Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon T2040-B004 0.040" (1.02 mm) Cured Self-Fusing Silicone Rubber

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon T2040-B004 0.040" (1.02 mm) Cured Self-Fusing Silicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: 1 inch wide x 40 mil thick, Black, Triangular cross-section, Self-Fusing Silicone TapeDesign/Construction: Interleave: Polyester Product: Cured Self-Fusing Silicone RubberCross-Section: Triangular Appearance: Black silicone rubber on polymer linerThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Arlon SQA-TMS-024
Water Absorption 0.10 %
0.10 %
Arlon SQA-TMS-016
Thickness 25.4 microns
1.00 mil
Interleave
1020 microns
40.0 mil
Overall; Arlon SQA-TMS-012
Mechanical Properties Metric English Comments
Hardness, Shore A 49
49
ASTM D2240
Tensile Strength 8.522 MPa
1236 psi
ASTM D412
Elongation at Break 716 %
716 %
ASTM D412
Tear Strength 28.0 kN/m
160 pli
ASTM D624
Peel Strength 0.491 kN/m
2.80 pli
Bond Strength; Arlon SQA-TMS-015
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 20.1 kV/mm
511 kV/in
ASTM D149
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 21.1 °C
12.0 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Black