Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 34 g/10 min @Load 2.16 kg, Temperature 230 °C |
34 g/10 min @Load 4.76 lb, Temperature 446 °F |
Procedure A; ASTM D1238 |
PolyOne Maxxam™ DP-9162-3 Polypropylene, Unspecified (PP, Unspecified) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Melt Flow | 34 g/10 min @Load 2.16 kg, Temperature 230 °C |
34 g/10 min @Load 4.76 lb, Temperature 446 °F |
Procedure A Condition L; ASTM D1238 |
Network Polymers NPP 20-3401 NC Description: Random Copolymer Polypropylene, Non ClarifiedInformation provided by Network Polymers Inc. |
|||
Melt Flow | 34 g/10 min @Load 2.16 kg, Temperature 260 °C |
34 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® CY5000 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Melt Flow | 34 g/10 min @Load 2.16 kg, Temperature 260 °C |
34 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® RCY6013 PC+ABS (Asia Pacific) Cycoloy* RCY6013 resin is an injection moldable high flow PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 30% post consumer recycle content with a UL-94 V0 @ 1.5 mm.. |
|||
Melt Flow | 34 g/10 min @Load 2.16 kg, Temperature 230 °C |
34 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Radici Heraflex® E 4718 TPC-ET Thermoplastic Elastomer TPC-ET Thermoplastic Elastomer. Low Modulus, Nominal Shore D/15s 43. Natural colorProcessing technology: Injection moldingInformation provided by Radici group. |
|||
Melt Flow | 34 g/10 min @Load 2.16 kg, Temperature 230 °C |
34 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
PolyMirae Moplen HP562S Fiber (Spunbond) Grade Polypropylene Moplen HP562S is the controlled rheology polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP562S is a homopolymer particularly suitable f.. |
|||
Melt Flow | 34 g/10 min | 34 g/10 min | ISO 1133 |
Solvay Engineered Polymers SEQUEL® 1490 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 1490 engineered polyolefin material is designed for automotive exterior applications that require a combination of stiffness, low-temperature impact resistance, and excellent p.. |
|||
Melt Flow | 34 g/10 min @Load 2.16 kg, Temperature 230 °C |
34 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Radici Heraflex® E 3918 TPC-ET Thermoplastic Elastomer TPC-ET Thermoplastic Elastomer. Lowest Modulus, Nominal Shore D/15s 35. Natural colorProcessing technology: Injection moldingInformation provided by Radici group. |
|||
Melt Flow | 34 g/10 min @Load 3.80 kg, Temperature 260 °C |
34 g/10 min @Load 8.38 lb, Temperature 500 °F |
ASTM D1238 |
Ravago Manufacturing Americas Hybrid B2035I Polycarbonate + PBT Alloy Available in North America High Impact Resistance Form: PelletsInformation provided by Ravago |
|||
Melt Flow | 34 g/10 min @Load 10.0 kg, Temperature 220 °C |
34 g/10 min @Load 22.0 lb, Temperature 428 °F |
Estimated using room temperature density |
Ineos ABS Lustran® M202AS Grade for self coloring, optimized base color, easy flowing, contains antistatic additives. ,Property data per ISO test methods. |
|||
Melt Flow | 34 g/10 min @Load 2.16 kg, Temperature 230 °C |
34 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LG Chemical SEETEC H7700 Polypropylene, Homopolymer Features: Seetec H7700 is designed for the extrusion of fine fibers with the spunbond technology. This grade is characterized by very narrow molecular weight distribution (MWD), with anti-gas fading.. |
|||
Melt Flow | 34 g/10 min @Load 2.16 kg, Temperature 230 °C |
34 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
Kuraray SEPTON® PM3 Polypropylene Modified Plastic Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are a series of hydrogenated styrenic blo.. |
|||
Melt Flow | 34 g/10 min @Load 2.16 kg, Temperature 260 °C |
34 g/10 min @Load 4.76 lb, Temperature 500 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Pocan® B 3215 Z 000000 PBT, 10% Glass Fiber PBT, 10% glass fibers, injection molding, impact modified |
|||
Melt Flow | 34 g/10 min @Load 2.16 kg, Temperature 260 °C |
34 g/10 min @Load 4.76 lb, Temperature 500 °F |
ISO 1133-1 |
Lanxess Pocan® B 5220 XF 000000 PBT, 20% Glass Spheres PBT, 20% glass spheres, injection molding, improved flowability, improved impact strength, low tendency to warpInformation provided by LANXESS. |
|||
Melt Flow | 34 g/10 min @Load 5.00 kg, Temperature 260 °C |
34 g/10 min @Load 11.0 lb, Temperature 500 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Pocan® S 1517 000000 PBT PBT, non-reinforced, injection molding, extrusion, impact modified |
|||
Melt Flow | 34 g/10 min @Load 5.00 kg, Temperature 270 °C |
34 g/10 min @Load 11.0 lb, Temperature 518 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Pocan® T 3150 XF 000000 PBT + PET, 55% Glass Fiber PBT+PET, 55% glass fibers, injection molding, improved flowability, low tendency to warp, increased temperature peak load, increased strength and increased modulus |
|||
Melt Flow | 34 g/10 min @Load 2.16 kg, Temperature 230 °C |
34 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
LyondellBasell Pro-faxâ„¢ PH835 Polypropylene Homopolymer Description: Pro-faxâ„¢ PH835 is a very high melt flow, controlled rheology polypropylene homopolymer resin designed for spunbond and continuous filament applications that require superior spinna.. |
|||
Melt Flow | 34 g/10 min | 34 g/10 min | ASTM D1238 |
LyondellBasell Alathon® H5234 High Density Polyethylene ApplicationsALATHON H 5234 is a high flow injection molding grade of resin designed for fast cycle and thin wall molding. It provides cold temperature impact resistance. Typical applications inclu.. |
|||
Melt Flow | 34 - 40 g/10 min @Load 5.00 kg, Temperature 365 °C |
34 - 40 g/10 min @Load 11.0 lb, Temperature 689 °F |
ASTM D1238 |
Solvay Specialty Polymers Radel® R-5600 Polyphenylsulfone (PPSU) Radel® R-5600 is a very high melt flow grade of Radel® polyphenylsulfone (PPSU). It is especially well-suited for parts requiring long flow length with thin walls. Radel® resins offer excep.. |
|||
Melt Flow | 34 g/10 min @Load 1.20 kg, Temperature 300 °C |
34 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Samyang Trirex® 3017PJ Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3017PJ is a super high flow grade.Information provided by Samyang. |
|||
Melt Flow | 34 g/10 min @Load 2.16 kg, Temperature 230 °C |
34 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
SABIC Innovative Plastics LNP THERMOCOMP M7002XXH PP LNP* THERMOCOMP* M7002XXH is a compound based on Polypropylene resin containing proprietary antimicrobial additives. Designed for touch surfaces in healthcare applications. Added features include:.. |
|||
Melt Flow | 34 g/10 min @Load 1.20 kg, Temperature 300 °C |
34 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Samyang Trirex® 3017IR Polycarbonate with Heat Stabilizer PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3017IR is a super high flow grade with added heat stabilizers, separating materials and.. |
|||
Melt Flow | 34 g/10 min @Load 2.16 kg, Temperature 230 °C |
34 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 1930-01 Polypropylene Copolymer Polypropylene DescriptionPolypropylene PP 1930-01 is an automotive recognized copolymer polypropylene for use on interior trim applications.Information provided by A. Schulman. |
|||
Melt Flow | 34 g/10 min @Load 10.0 kg, Temperature 220 °C |
34 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Ter Hell Plastic Terez® ABS 3320 A UV Acrylonitrile Butadiene Styrene Rapid flowing ABS with high impact strength, antistatic agent and UV stabilizer.Application: For all kinds of injection molding thin-walled parts.Information provided by Ter Hell Plastic GMBH. |
|||
Melt Flow | 34 g/10 min @Load 2.16 kg, Temperature 230 °C |
34 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 1930-01 Polypropylene Copolymer Polypropylene DescriptionPolypropylene PP 1930-01 is an automotive recognized copolymer polypropylene for use on interior trim applications.Information provided by A. Schulman. |
|||
Melt Flow | 34 g/10 min @Load 2.16 kg, Temperature 230 °C |
34 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 1930-01 Polypropylene Copolymer Polypropylene DescriptionPolypropylene PP 1930-01 is an automotive recognized copolymer polypropylene for use on interior trim applications.Information provided by A. Schulman. |
|||
Melt Flow | 34 g/10 min @Load 2.16 kg, Temperature 230 °C |
34 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 1930-01 Polypropylene Copolymer Polypropylene DescriptionPolypropylene PP 1930-01 is an automotive recognized copolymer polypropylene for use on interior trim applications.Information provided by A. Schulman. |
|||
Melt Flow | 34 g/10 min @Load 2.16 kg, Temperature 230 °C |
34 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 1930-01 Polypropylene Copolymer Polypropylene DescriptionPolypropylene PP 1930-01 is an automotive recognized copolymer polypropylene for use on interior trim applications.Information provided by A. Schulman. |
|||
Melt Flow | 34 g/10 min @Load 2.16 kg, Temperature 230 °C |
34 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LG Chemical SEETEC R7700 Polypropylene, Random Copolymer Features: Seetec R7700 is designed for the extrusion of fibers with the spunbond technology. This grade is characterized by narrow MWD and good processability. SEETEC R7700 meets the FDA requirement.. |
|||
Melt Flow | 34 g/10 min | 34 g/10 min | Melt Flow Ratio (I10/I2) is 7.3; ASTM D1238 |
Huntsman Rexell® H2104 Injection Molding LLDPE
(discontinued **) Linear-low high density homopolymer, injection molding, FDA compliant.Features: High flow and short cycle times.Applications: Thin wall containers.FDA Notes: Conforms to FDA regulation 21 CFR 177.15.. |