Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 14 g/10 min | 14 g/10 min | ASTM D1238 |
Multibase Multi-Pro® 3014 CUW Polypropylene Calcium Carbonate Filler, 30% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 230 °C |
14 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products T40P250-00 40% Talc Reinforced Polypropylene Copolymer, Natural Applications: BracketsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 260 °C |
14 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® FXC630ME PC+ABS (Asia Pacific) PC+ABS, ECO-conforming flame retardant with metallic or pearlescent appearance. |
|||
Melt Flow | 14 - 20 g/10 min @Load 1.20 kg, Temperature 300 °C |
14 - 20 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-FD3 Polycarbonate, FDA-compliant Feedstocks, High Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, High Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Melt Flow | 14 - 20 g/10 min @Load 1.20 kg, Temperature 300 °C |
14 - 20 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-GP3-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, High Flow Polycarbonate, FDA-compliant Feedstocks, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Melt Flow | 14 - 20 g/10 min @Load 1.20 kg, Temperature 300 °C |
14 - 20 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-GP3-TFE10 Polycarbonate, 10% PTFE, High Flow, Wear Resistant Polycarbonate, General Purpose, High Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Melt Flow | 14 g/10 min | 14 g/10 min | ISO 1133 |
Solvay Engineered Polymers SEQUEL® 1820 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 1820 engineered polyolefin is designed for automotive exterior applications that require energy management combined with excellent ductility and stiffness over a broad temperat.. |
|||
Melt Flow | 14 g/10 min @Load 5.00 kg, Temperature 260 °C |
14 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® CP8320 PC+ABS (Europe-Africa-Middle East) Cycoloy Medium Heat Plating Grade for Automotive |
|||
Melt Flow | 14 g/10 min @Load 5.00 kg, Temperature 200 °C |
14 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers NPS 80-1410 Polystyrene Description: Injection Molding Grade, Medium Impact, High Melt FlowInformation provided by Network Polymers Inc. |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 190 °C |
14 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® FG500TL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG500TL medium viscosity acetal homopolymer resin containing 1.5% Teflon® PTFE Micropowder. It has been developed for consideration into applications such as parts for the food industry.In.. |
|||
Melt Flow | 14 g/10 min | 14 g/10 min | ASTM D1238 |
Kolon KOCETAL® K500 Standard Grade Acetal Resin General injection molding grade. Easy flow grade for hard-to fill molds and mechanical thin-wall parts.Applications: General injection molding products.Information provided by API-Kolon. |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 230 °C |
14 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Inno-Comp INNOPOL® CS 2-3302 TO BU Elastomer Modified, UV-Stabilized Polypropylene Block-Copolymer INNOPOL® CS 2-3302 TO BU is an elastomer modified, UV-stabilized compound based on polypropylene block-copolymer.INNOPOL® CS 2-3302 TO BU is developed for producing injection molded automotive.. |
|||
Melt Flow | 14 g/10 min @Load 5.00 kg, Temperature 200 °C |
14 g/10 min @Load 11.0 lb, Temperature 392 °F |
|
Kraton® D1193 P (SIS) Linear Triblock Copolymer Description: Kraton D1193 P is a clear, linear triblock copolymer based on styrene and isoprene, with a polystyrene content of 24%. It is supplied from North America in the physical form identified:.. |
|||
Melt Flow | 14 g/10 min @Load 5.00 kg, Temperature 280 °C |
14 g/10 min @Load 11.0 lb, Temperature 536 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Durethan® AKV 30 HR H2.0 901510 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, hydrolysis stabilized, good heat-ageing resistance |
|||
Melt Flow | 14 g/10 min @Load 5.00 kg, Temperature 250 °C |
14 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Xenoy® CL100 PBT+PC Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom.. |
|||
Melt Flow | 14 g/10 min @Load 1.00 kg, Temperature 190 °C |
14 g/10 min @Load 2.20 lb, Temperature 374 °F |
ASTM D1238R |
UBE PAE1200U2 Electronic Grade Nylon Elastomer Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 190 °C |
14 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Orange 1096 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 1096 is an orange color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 1096 is he.. |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 190 °C |
14 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Red 5505 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 5505 is a red color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 5505 is heavy .. |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 190 °C |
14 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Green 3251V Concentrate Based In Polyethylene DescriptionPOLYBATCH® 3251V is a green color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 3251V conta.. |
|||
Melt Flow | 14 g/10 min @Load 5.00 kg, Temperature 265 °C |
14 g/10 min @Load 11.0 lb, Temperature 509 °F |
cm³/10 min. |
Covestro Makroblend® EL-700 Polycarbonate + Polyester Blend Key Features:Flame retarding agentUnfilledHigh impact or high impact modifiedLight stabilized or stable to lightSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As.. |
|||
Melt Flow | 14 g/10 min @Load 5.00 kg, Temperature 260 °C |
14 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Covestro Makroblend® KU 2-7608 Polycarbonate + PBT, Mineral Filled Impact Grade ISO 7792-1-PC/PBT,MHPR,-030,MD10(PC+PBT)-blendsimpact modifiedInjection molding grade 10% mineral filledPreprocessingMax. Water content |
|||
Melt Flow | 14 g/10 min @Load 10.0 kg, Temperature 220 °C |
14 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D-1238 |
Bhansali Engineering Abstron IM-11G ABS Injection Molding Grade High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 190 °C |
14 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont™ Surlyn® 1702 Zinc Ionomer Resin for Extrusion Coating Surlyn® 1702 is an ionomer resin available for use in conventional extrusion coating and coextrusion coating equipment designed to process polyethylene resins. Applications: Medical/pharmaceutical.. |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 230 °C |
14 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polyplastic Armlen® PP MF 40-2HS Polypropylene, 40% Mineral Filled Impact modified, injection moldingInformation provided by PolyPlastic Group. |
|||
Melt Flow | 14 g/10 min @Load 1.00 kg, Temperature 235 °C |
14 g/10 min @Load 2.20 lb, Temperature 455 °F |
|
Arkema Group Pebax® MX 1283 Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE (PEBA) Supersoft grade (hardness 72 shore A) Modified 2533SN01 Applications: sport (tennis shoes parts)ISO data provided by the manufacturer, Arkema. |
|||
Melt Flow | 14 - 16 g/10 min | 14 - 16 g/10 min | ASTM D1238 |
Polymer Resources AH-GP2 Acetal Homopolymer, Medium Flow, General Purpose Molding
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Flow | 14 g/10 min | 14 g/10 min | ISO 1133 |
Solvay Engineered Polymers DEXFLEX® 880 TPO
(discontinued **) Description: DEXFLEX® 880 is a thermoplastic olefinic elastomer (TPO) designed for automotive exterior applications that require a combination of stiffness, low-temperature impact, good processabil.. |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 230 °C |
14 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM-D1238 |
Braskem CP 284R HECO Polypropylene Heterophasic Copolymer CP 284R is a heterophasic copolymer designed for injection molding of pails and containers with excellent stiffness/impact strength balance. This resin also exhibits excellent productivity and proce.. |