Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.010 - 0.020 cm/cm | 0.010 - 0.020 in/in | ASTM D955 |
PolyOne LubriOne™ NL-30CF/15T Black Polyamide 612 (Nylon 612) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 - 0.020 cm/cm | 0.017 - 0.020 in/in | |
LATI Latiohm 75/4-10 CNT PBT Semiconductive/dissipative product based on Polybutylene Terephthalate (PBT). Carbon nanotubes. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.020 cm/cm @Time 86400 sec |
0.0090 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP DX09410H PC LNP* LUBRICOMP* DX09410H is a compound based on Polycarbonate resin containing Proprietary FIllers. Added features of this grade include: Healthcare, Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.020 cm/cm @Time 86400 sec |
0.0090 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP SX93441D PA12 LNP* Lubricomp* SX93441D is a compound based on Nylon 12 containing Proprietary Fillers. Characteristics of this grade are: Internally Lubricated. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.020 cm/cm @Time 86400 sec |
0.0090 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP WFL34H PBT LNP LUBRICOMP* WFL34H is a compound based on PBT resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Healthcare. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.020 cm/cm @Time 86400 sec |
0.0090 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP ZX07421 PPO LN:* LUBRICOMP* ZX07421 is a compound based on PPO resin containing proprietary fillers. Added feature of this grade is: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.020 cm/cm @Thickness 3.20 mm |
0.016 - 0.020 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 175 PBT Unreinforced, neat PBT resin for compounding only. Natural Color Only, Not intended for injection molding.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.020 cm/cm @Thickness 3.20 mm |
0.016 - 0.020 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 176 PBT Unreinforced, neat PBT resin for fibers. Natural Color Only, Not intended for injection molding. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.020 cm/cm @Thickness 3.20 mm |
0.016 - 0.020 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 176HP PBT Unreinforced, FDA compliant neat PBT resin for fibers. Natural Color Only, Not intended for injection molding. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.020 cm/cm @Time 86400 sec |
0.0090 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP QF007 PA 6/10 LNP* THERMOCOMP* QF007 is a compound based on Nylon 6/10 resin containing 35% Glass Fiber. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.020 cm/cm @Time 86400 sec |
0.0090 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP RF006SXZ PA 66 LNP* THERMOCOMP* RF006SXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added feature of this material is: Heat Stabilized. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.020 cm/cm @Time 86400 sec |
0.0090 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP RF006XXH PA 66 LNP* THERMOCOMP* RF006XXH is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added feature of this material is: Healthcare. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.020 cm/cm @Time 86400 sec |
0.0090 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP RF007ES PA 66 LNP* THERMOCOMP* RF007ES is a compound based on Nylon 66 resin containing 35% Glass Fiber. Added features of this material include: Heat Stabilized, Easy Molding. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.020 cm/cm @Time 86400 sec |
0.0090 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP RFB53XXZ PA 66 LNP* THERMOCOMP* RFB53XXZ is a compound based on Nylon 66 resin containing 15% Glass Fiber, 25% Glass Bead. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.020 cm/cm @Time 86400 sec |
0.0090 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP RFB66 PA 66 LNP* THERMOCOMP* RFB66 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 30% Glass Bead. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.020 cm/cm | 0.0080 - 0.020 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® D201 PBT Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.020 cm/cm | 0.0080 - 0.020 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® T101 PET Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.020 cm/cm @Time 86400 sec |
0.0090 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-LOY PF303 PA 6 LNP* STAT-LOY* PF303 is a Nylon 6 base resin containing 15% Glass Fiber. Added features of this grade includes: Antistat. |
|||
Linear Mold Shrinkage, Transverse | 0.015 - 0.020 cm/cm | 0.015 - 0.020 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® N602 Nylon 66 Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Transverse | 0.018 - 0.020 cm/cm | 0.018 - 0.020 in/in | ISO DIS 294-4 |
Wellman Wellamid® MRT1487 BK 32% Mineral Reinforced, Toughened Grade Nylon 66 Description: Mineral Reinforced, Toughened Grade Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.020 cm/cm | 0.016 - 0.020 in/in | ISO DIS 294-4 |
Wellman Wellamid® XT1482-WT1 High Impact Nylon 66 Description: High Impact Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.020 cm/cm | 0.016 - 0.020 in/in | ISO DIS 294-4 |
Wellman Wellamid® XT1486-BK Medium Impact Nylon 66 Description: Medium Impact Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.00 - 0.020 cm/cm | 0.00 - 0.020 in/in | Flame Bar; ASTM D955 |
DSM Biomedical Elasthane™ 80A Thermoplastic Polyether Polyurethane (TPU) A high tensile strength, aromatic biomedical polymer with an exceptional combination of mechanical properties plus biological compatibility
Elasthane™ TPU exhibits outstanding hydrolytic stabilit.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.020 cm/cm | 0.016 - 0.020 in/in | ISO DIS 294-4 |
Wellman Wellamid® MRB40K004-WT1 40% Mineral Reinforced Nylon 66 Description: Mineral Reinforced Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.017 - 0.020 cm/cm | 0.017 - 0.020 in/in | |
LATI Later 4 PBT Polybutylene Terephthalate (PBT). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A. |
|||
Linear Mold Shrinkage, Transverse | 0.015 - 0.020 cm/cm | 0.015 - 0.020 in/in | |
Solvay TECHNYL® 1015CR PA6, DRY Description: Polyamide 6, unfilled, standard for fast injection cycles, for injection molding Available in: Asia Pacific Product Applications: TECHNYL® 1015CR has high fluidity and a good mould re.. |