| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Flow | 4.0 - 16 g/10 min @Load 3.80 kg, Temperature 230 °C |
4.0 - 16 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
| Polymer Resources ABS-FR Flame Retardant ABS Flame Retardant Acrylonitrile Butadiene StyreneFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch.. |
|||
| Melt Flow | 4.0 - 16 g/10 min @Load 3.80 kg, Temperature 230 °C |
4.0 - 16 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
| Polymer Resources ABS-FR-[color]-UV Flame Retardant ABS, UV-stabilized Flame Retardant Acrylonitrile Butadiene Styrene, UV-stabilizedFeatures: • Flame Retardant • Self Extinguishing • Good UV ResistanceProcess: Injection MoldingNotes: All physical, mechanical and.. |
|||
| Melt Flow | 14 - 16 g/10 min | 14 - 16 g/10 min | ASTM D1238 |
| Polymer Resources AH-GP2-[color]-H Acetal Homopolymer, Medium Flow, General Purpose Molding, Heat Stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
| Melt Flow | 9.0 - 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 - 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
| Polymer Resources PC-FR2A-D-[color]-3 Polycarbonate, Flame Retardant, Medium Flow, UV-stabilized Polycarbonate, Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
| Melt Flow | 9.0 - 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 - 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
| Polymer Resources PC-FR2-D Polycarbonate, Improved Flame Retardant, Medium Flow Polycarbonate, Improved Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted.. |
|||
| Melt Flow | 9.0 - 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 - 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
| Polymer Resources PC-FR-UV-10-0002-16A Polycarbonate, Flame Retardant, Medium Flow Polycarbonate, Flame Retardant, Medium FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on.. |
|||
| Melt Flow | 9.0 - 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 - 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
| Polymer Resources PC-GP2-D Polycarbonate, General Purpose, Medium Flow Polycarbonate, General Purpose, Medium FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on.. |
|||
| Melt Flow | 9.0 - 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 - 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
| Polymer Resources PC-GP2-D-[color]-1 Polycarbonate, General Purpose, Medium Flow with Mold Release Polycarbonate, General Purpose, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf.. |
|||
| Melt Flow | 9.0 - 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 - 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
| Polymer Resources PC-GP2-D-[color]-6 Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
| Melt Flow | 9.0 - 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 - 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
| Polymer Resources PC-GP2-TFE5 Polycarbonate, 5% PTFE, Wear Resistant, Medium Flow Polycarbonate, 5% PTFE, General Purpose, Medium Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samp.. |
|||
| Melt Flow | 9.0 - 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 - 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
| Polymer Resources PC-IM2 Polycarbonate, Impact Modified, Medium Flow Polycarbonate, Impact Modified, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided .. |
|||
| Melt Flow | 8.0 - 16 g/10 min @Load 2.16 kg, Temperature 250 °C |
8.0 - 16 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
| Polymer Resources TP-IM-G15 Polybutylene Terephthalate, 15% Glass Reinforced, Impact Modified Polybutylene Terephthalate, 15% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
| Melt Flow | 9.0 - 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 - 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
| Polymer Resources PC-FD2 Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
| Melt Flow | 8.0 - 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
8.0 - 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
| Polymer Resources PC-HM-FR2-[color]-3 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
| Melt Flow | 9.0 - 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 - 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
| Polymer Resources PC-UV2-D Polycarbonate, UV-stabilized, Medium Flow Polycarbonate, UV-stabilized, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
| Melt Flow | 8.0 - 16 g/10 min | 8.0 - 16 g/10 min | ASTM D1238 |
| A. Schulman POLYFORT™ FPP 1236-2939 Fiberglass Reinforced Homopolymer Polypropylene DescriptionPolyfort® FPP 1236-2939 is a 20% fiberglass reinforced homopolymer polypropylene.Information provided by A. Schulman. |
|||
| Melt Flow | 12 - 16 g/10 min | 12 - 16 g/10 min | Cond L; ASTM D1238 |
| Washington Penn PPH4CF2.5 Polypropylene, 25% Calcium Carbonate Filled UV Stabilized; Injection molding grade.Applications: High flow for thin wall parts requiring long-flow. Outdoor furniture.Data provided by Washington Penn Plastic Co., Inc. |
|||
| Melt Flow | 12 - 16 g/10 min | 12 - 16 g/10 min | Cond L; ASTM D1238 |
| Washington Penn PPH5CF5 Polypropylene, 50% Calcium Carbonate Filled UV Stabilized; Injection molding grade.Applications: Commonly used as a concentrate. High flow for thin wall parts requiring long-flow. Toys, small appliances, outdoor furniture.Data provided by W.. |
|||
| Melt Flow | 8.0 - 16 g/10 min | 8.0 - 16 g/10 min | ASTM D1238 |
| A. Schulman POLYFORT™ FPP 1236-2939 Fiberglass Reinforced Homopolymer Polypropylene DescriptionPolyfort® FPP 1236-2939 is a 20% fiberglass reinforced homopolymer polypropylene.Information provided by A. Schulman. |
|||
| Melt Flow | 8.0 - 16 g/10 min | 8.0 - 16 g/10 min | ASTM D1238 |
| A. Schulman POLYFORT™ FPP 1236-2939 Fiberglass Reinforced Homopolymer Polypropylene DescriptionPolyfort® FPP 1236-2939 is a 20% fiberglass reinforced homopolymer polypropylene.Information provided by A. Schulman. |
|||
| Melt Flow | 8.0 - 16 g/10 min | 8.0 - 16 g/10 min | ASTM D1238 |
| A. Schulman POLYFORT™ FPP 1236-2939 Fiberglass Reinforced Homopolymer Polypropylene DescriptionPolyfort® FPP 1236-2939 is a 20% fiberglass reinforced homopolymer polypropylene.Information provided by A. Schulman. |
|||
| Melt Flow | 8.0 - 16 g/10 min @Load 5.00 kg, Temperature 372 °C |
8.0 - 16 g/10 min @Load 11.0 lb, Temperature 702 °F |
|
| Daikin NEOFLON EP-521 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
| Melt Flow | 10 - 16 g/10 min | 10 - 16 g/10 min | ASTM D1238 |
| Buckeye Polymers BP RPP 4010 T NAT Polypropylene, Talc Filled Product Information: Our Talc filled product lines exhibit excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and .. |
|||
| Melt Flow | 10 - 16 g/10 min | 10 - 16 g/10 min | ASTM D1238 |
| Buckeye Polymers BP RPPC 1813 C BLK Polypropylene, Calcium Filled Product Information: Calcium Carbonate Filled PP Grades have a high impact toughness, moderate increased stiffness, and excel in high gloss applications. Our BP RPP C series product line ranges fro.. |
|||
| Melt Flow | 10 - 16 g/10 min | 10 - 16 g/10 min | ASTM D1238 |
| Buckeye Polymers BP RPP 2012 TR BLK Polypropylene, Talc Filled Product Information: Our Talc filled product lines exhibit excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and .. |
|||
| Melt Flow | 8.0 - 16 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.0 - 16 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
| Ravago Manufacturing Americas Echo® RPH20TC BK Recycled Polypropylene Homopolymer, 20% Talc Filled Post Consumer Homopolymer Propylene (Nylon content < 5%), 12 Melt Flow, 20% Talc Filled, Heat Stabilized, BlackInformation provided by Ravago. |
|||
| Melt Flow | 14 - 16 g/10 min | 14 - 16 g/10 min | ASTM D1238 |
| Polymer Resources AH-GP2 Acetal Homopolymer, Medium Flow, General Purpose Molding
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
| Melt Flow | 12.1 - 16 g/10 min | 12.1 - 16 g/10 min | D |
| Shandong Dongyue Shenzhou New Material Co DS608 Fluorinated Ethylene-Propylene Copolymer For High-Speed Extrusion Conformable with: Q/DYS 003-2007Fluorinated Ethylene Propylene is the copolymer of TFE and HFP, with good thermal stability, outstanding chemical inertness, good electrical insulation, and low coeff.. |
|||
| Melt Flow | 8.0 - 16 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.0 - 16 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 - ISO 1133 |
| DuPont Elvaloy® HP663 Ethylene/N-Butyl Acrylate/Carbon Monoxide Copolymer
(discontinued **) Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont. |
|||