Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0060 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® CFR5630 PC COPOLYMER (Asia Pacific) LEXAN™ CFR5630 Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density an.. |
|||
Linear Mold Shrinkage, Transverse | 0.0060 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LUX7432C PC COPOLYMER (Asia Pacific) Lexan* LUX7432C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Linear Mold Shrinkage, Transverse | 0.0060 cm/cm | 0.0060 in/in | ASTM D955 |
LNP Lubricomp® PDX-O-90351 Polyphenylene Sulfide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Linear Mold Shrinkage, Transverse | 0.0060 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® DMX1132 PC Copolymer (Europe-Africa-Middle East) Lexan* DMX1132 is a high flow polycarbonate copolymer resin with improved ammonia resistance over regular polycarbonate resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East reg.. |
|||
Linear Mold Shrinkage, Transverse | 0.0060 cm/cm | 0.0060 in/in | 410°C nozzle, 190°C tool; ISO 294-4 |
Victrex® WG102™ Polyaryletherketone Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact compliantWG102 does not c.. |
|||
Linear Mold Shrinkage, Transverse | 0.0060 cm/cm | 0.0060 in/in | ASTM D955 |
LNP Thermocomp® EF-1002 EP BK8-114 Polyetherimide, Glass Fiber Reinforcement
(discontinued **) Features: Good ProcessabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are.. |
|||
Linear Mold Shrinkage, Transverse | 0.0060 cm/cm | 0.0060 in/in | ASTM D955 |
LNP Lubricomp® GFL-4034 EM M Polysulfone, Milled Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **)& Features: Good Moldability, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP g.. |
|||
Linear Mold Shrinkage, Transverse | 0.0060 cm/cm | 0.0060 in/in | ASTM D955 |
LNP Thermocomp® GF-1006 Polysulfone, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Linear Mold Shrinkage, Transverse | 0.0060 cm/cm @Temperature 80.0 °C |
0.0060 in/in @Temperature 176 °F |
60x60x2 mm; ISO 294-4 |
Gromax BFG30-EN04B2 Nylon 6 36% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Linear Mold Shrinkage, Transverse | 0.0060 cm/cm | 0.0060 in/in | 60x60x2; 280°C / MT 80°C; 600 bar; ISO 294-4 |
Lanxess Durethan® BKV 40H2.0 EF 900116 Nylon 6, Glass Fiber Reinforced PA 6, 40% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.0060 cm/cm | 0.0060 in/in | ISO 294-4, 2577 |
Lanxess Durethan® TP 036-052 000000 Nylon 6, 60% Glass Fiber PA 6, injection molding grade, 60% glass fibers, good flowability (Easy Flow), good heat-resistance |
|||
Linear Mold Shrinkage, Transverse | 0.0060 - 0.0085 cm/cm | 0.0060 - 0.0085 in/in | |
LATI Latigloss 66 H2 G/60 PA 66, 60% Glass Fiber Reinforced, Heat Stabilized Product with high mechanical properties and exceptional surface finish based on Polyamide 66 (PA66). Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am.. |
|||
Linear Mold Shrinkage, Transverse | 0.0060 cm/cm @Time 86400 sec |
0.0060 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP AX06437 ABS LNP* THERMOCOMP* AX06437 is a compound based on ABS resin containing Proprietary Filler(s). Added feature of this grade is: Platable. |
|||
Linear Mold Shrinkage, Transverse | 0.0060 - 0.0065 cm/cm @Time 86400 sec |
0.0060 - 0.0065 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP DX11354 PC (Asia Pacific) This is a PC compound with good plating, surface and mechanical performance, a good candidate for Laser Direct Structuring applications. |
|||
Linear Mold Shrinkage, Transverse | 0.0060 - 0.0080 cm/cm @Time 86400 sec |
0.0060 - 0.0080 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp JF003L PES LNP* Thermocomp* JF003L is a compound based on Polyethersulfone (PES) containing Glass Fiber. Characteristics of this grade are Low Extractable.This data was supplied by SABIC-IP for the Americas r.. |
|||
Linear Mold Shrinkage, Transverse | 0.0060 - 0.0090 cm/cm | 0.0060 - 0.0090 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® SHF4930 PBT (Europe-Africa-Middle East) Super high flow FR PBT grade with 15% Glass reinforced |
|||
Linear Mold Shrinkage, Transverse | 0.0060 cm/cm @Time 86400 sec |
0.0060 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP NX11302 PC+ABS (Asia Pacific) This is a PC/ABS compound with colorable, good plating, surface and mechanical performance, a good candidate for Laser Direct Structuring applications |
|||
Linear Mold Shrinkage, Transverse | 0.0060 - 0.010 cm/cm | 0.0060 - 0.010 in/in | ISO DIS 294-4 |
Wellman Wellamid® FRGF1827-BK1 10% Glass Fiber Reinforced Flame Retardant Nylon 66 Description: Glass Fiber Reinforced Flame Retardant Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.0060 cm/cm | 0.0060 in/in | ISO 294-4,2577 |
Covestro Makrolon® SF805 Polycarbonate, 5% Glass Filled MVR (300 °C/1.2 kg) 7.0 cm3/10 minStructural foam5 % Glass fiber reinforcedNormal fiberChlorine- and bromine-free flame retardantHigh viscosityEasy releaseInjection moldingAvailable in natural (opa.. |
|||
Linear Mold Shrinkage, Transverse | 0.0060 cm/cm | 0.0060 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® BG-15 S PA6-GF15 Product description: Grilon BG-15 S is a heat stabilized PA6 injection molding grade with 15% glass fibers. Grilon BG-15 S has the following important properties: Excellent surface finishEasy flowin.. |
|||
Linear Mold Shrinkage, Transverse | 0.0060 cm/cm | 0.0060 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® BG-30 S FA PA6-GF30 Product description: Grilon BG-30 S FA is a heat stabilized PA6 injection molding grade with 30% glass fibers. Grilon BG-30 S FA has the following important properties: Excellent surface finishEasy .. |
|||
Linear Mold Shrinkage, Transverse | 0.0060 cm/cm | 0.0060 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® 80G43HS1L BK104 Nylon 66
(Unverified Data**) 43% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G43HS1L BK104 is a 43% glass fiber reinforced heat stabilized black polyamide 66 resin with superior impact resistance.Information.. |
|||
Linear Mold Shrinkage, Transverse | 0.0060 cm/cm | 0.0060 in/in | Eurotec |
Eurotec® Tecomid® NT40 GR60 NL HS PPA, 60% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Transverse | 0.0060 cm/cm | 0.0060 in/in | Eurotec |
Eurotec® Tecotek® PC30 NL TD 700 PC, unfilled, flame retardant - halogen (RoHS compliant), impact modified, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Transverse | 0.0060 cm/cm | 0.0060 in/in | |
E-Polymers SEPAZ® LC30 PP Copolymer LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Linear Mold Shrinkage, Transverse | 0.0060 cm/cm @Temperature 80.0 °C |
0.0060 in/in @Temperature 176 °F |
60x60x2 mm; ISO 294-4 |
Gromax CFG45-RN13N1 Nylon 6 46% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |