Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.11 g/cc | 1.11 g/cc | as molded- 10 minutes at 116°C |
Multibase SILASTIC® Q7-4720 Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | 23/23°C; ASTM D792 |
RheTech Products FT4200-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Body side moldingsGrillesElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | 23/23°C; ASTM D792 |
RheTech Products M25UVP250-01 25% Mica Reinforced Polypropylene Copolymer, UV Stabilized, Black Applications: BracketsCowl screensRigid exterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D792 |
Polymax® Maxelast® F02-137D TPE, Halogen Free Extrusion Grade Characteristics: Good melt strengthSoft touchSmooth surface with dry feelGood weather and heat resistanceWide range of hardnessEasy processing Halogen FreeLow smoke emissionRoHs compliantDesigned to.. |
|||
Specific Gravity | 1.11 - 1.17 g/cc | 1.11 - 1.17 g/cc | ASTM D792 |
S&E Specialty Polymers GM-3950-095 PVC Non-toxic PVC material designed for molding applications.Information provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D792 |
Quadrant EPP Nylatron® 703 XL Cast, Wear Resistant, Zero 'Stick-Slip' (ASTM Product Data Sheet) |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D792 |
Ravago Manufacturing Americas Enviramid™ N2300THL BK/HF Post Consumer Recycle Nylon 6 Impact Modified, High Flow, Heat Stabilized, Lubricated, Black and Made from EnViramid Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D 792 |
SABIC Innovative Plastics Geloy FXTW26SK ASA (Europe-Africa-Middle East) Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Europe-Africa-Middle.. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D792 |
PolyOne Edgetek® AS-10GF/000 BLACK Acrylonitrile Butadiene Styrene (ABS) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D792 |
LG Chemical LUMID HI5083A(W) PA6/ABS+MF8%, High Impact Feature: Injection Molding, PA6/ABS+MF8%, High ImpactApplication: Electric/Electronic Components (Shaver Die)CAS No. 25038-54-4, 9003-56-9, 9003-54-7 and 14807-96-6Information provided by LG Chemica.. |
|||
Specific Gravity | 1.11 - 1.17 g/cc | 1.11 - 1.17 g/cc | BAM 1014 |
Kraton® G7820 GU-N (SEBS) Compound Description: Kraton G7820 GU-N is an easy processing, general purpose 90 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D792 |
Lubrizol Advanced Materials Pearlthane® D91F65D Thermoplastic Polyurethane Elastomer PEARLTHANE® D91F65D is an aliphatic TPU supplied in colourless natural pellets. In addition to typical TPU properties like outstanding abrasion loss, PEARLTHANE® D91F65D offers excellent colou.. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | |
Momentive Performance Materials Siloprenâ„¢ Electro 242-3 Electrically Insulating Liquid Silicone Rubber This LSR elastomer is an electrically insulating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | |
Momentive Performance Materials Siloprenâ„¢ LIM 9071E Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | |
Momentive Performance Materials TUFELâ„¢ II 94405 Low Volatile Extrusion Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ISO 2781 |
Lubrizol Advanced Materials PEARLTHANE® 91T85 Thermoplastic Polyurethane Elastomer Type : Pearlthane® 91T85 is a aliphatic-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Low density, fast processing and excellent elasticity properties.A.. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL V0150B PPE+HIPS Noryl* V0150B is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm a.. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D792 |
Samsung Cheil Industries Starex® SF-0505H MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D 792 |
SABIC Innovative Plastics Noryl LS175 PPE+HIPS Noryl* LS175 modified polyphenylene ether resin is an unfilled grade suitable for both extrusion and injection molding conversion routes. It uses non-chlorinated, non-brominated FR additives to del.. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Europe-Africa-Middle East) Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity... |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL PN275 PPE+PS PPE+PS with low mineral loading. High heat, platable applications. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL PN275F PPE+PS PPE+PS with low mineral loading. High heat, platable applications. NSF approved for water contact applications. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL PVX0800 PPE NORYL* PVX0800 resin is a high flow, V0 = 1.5 mm grade, suitable for a variety of electronics applications. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL FXN4020H PPE+HIPS (Asia Pacific) high gloss Noryl |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ISO 1183/1 |
A. Schulman FORMION™ FI 232 10% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 232 is an injection molding grade, 10% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness.App.. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | DIN 53479 |
Lubrizol ESTANE® 54640 Ether Based Thermoplastic Polyurethane (European Grade) Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability in a flexible.. |
|||
Specific Gravity | 1.11 g/cc @Temperature 25.0 °C |
1.11 g/cc @Temperature 77.0 °F |
|
Dow Corning SILASTIC® 25140 SILICONE RUBBER 40 durometer, peroxide cured, general purpose silicone rubber compoundInformation provided by Dow Corning |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D792 |
Diamond Polymers ABS TR-5000 Transparent Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D792 |
E-Polymers TEKAMID® H12TW Unreinforced Low warpage PA/ABS Alloy Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.H-series: PA6/ABS, PA66/AB.. |