Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Epoxy, Electrically Conductive

Category Polymer , Thermoset , Epoxy , Epoxy, Electrically Conductive
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Epoxy, Electrically Conductive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Electrically Conductive". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.940 - 5.30 g/cc
0.0340 - 0.191 lb/in³
Average value: 2.75 g/cc Grade Count:96
Volatile Organic Compounds (VOC) Content 0.000 - 591 g/l
0.000 - 591 g/l
Average value: 88.7 g/l Grade Count:7
Solubility in Water 0.000 %
0.000 %
Average value: 0.000 % Grade Count:4
Particle Size 2.00 - 50.0 µm
2.00 - 50.0 µm
Average value: 30.4 µm Grade Count:43
Viscosity 220 - 2.50e+6 cP
220 - 2.50e+6 cP
Average value: 93400 cP Grade Count:78
Thickness 25.4 - 254 microns
1.00 - 10.0 mil
Average value: 127 microns Grade Count:7
Mechanical Properties Metric English Comments
Hardness, Shore A 55.0 - 93.0
55.0 - 93.0
Average value: 71.0 Grade Count:6
Hardness, Shore D 19.0 - 90.0
19.0 - 90.0
Average value: 75.9 Grade Count:69
Elongation at Break 0.200 - 60.0 %
0.200 - 60.0 %
Average value: 35.0 % Grade Count:5
Modulus of Elasticity 0.146 - 7.87 GPa
21.2 - 1140 ksi
Average value: 3.89 GPa Grade Count:41
Shear Strength 4.48 - 35.2 MPa
650 - 5100 psi
Average value: 14.2 MPa Grade Count:58
9.65266 - 11.0316 MPa

@Temperature 65.6 - 116 °C
1400.00 - 1600.00 psi

@Temperature 150 - 240 °F
Average value: 10.1 MPa Grade Count:3
9.65266 - 11.0316 MPa

@Time 900 - 7200 sec
1400.00 - 1600.00 psi

@Time 0.250 - 2.00 hour
Average value: 10.1 MPa Grade Count:3
Adhesive Bond Strength 0.621 - 39.3 MPa
90.0 - 5700 psi
Average value: 8.98 MPa Grade Count:51
Peel Strength 0.877 - 3.51 kN/m
5.00 - 20.0 pli
Average value: 2.48 kN/m Grade Count:6
Thermal Properties Metric English Comments
CTE, linear 4.50 - 280 µm/m-°C
2.50 - 156 µin/in-°F
Average value: 78.7 µm/m-°C Grade Count:69
Thermal Conductivity 0.550 - 29.0 W/m-K
3.82 - 201 BTU-in/hr-ft²-°F
Average value: 2.78 W/m-K Grade Count:72
10.9 - 23.0 W/m-K

@Temperature 150 - 150 °C
75.6 - 160 BTU-in/hr-ft²-°F

@Temperature 302 - 302 °F
Average value: 17.0 W/m-K Grade Count:1
10.9 - 23.0 W/m-K

@Time 3600 - 3600 sec
75.6 - 160 BTU-in/hr-ft²-°F

@Time 1.00 - 1.00 hour
Average value: 17.0 W/m-K Grade Count:1
Maximum Service Temperature, Air -150 - 538 °C
-238 - 1000 °F
Average value: 198 °C Grade Count:111
Minimum Service Temperature, Air -269 - -20.0 °C
-452 - -4.00 °F
Average value: -66.1 °C Grade Count:93
Glass Transition Temp, Tg -5.00 - 155 °C
23.0 - 311 °F
Average value: 74.0 °C Grade Count:80
Decomposition Temperature 316 - 478 °C
601 - 892 °F
Average value: 397 °C Grade Count:43
Flash Point 7.22 - 150 °C
45.0 - 302 °F
Average value: 105 °C Grade Count:7
Component Elements Properties Metric English Comments
Carbon, C 4.40 - 69.0 %
4.40 - 69.0 %
Average value: 22.5 % Grade Count:10
Silver, Ag 40.0 - 85.0 %
40.0 - 85.0 %
Average value: 66.3 % Grade Count:4
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000800 ohm-cm - 1e+05
0.0000800 ohm-cm - 1e+05
Average value: 0.0736 ohm-cm Grade Count:105
0.000300 - 0.00200 ohm-cm

@Temperature 65.0 - 150 °C
0.000300 - 0.00200 ohm-cm

@Temperature 149 - 302 °F
Average value: 0.00364 ohm-cm Grade Count:2
<= 0.0100 ohm-cm

@Temperature 65.6 - 150 °C
<= 0.0100 ohm-cm

@Temperature 150 - 302 °F
Average value: 0.00364 ohm-cm Grade Count:5
<= 0.0100 ohm-cm

@Time 900 - 10800 sec
<= 0.0100 ohm-cm

@Time 0.250 - 3.00 hour
Average value: 0.00364 ohm-cm Grade Count:5
Surface Resistance 0.0100 - 6.00e+6 ohm
0.0100 - 6.00e+6 ohm
Average value: 436000 ohm Grade Count:18
Processing Properties Metric English Comments
Processing Temperature 65.0 - 165 °C
149 - 329 °F
Average value: 106 °C Grade Count:5
Cure Time 1.00 - 10100 min
0.0167 - 168 hour
Average value: 1950 min Grade Count:63
0.750 - 1440 min

@Temperature 40.0 - 302 °C
0.0125 - 24.0 hour

@Temperature 104 - 576 °F
Average value: 81.6 min Grade Count:121
Pot Life 10.0 - 130000 min
10.0 - 130000 min
Average value: 5130 min Grade Count:105
2880 - 2880 min

@Temperature 5.00 - 5.00 °C
2880 - 2880 min

@Temperature 41.0 - 41.0 °F
Average value: 2880 min Grade Count:1
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved