SABIC Innovative Plastics LNP THERMOCOMP M7002XXH PP

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP M7002XXH PP.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* THERMOCOMP* M7002XXH is a compound based on Polypropylene resin containing proprietary antimicrobial additives. Designed for touch surfaces in healthcare applications. Added features include: low antimicrobial performance, high mechanical strength, healthcare.
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
ASTM D792
Moisture Absorption 0.0100 %
0.0100 %
50% RH, 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0050 cm/cm

@Time 86400 sec
0.0050 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0070 cm/cm

@Time 86400 sec
0.0070 in/in

@Time 24.0 hour
ASTM D955
Melt Flow 34 g/10 min

@Load 2.16 kg,
Temperature 230 °C
34 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 36.0 MPa
5220 psi
5 mm/min; ISO 527
38.0 MPa
5510 psi
Type I, 5 mm/min; ASTM D638
Tensile Modulus 1.80 GPa
261 ksi
1 mm/min; ISO 527
1.85 GPa
268 ksi
5 mm/min; ASTM D638
Flexural Strength 35.0 MPa
5080 psi
ISO 178
Flexural Yield Strength 40.0 MPa
5800 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 1.25 GPa
181 ksi
2 mm/min; ISO 178
1.40 GPa
203 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.280 J/cm
0.525 ft-lb/in
ASTM D256
Izod Impact, Notched (ISO) 2.00 kJ/m²
0.952 ft-lb/in²
80*10*4; ISO 180/1A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
115 °C

@Thickness 3.20 mm
239 °F

@Thickness 0.126 in
unannealed; ASTM D648