Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® FF D0 Very Low Density Polyethylene Clearflex FF D0 is a linear low density polyethylene, with antioxidants, suitable for blown film technology.Films made with Clearflex FF D0 are highly transparent, have excellent sealing properties,.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® FG 308 Octene Copolymer Linear Low Density Polyethylene Clearflex FG 308 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidant and processing aid, suitable for blown film extrusion.Films manufactured with Clearflex FG 308 ar.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® FG B3 Very Low Density Polyethylene Clearflex FG B3 is a linear low density polyethylene, with antioxidants, slip and antiblocking agents, suitable for blown film technology. The product is characterized by a very low density and a h.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® FH 50 Linear Medium Density Polyethylene Clearflex FH 50 is a linear medium density polyethylene, with antioxidants, suitable for blown film extrusion.Films manufactured with Clearflex FH 50 are characterized by a good balance between toug.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® H&T FGH 196 Hexene Copolymer Linear Low Density Polyethylene Clearflex H&T FGH 196 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films obtained from Clearflex H&T FGH .. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® H&T FHH 508 Octene Copolymer Linear Medium Density Polyethylene Clearflex H&T FHH 508 is an octene copolymer linear medium density polyethylene (C8-LMDPE), with antioxidant, suitable for blown film extrusion.Films obtained from Clearflex H&T FHH 508 show good op.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® H&T LFH 208 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T LFH 208 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films obtained from Clearflex H&T LFH.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® H&T LFH 238 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T LFH 238 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion. It contains slip and antiblocking a.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Eraclene® FA 706 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion Eraclene FA 706 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Films manufactured with Eraclene FA 706 show good processability t.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Eraclene® FB 506 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion Eraclene FB 506 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Its broad molecular weight distribution and density successfully c.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® FF 106 Hexene Copolymer Linear Low Density Polyethylene Clearflex FF 106 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Clearflex FF 106 are characterized by .. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® FF 508 Octene Copolymer Linear Medium Density Polyethylene Clearflex FF 508 is an octene copolymer linear medium density polyethylene (C8-LMDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films manufactured with Clearflex FF 50.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® FG B0 Very Low Density Polyethylene Clearflex FG B0 is a linear low density polyethylene, with antioxidants, suitable for blown film technology.Films made with Clearflex FG B0 are highly transparent, have good sealing properties, even.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® H&T LGH 138 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T LGH 138 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants, slip agent, antiblocking and processing aid, suitable for blown film extrusion.Films obtai.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Flexirene® CL 10 Butene Copolymer Linear Low Density Polyethylene Flexirene CL 10 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for cast extrusion of thin film with high optical properties.Main Applications: Flexire.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Average value: 32.1 microns Grade Count:41 |
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Butene, Film This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Butene, Film". Each property range of values reported is minimum.. |
|||
Thickness | 10.0 - 75.0 microns | 0.394 - 2.95 mil | Average value: 25.4 microns Grade Count:88 |
Overview of materials for High Density Polyethylene (HDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max.. |
|||
Thickness | 10.0 - 14.0 microns | 0.394 - 0.551 mil | Fired |
Lord Adhesives Metech 3288 Silver Conductor This product is a silver paste composition designed for screen print application of a solderable electrode base onto various types of electrical ceramic component devices. The fired film forms a hig.. |
|||
Thickness | 10.0 - 13.0 microns | 0.394 - 0.512 mil | Fired |
Lord Adhesives Metech 3615 Platinum Gold Conductor Composition Platinum gold conductor composition 3615 is a mixed bond conductor designed for military, aerospace, and other high reliability applications that require soldered connections. This composition is de.. |
|||
Thickness | 10.0 - 15.0 microns | 0.394 - 0.591 mil | Fired |
Lord Adhesives Metech 7806A Cermet Resistor Overglaze Composition Resistor overglaze composition 7806A is an acid resistant, laser trimable glaze designed to be printed and fired over thick film resistors. 7806A improves the stability of laser or air-abrasive trim.. |
|||
Thickness | 10.0 - 30.0 microns | 0.394 - 1.18 mil | |
Möller Medical TafSkin 103 NanoCoating Highly flexible, non-abrasive, chemical-resistant PTFE coating with very good easy-to-clean properties, biocompatible.Information provided by Möller Medical, Member of CENTROTEC Group |
|||
Thickness | 10.0 microns | 0.394 mil | Cured, Printed through 230 stainless steel mesh with 13 micron emulsion |
Gwent Electronic Materials C2000511D1 Platinized Carbon Ink Platinised Carbon Ink is designed to be used for screen printing working electrodes. It has been optimized to give superior electrochemical performance and designed to be used for printing working e.. |
|||
Thickness | 10.0 - 30.0 microns | 0.394 - 1.18 mil | cured |
Gwent Electronic Materials C2121119D9 Nanocopper based Paste This product is a nanocopper based paste that is designed for flat bed screens. The product is compatible with printing on PET substrates such as the DuPont Melinex ST-505. Produced using nano-par.. |
|||
Thickness | >= 10.0 microns | >= 0.394 mil | DIN 53353 |
Stanelco Bioplast® GF 106 Biodegradable Plastic Bioplast 106 is a versatile soft product, suitable for blown film extrusion of completely biodegradable products. Many customers find it is a natural replacement for LDPE. Made from potato starch m.. |
|||
Thickness | 10.0 microns | 0.394 mil | |
Applied Nanostructured Solutions Carbon NanoStructure Encapsulated Flakes Carbon NanoStructure (CNS) Encapsulated Flakes are a unique form of carbon nanotubes, produced using a proprietary ANS process. The ANS process creates cross-linked multiwall carbon nanotube-based n.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® H&T LGH 108 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T LGH 108 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films obtained from Clearflex H&T LGH.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Eraclene® FA 506 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion Eraclene FA 506 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Its broad molecular weight distribution and density successfully c.. |
|||
Thickness | 10.0 microns | 0.394 mil | Cured Film Thickness on 175µm ITO coated polyester |
Gwent Electronic Materials C2090210P12 Silver Ink This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera.. |
|||
Thickness | 10.0 microns | 0.394 mil | Cured, Printed through 230 stainless steel mesh with 13 micron emulsion |
Gwent Electronic Materials C2000802P2 Carbon Graphite Ink This product is designed to be used for screen-printing working electrodes. This ink has been optimized to give superior electrochemical performance. It combines good line definition and good electr.. |