Material Notes:
Rapid flowing ABS with high impact strength, antistatic agent and UV stabilizer.Application: For all kinds of injection molding thin-walled parts.Information provided by Ter Hell Plastic GMBH.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ISO 1183
Water Absorption 0.95 %
0.95 %
ISO 62
Melt Flow 34 g/10 min

@Load 10.0 kg,
Temperature 220 °C
34 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength 60.0 MPa
8700 psi
dry; ISO 527
Tensile Strength, Yield 44.0 MPa
6380 psi
dry; ISO 527
Elongation at Break 12 %
12 %
dry; ISO 527
Elongation at Yield 2.4 %
2.4 %
dry; ISO 527
Tensile Modulus 2.30 GPa
334 ksi
dry; ISO 527
Charpy Impact Unnotched 12.5 J/cm²
59.5 ft-lb/in²
dry; ISO 179
Charpy Impact, Notched 1.90 J/cm²
9.04 ft-lb/in²
dry; ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °C
210 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 94.0 °C
201 °F
ISO 75
Vicat Softening Point 95.0 °C
203 °F
B/50; ISO 306
Flammability, UL94 HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
IEC 60093
Processing Properties Metric English Comments
Drying Temperature 80.0 °C
176 °F
Dry Time 2 - 4 hour
2 - 4 hour