| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.32 g/cc | 0.0477 lb/in³ | |
| Linear Mold Shrinkage, Flow | 0.017 - 0.020 cm/cm | 0.017 - 0.020 in/in | |
| Linear Mold Shrinkage, Transverse | 0.017 - 0.020 cm/cm | 0.017 - 0.020 in/in |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Elongation at Break | >= 100 % <br>@Temperature 23.0 °C |
>= 100 % <br>@Temperature 73.4 °F |
|
| >= 100 % <br>@Temperature 60.0 °C |
>= 100 % <br>@Temperature 140 °F |
||
| >= 100 % <br>@Temperature 90.0 °C |
>= 100 % <br>@Temperature 194 °F |
||
| >= 100 % <br>@Temperature 120 °C |
>= 100 % <br>@Temperature 248 °F |
||
| Elongation at Yield | 6.0 % <br>@Temperature 23.0 °C |
6.0 % <br>@Temperature 73.4 °F |
|
| Tensile Modulus | 0.400 GPa <br>@Temperature 120 °C |
58.0 ksi <br>@Temperature 248 °F |
|
| 0.650 GPa <br>@Temperature 90.0 °C |
94.3 ksi <br>@Temperature 194 °F |
||
| 0.900 GPa <br>@Temperature 60.0 °C |
131 ksi <br>@Temperature 140 °F |
||
| 2.40 GPa <br>@Temperature 23.0 °C |
348 ksi <br>@Temperature 73.4 °F |
||
| Charpy Impact Unnotched | NB | NB | |
| Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 120 °C | 248 °F | |
| Deflection Temperature at 0.46 MPa (66 psi) | 165 °C | 329 °F | |
| Deflection Temperature at 1.8 MPa (264 psi) | 55.0 °C | 131 °F | |
| Vicat Softening Point | 170 °C <br>@Load 5.00 kg |
338 °F <br>@Load 11.0 lb |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 230 - 245 °C | 446 - 473 °F | |
| Mold Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
| Drying Temperature | 110 - 130 °C <br>@Time 10800 sec |
230 - 266 °F <br>@Time 3.00 hour |
| Descriptive Properties | Value | Comments |
|---|---|---|
| ISO Shrinkage - Pressure | 60 MPa |