Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon A3020-R008-16.5 0.020" (0.508 mm) Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate &nb

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon A3020-R008-16.5 0.020" (0.508 mm) Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate &nb.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
2 inches width and 50 inches long. Design/Construction: Side 1: Cured Fusible Silicone Rubber Substrate: 25% sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester Film This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 25.4 microns
1.00 mil
Interleave
203 microns
8.00 mil
Substrate; Arlon SQA-TMS-003
508 microns
20.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
Silicone Property; ASTM D2240
Tensile Strength 7.93 MPa
1150 psi
Silicone Property; ASTM D412
31.25 MPa
4533 psi
Product Property; Arlon SQA-TMS-048
Elongation at Break 34 %
34 %
Tape Property; Arlon SQA-TMS-048
430 %
430 %
Silicone Property; ASTM D412
Tear Strength 15.8 kN/m
90.0 pli
Die B, Silicone Property; ASTM D624
Peel Strength 1.05 kN/m
6.00 pli
Adhesion Strength, Tape Property; Arlon SQA-TMS-047
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 26.6 kV/mm
675 kV/in
Tape Property; ASTM D149
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 21.1 °C
12.0 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Off White
Substrate
Red
Users viewing this material also viewed the following: