Material Notes:
Product Description: StarFlex P 7370-9000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelGood WeatherabilityFDA and medical grades availableProcessing Method: Injection MoldingInformation Provided by STAR Thermoplastic Elastomers
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Viscosity 8000 cP

@Shear Rate 10994 1/s,
Temperature 210 °C
8000 cP

@Shear Rate 10994 1/s,
Temperature 410 °F
ASTM D3835
Mechanical Properties Metric English Comments
Hardness, Shore A 70

@Time 10.0 sec
70

@Time 0.00278 hour
ASTM D2240
Tensile Strength at Break 5.34 MPa

@Time 7200 sec
775 psi

@Time 2.00 hour
Die C; ASTM D414
Elongation at Break 702 %

@Time 7200 sec
702 %

@Time 2.00 hour
Die C; ASTM D412
300% Modulus 0.00267 GPa

@Time 7200 sec
0.387 ksi

@Time 2.00 hour
Die C; ASTM D412
Tear Strength 25.1 kN/m
143 pli
ASTM D624
Descriptive Properties Value Comments