| Category | Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber |
| Manufacturer | Dow Corning |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Dow Corning 3110 SILICONE RUBBER ENCAPSULANT.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.14 g/cc <br>@Temperature 25.0 °C |
1.14 g/cc <br>@Temperature 77.0 °F |
|
| Viscosity | 13000 cP | 13000 cP | dynamic |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 45 | 45 | |
| Tensile Strength, Ultimate | 2.76 MPa | 400 psi | |
| Elongation at Break | 175 % | 175 % | |
| Tear Strength | 3.51 kN/m | 20.0 pli |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 200 °C | 392 °F | |
| Minimum Service Temperature, Air | -55.0 °C | -67.0 °F |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 7.30e+12 ohm-cm | 7.30e+12 ohm-cm | |
| Dielectric Constant | 2.2 <br>@Frequency 100000 Hz |
2.2 <br>@Frequency 100000 Hz |
|
| 2.29 <br>@Frequency 100 Hz |
2.29 <br>@Frequency 100 Hz |
||
| Dielectric Strength | 17.1 kV/mm | 434 kV/in | |
| Dissipation Factor | 0.0010 <br>@Frequency 100000 Hz |
0.0010 <br>@Frequency 100000 Hz |
|
| 0.010 <br>@Frequency 100 Hz |
0.010 <br>@Frequency 100 Hz |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Shelf Life | 18.0 Month | 18.0 Month |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | white | |
| Mix Ratio (X:1) | 10 | Base to Catalyst ETN |