Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kuraray SEPTON® PM3 Polypropylene Modified Plastic

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber , Polypropylene (PP)
Manufacturer Kuraray Company
Trade Name SEPTON®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kuraray SEPTON® PM3 Polypropylene Modified Plastic.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are a series of hydrogenated styrenic block copolymers, which exhibit rubber-like properties over a wide range of temperatures. SEPTON®'s characteristics include:Excellent Mechanical PropertiesGood WeatherabilityExcellent Low Temperature PropertiesExcellent Electrical PropertiesSuperior Heat ResistanceExcellent Chemical ResistanceLow ToxicitySEPTON® grades are available with a range of Shore A hardness of 35-95 and tensile strengths of 290-5600 psi. SEPTON® resins are highly extendible with fillers, resins and oils, which allows formulation of a variety of hardness for adhesives, sealants and various compounds. As an additive, SEPTON® resins can be used to improve toughness of a variety of plastics. Several SEPTON® grades have U.S. FDA and USP Class VI approval.SEPTON® has a versatile series of grades which can be used in numerous processing techniques such as blow molding, injection molding, extrusion, hot melt and solution coatings. SEPTON® resins are thermoplastics therefore, the scrap is recyclable without significant loss of properties.Formulation (parts by weight): PP (Block Copolymer) - 80, SEPTON® 2002 - 20Information provided by The Kuraray Group.
Physical Properties Metric English Comments
Melt Flow 34 g/10 min

@Load 2.16 kg,
Temperature 230 °C
34 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Mechanical Properties Metric English Comments
Flexural Modulus 0.615 GPa
89.2 ksi
Izod Impact, Notched 6.29 J/cm
11.8 ft-lb/in
1.70 J/cm

@Temperature -20.0 °C
3.18 ft-lb/in

@Temperature -4.00 °F
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved