Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.14 g/cc | 1.14 g/cc | 23/23°C; ASTM D792 |
RheTech Products G30P100-01 30% Glass Fiber Reinforced Polypropylene, Black Applications: Fender apronsUnderhood componentsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 1.14 g/cc | 1.14 g/cc | ASTM D792 |
S&E Specialty Polymers TufFlex™ GF 1831 PVC/Nitrile Alloy Application: High Grade Oil Resistant PVC/Nitrile Soling Material with excellent Abrasion and slip resistant properties designed for work boot applications.Information provided by S&E Specialty Poly.. |
|||
Specific Gravity | 1.14 g/cc | 1.14 g/cc | ASTM D 792 |
SABIC Innovative Plastics Cycoloy® CE8510 PC+ABS (Asia Pacific) Extrusion grade PC/ABS. Low viscosity, high impact and ductility.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Specific Gravity | 1.14 g/cc | 1.14 g/cc | ASTM D 792 |
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS (Europe-Africa-Middle East) PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Europe-Africa-Middle East re.. |
|||
Specific Gravity | 1.14 g/cc | 1.14 g/cc | |
Radici Radilon® CS 35FL (dry) Nylon 6/66 Radilon® CS is a range of polyamide 6/66 copolymers obtained through the polymerization of caprolactam and hexamethylendiamine salt with adipic acid.Information provided by Radici group. |
|||
Specific Gravity | 1.14 g/cc | 1.14 g/cc | ASTM D792 |
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS UV stabilized, non-FR PC/ABS of excellent flow and impact performance |
|||
Specific Gravity | 1.14 g/cc | 1.14 g/cc | (Dry) |
Radici Radilon® A 38 (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Specific Gravity | 1.14 g/cc | 1.14 g/cc | ASTM D792 |
Ravago Manufacturing Americas Hylon® N1200HL BK Nylon 6/6
(discontinued **) Available in North AmericaAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedAuto Specifications: DELPHI QMPL-1257 Color: BlackForm: PelletsInformation provided by Rava.. |
|||
Specific Gravity | 1.14 g/cc | 1.14 g/cc | |
Huntsman IROGRAN® A 92 P 4851 Ether-Based TPU-For Cable Industry Introduction: IROGRAN A 92 P 4851 is a thermoplastic polyether- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are high extrudability and lo.. |
|||
Specific Gravity | 1.14 g/cc | 1.14 g/cc | ASTM D792 |
LG Chemical LUMID GP1000B(W) PA66, General Purpose, Low Viscosity Feature: Injection Molding, PA66, General Purpose, Low ViscosityApplication: Buckles, Chair NobCAS No. 32131-17-2Information provided by LG Chemical |
|||
Specific Gravity | 1.14 g/cc | 1.14 g/cc | ISO 1183 |
Lanxess Durethan® B 31 FCS 000000 Nylon 6, Film Grade PA 6, non-reinforced, extrusion, low viscosity, slip agentInformation provided by LANXESS. |
|||
Specific Gravity | 1.14 g/cc | 1.14 g/cc | ASTM D792 |
Lucent Polymers CPP-230 Polypropylene, 30% Calcium Carbonate Filled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Specific Gravity | 1.14 g/cc | 1.14 g/cc | ASTM D792 |
Lucent Polymers PC/ABS-1208 Polycarbonate+ABS, General Purpose, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Specific Gravity | 1.14 g/cc | 1.14 g/cc | |
Momentive Performance Materials Siloprenâ„¢ LSR 2645 Custom Liquid Silicone Rubber - Infant Care This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Specific Gravity | 1.14 g/cc | 1.14 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP NXCY620 PC+ABS LNP* LUBRICOMP* NXCY620 is a compound based on Cycoloy* XCY620 containing Silicone. Added feature of this material is: Lubricant. |
|||
Specific Gravity | 1.14 g/cc | 1.14 g/cc | |
Spartech 114-4-62 PVC and Alloy Products for Footwear Used for waterproof boots.Information provided by Spartech |
|||
Specific Gravity | 1.14 g/cc | 1.14 g/cc | ASTM D792 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7370-9000 TPE Product Description: StarFlex P 7370-9000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelGood WeatherabilityFDA and medical grades availableProcessing Method.. |
|||
Specific Gravity | 1.14 g/cc | 1.14 g/cc | ASTM D792 |
Teknor Apex Chemlon® 100 Nylon 66, Unreinforced Features: Basic nylon 66 with internal lubrication. Widely used for automotive, electronic and appliance applications. Processing Method: Injection Molding Forms: Pellets Automotive Specifications: .. |
|||
Specific Gravity | 1.14 g/cc | 1.14 g/cc | ASTM D792 |
Lubrizol Estane® 2103-90AEL Film Grade Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film resin for injection blow moldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product .. |
|||
Specific Gravity | 1.14 - 1.158 g/cc | 1.14 - 1.158 g/cc | |
Dow CYRACURE™ UVR-6128 Cycloaliphatic Epoxide CYRACURE™ UVR-6107 cycloaliphatic epoxide is a standard flexibilizing cycloaliphatic epoxide resin. Typical applications include: Metal decoration coatings Overprint varnishes Flexible packaging .. |
|||
Specific Gravity | 1.14 g/cc | 1.14 g/cc | ASTM D792 |
Clariant Renol PA101LRD-190 Nylon 66, General Purpose, Lubricated Data provided by Clariant Masterbatches |
|||
Specific Gravity | 1.14 g/cc | 1.14 g/cc | ASTM D792 |
Clariant Renol PA111 Nylon 66, General Purpose Data provided by Clariant Masterbatches |
|||
Specific Gravity | 1.14 g/cc @Temperature 25.0 °C |
1.14 g/cc @Temperature 77.0 °F |
|
Dow Corning 3110 SILICONE RUBBER ENCAPSULANT Two-part, white, condensation cure, moderate flow, general purpose encapsulant, cure speed varied by catalyst type and mix ratio.Information provided by Dow Corning |
|||
Specific Gravity | 1.14 g/cc | 1.14 g/cc | ASTM D792 |
PolyOne Synprene® RT-3780 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledNaturalApplications:General PurposeMarket:Consumer GoodsIndustrialBuilding and ConstructionProcessing Method:Injection Molding.. |
|||
Specific Gravity | 1.14 g/cc | 1.14 g/cc | (Dry) |
Radici Radilon® A 42 (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Specific Gravity | 1.14 g/cc | 1.14 g/cc | ISO 1183 |
Cathay PA56 Renewable Engineering Polyamide, 50% RH Cathay engineering polyamides contain 26-100% renewably sourced material. Advantages: Operates at similar conditions to PA66; Suitable for injection, compounding and extrusion; Stable mechanical pr.. |
|||
Specific Gravity | 1.14 g/cc | 1.14 g/cc | ASTM D792 |
LG Chemical LUPOL GP2300 PP+GF30% Description: Injection Molding, PP+GF30%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical |