Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Radici Radilon® A 42 (cond.) Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced
Manufacturer Radici Group Plastics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radilon® A 42 (cond.) Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
(Dry)
Water Absorption 8.4 %
8.4 %
initially dry
Moisture Absorption at Equilibrium 2.1 %
2.1 %
initially dry
Viscosity Measurement 240
240
cm³/g Viscosity Number
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.0 MPa
8700 psi
Elongation at Break >= 50 %
>= 50 %
Nominal
Elongation at Yield 28 %
28 %
Tensile Modulus 1.60 GPa
232 ksi
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
Charpy Impact, Notched 0.750 J/cm²

@Temperature 23.0 °C
3.57 ft-lb/in²

@Temperature 73.4 °F
0.750 J/cm²

@Temperature -30.0 °C
3.57 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
(Dry)
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Comparative Tracking Index 600 V
600 V