00 mil | |
M. Holland Company MAGMA® LL1091 LLDPE
(discontinued **) Features: Good Heat Seal, Good ToughnessUses: PackagingProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Thickness | 25.4 - 254 microns | 1.00 - 10.0 mil | Average value: 127 microns Grade Count:7 |
Overview of materials for Epoxy, Electrically Conductive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Electrically Conductive". Each property range of values reported is minimum and maximum values of.. |
|||
Thickness | 25.4 microns | 1.00 mil | Interleave |
Arlon A3020-R008-16.5 0.020" (0.508 mm) Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate
&nb 2 inches width and 50 inches long. Design/Construction: Side 1: Cured Fusible Silicone Rubber Substrate: 25% sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester Film Th.. |
|||
Thickness | 25.4 microns | 1.00 mil | |
Total 6410 HDPE Film Resin Unique combination of high stiffness and clarity; Good moisture barrier properties; Good processability; Good compatibility with LDPE and LLDPEApplications: paper overwrap, cup overwrap, plate overw.. |
|||
Thickness | 25.4 microns | 1.00 mil | |
Westlake Hifor Xtreme SC74844 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme SC74844 polymer is a high strength linear low density polyethylene designed for blown film extrusion that contains medium slip, high antiblock and processing aid. Films produce.. |
|||
Thickness | 25.4 microns | 1.00 mil | |
Westlake LF1050 Butene Linear Low Density Polyethylene Westlake LF1050 is a butene LLDPE with high stiffness suitable for cast film extrusion. This material can be used at 100% or as blending stock with LDPE or MDPE.Application/UsesCast film extrusionPr.. |
|||
Thickness | 25.4 microns | 1.00 mil | Nominal; ExxonMobil Method |
ExxonMobil Bicor® 100 LTSC OPP Film Product Description: Bicor LTSC is a two-side coated OPP film which is designed for use in high-speed or demanding horizontal, fin seal, packaging applications. The low-temperature seal coating (LTS.. |
|||
Thickness | 25.4 microns | 1.00 mil | |
ExxonMobil EXACT™ 4151 Plastomer for Cast Film Product Description: Exact 4151 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 4151 is designed for both monolayer multilayer coextru.. |
|||
Thickness | 25.4 microns | 1.00 mil | |
Dow 611A Low Density Polyethylene (LDPE) A shrink film resin with good optics packaging applications Optimum gauge range: 1.0 - 3.0 mil Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow |
|||
Thickness | 25.4 microns | 1.00 mil | 2.5:1 blow-up ratio |
Bapolene® 122B Polyethylene, Film Grade Bapolene LL122B is a general purpose LLDPE for blown film extrusion. This resin offers excellent tensile and toughness properties. Contains no slip and no antiblock additives. This product meets .. |
|||
Thickness | 25.4 microns | 1.00 mil | laminated foil; Arlon SQA-TMS-003 |
Arlon I51576R015 Silicone Rubber/Fiberglass/Alloy Laminate Top layer of side 2: alloy 600 foil; Bottom layer of side 2: cured silicone rubber; Substrate is 7628 fiberglass; Side 1: cured silicone rubber |
|||
Thickness | 25.4 microns | 1.00 mil | Liner |
3M FM0186N Clear Polyester Label Products 3M™ Clear Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is.. |
|||
Thickness | 25.4 microns | 1.00 mil | Liner |
Arlon Thermabond® T20 (99710W008) 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: 8 mil thick Thermabond® T20 electrically insulating electronic adhesive.Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Prim.. |
|||
Thickness | 25.4 microns | 1.00 mil | Facestock |
3M FM078 Indoor UL Recognized Clear Polyester Overlaminate Label Product 3M™ Indoor UL Recognized Matte Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester ov.. |
|||
Thickness | 25.4 microns | 1.00 mil | Facestock |
3M FM282 Indoor UL Recognized White Polyester Label Products 3M™ Indoor UL Recognized White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ A.. |
|||
Thickness | 25.4 microns | 1.00 mil | recommended dry film thickness |
Aremco Aremco-Seal™ 617 High Temperature Glass Coating Glass-filled adhesive/sealer for use with porous ceramics and refractories to 1500 ºF (816 ºC). |
|||
Thickness | 25.4 microns | 1.00 mil | recommended dry film thickness |
Aremco Corr-Paint™ CP4010-S1 High Temperature Protective Coating, Silicone |
|||
Thickness | 25.4 microns | 1.00 mil | recommended dry film thickness |
Aremco Quartz-Coat™ 845 High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, brown-black coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps.. |
|||
Thickness | 25.4 microns | 1.00 mil | Facestock |
3M 8417 Polyester Film Tape 3M™ Polyester Film Tape 8417 is a self-wound (linerless) transparent polyester film coated with 3M™ Adhesive 100 High-temperature Acrylic. It is often used as an overlaminate in conjunction with 3.. |
|||
Thickness | 25.4 microns | 1.00 mil | Interleave |
Arlon T2040-B004 0.040" (1.02 mm) Cured Self-Fusing Silicone Rubber Description: 1 inch wide x 40 mil thick, Black, Triangular cross-section, Self-Fusing Silicone TapeDesign/Construction: Interleave: Polyester Product: Cured Self-Fusing Silicone RubberCross-Section:.. |
|||
Thickness | 25.4 microns | 1.00 mil | Facestock |
3M FM239 Indoor UL Recognized Matte Clear Polyester Label Products 3M™ Indoor UL Recognized Matte Clear Polyester Label Products FM23N, FM232 and FM239 are durable, high performance materials that offer excellent thermal stability and moisture resistance. These po.. |
|||
Thickness | 25.4 microns | 1.00 mil | recommended dry film thickness |
Aremco Cerama-Dip™ 538-N-GRN High Temperature Specialty Ceramic-Inorganic Coating Low viscosity, light gray coating for powder resistors and rheostats to 2600°F (1427°C). black and green pigments also available. |
|||
Thickness | 25.4 microns | 1.00 mil | recommended dry film thickness |
Aremco Lamp-Coat™ LC4040-SG High Temperature Coating, Silicone White reflective coating for use on mercury vapor lamps and other high temperature glass and quartz components to 1200 ºF (649 ºC). |
|||
Thickness | 25.4 microns | 1.00 mil | recommended dry film thickness |
Aremco Quartz-Coat™ 850 High Temperature Specialty Coatings Inorganic, Glass-Ceramic Filled Glass-ceramic, white reflective coating for glass and quartz to 1500°F (816°F) |
|||
Thickness | 25.4 microns | 1.00 mil | Adhesive |
3M 7902 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Thickness | 25.4 microns | 1.00 mil | Adhesive |
3M 7906 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Thickness | 25.4 microns | 1.00 mil | Liner |
3M FV02610N Textured Vinyl Label Products 3M™ Textured Vinyl Label Product FV02610N is a flexible and conformable clear vinyl label stock that offers durability and moisture resistance. This vinyl label utilizes 3M™ Adhesive P1400, which .. |
|||
Thickness | 25.4 microns | 1.00 mil | Liner |
3M OFL010N Outdoor UL Recognized Lexan Label Products 3M™ Outdoor UL Recognized Lexan Label Products are durable, matte clear polycarbonate overlaminates that offer excellent moisture and abrasion resistance. These lexan labels utilize 3M™ Adhesive P.. |