Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0060 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® EXL4019 PC (Asia Pacific) Lexan* EXL4019 is an opaque 9% Glass Fiber (GF) reinforced polycarbonate (PC) siloxane copolymer resin for injection molding (IM) applications requiring improved stiffness. This resin also offers im.. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm @Time 86400 sec |
0.0040 - 0.0060 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Lubricomp DFP22 PC LNP* DFP22 is a Polycarbonate base resin containing glass fiber and PTFE/Silicone Lubricants. Characteristic of this grade is: Internally Lubricated.This data was supplied by SABIC-IP for the Amer.. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | ISO 294-4 |
Ineos ABS Lustran® ABS 450 Injection Molding Grade Lustran® ABS 450 has medium impact strength, high flow, and is injection molding grade. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | |
LATI Laticonther 62 GR/50 PA 6, 50% Graphite Reinforced High thermal conductivity product based on Polyamide 6 (PA6). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Te.. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | |
LATI Latilon 28D G/20-V0 PC, 20% Glass Fiber Reinforced, Flame Retardant Polycarbonate (PC) based compound. Glass fibers. UL94 V-0 classified, brominated and chlorinated halogens-based flame retardants free. Low smoke density and low toxicity index. High dimensional stab.. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics ULTEM 2312EPR PEI 30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics ULTEM 2312EPR PEI (Asia Pacific) 30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | ASTM D955 |
Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-848 CF30 is a 30% carbon fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparabl.. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm @Thickness 1.50 - 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.0591 - 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 420 PBT 30% GR, excellent strength, stiffness and dimensional stability. High heat resistance. Appliance handles, spotlights, electric motors, connectors. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics XYLEX X8300 PC+POLYESTER PC+Polyester, UV Stabilized, Transparent |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xylex X8300HP PC+POLYESTER (Asia Pacific) Transparent, US Food Contact compliant, chemically resistant.
This grade will no longer be supported with biocompatibility information and should not be used for medical applications which require b.. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xylex X8300HP PC+POLYESTER (Europe-Africa-Middle East) Transparent, US Food Contact compliant, chemically resistant.
This grade will no longer be supported with biocompatibility information and should not be used for medical applications which require b.. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Infino® AE-2130 PC/PET, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm @Thickness 4.00 mm |
0.0040 - 0.0060 in/in @Thickness 0.157 in |
|
Teijin Multilon TN-7100F Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy Halogen-free flame retardant PC/ABS polymer alloy, and is also antimony-free. High stiffness and flowability realize the thin wall of large-scale business machine chassis.Information provided by Tei.. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm @Thickness 4.00 mm |
0.0040 - 0.0060 in/in @Thickness 0.157 in |
|
Teijin Panlite® BN-8110R Improved Mold Release, Carbon Fiber Reinforced, Flame Resistant Polycarbonate Resin CF 10% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are flame retardance, low molding shrinkage and dimensiona.. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0060 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Infino® WP-1069 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0060 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Starex® VE-0855YS ABS, Unreinforced FR Flame-retardant ABS that can be used in the exterior of monitorsInformation provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Infino® HP-1000XA PC/ABS, Unreinforced PC/ABS material for automobile IP-coreInformation provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm @Time 86400 sec |
0.0040 - 0.0060 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP JCL36E PES LNP* LUBRICOMP* JCL36E is a compound based on Polyethersulfone (PES) resin containing 30% Carbon Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm @Time 86400 sec |
0.0040 - 0.0060 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP NF001XXX PC+ABS LNP* THERMOCOMP* PCA-F-1001 is a compound based on PC+ABS resin containing 5% Glass Fiber. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0060 cm/cm | 0.0020 - 0.0060 in/in | ASTM D955 |
Lubrizol Estane® 2355-80AE Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Damping capacityAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009... |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm @Thickness 4.00 mm |
0.0040 - 0.0060 in/in @Thickness 0.157 in |
|
Teijin Panlite® G-3410H Low Anisotropy, Glass Fiber Reinforced Polycarbonate Resin Reinforced with 10 % of special GF and improved appearance grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need good appearance and mechanical propertyPreci.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0060 cm/cm | 0.0020 - 0.0060 in/in | |
LATI Latimass 37 B01-01 D025 Bio-Polymer Specific density compound based on Bio-Polymer (PLA, PHB, ...). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |