Aremco Cerama-Dip™ 538-N-GRN High Temperature Specialty Ceramic-Inorganic Coating

Category Ceramic , Oxide , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Aremco
Trade Name Cerama-Dip™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco Cerama-Dip™ 538-N-GRN High Temperature Specialty Ceramic-Inorganic Coating.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Low viscosity, light gray coating for powder resistors and rheostats to 2600°F (1427°C). black and green pigments also available.
Physical Properties Metric English Comments
Specific Gravity 1.68 g/cc
1.68 g/cc
Solids Content 39.8 %
39.8 %
by volume
62.9 %
62.9 %
by weight
Volatile Organic Compounds (VOC) Content 0.00 g/l
0.00 g/l
Viscosity 2000 - 2500 cP
2000 - 2500 cP
Brooksfield LV Viscometer
Thickness 25.4 microns
1.00 mil
recommended dry film thickness
63.8 microns
2.51 mil
estimated wet film thickness
Storage Temperature 12.8 - 30.0 °C
55.0 - 86.0 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1430 °C
2600 °F
Continuous
Electrical Properties Metric English Comments
Dielectric Strength 5.59 kV/mm
142 kV/in
Processing Properties Metric English Comments
Dry Time 1 hour
1 hour
Touch
1 hour
1 hour
Handling
Cure Time >= 60.0 min
>= 1.00 hour
Air Set prior to curing
180 - 360 min
3.00 - 6.00 hour
2-4 hr at 200°F followed by 1-2 hr at 350°F
Shelf Life 6.0 Month

@Temperature 12.8 - 29.4 °C
6.0 Month

@Temperature 55.0 - 85.0 °F
Descriptive Properties Value Comments
Application Temperature 50 - 90°F
Color Green
Dry Film Coverage ft2/gal 639
at 1 mil
Thinner 538-N-T