Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.90 g/cc | 1.90 g/cc | Slurry |
Omya OMYACARB® F - FL Calcium Carbonate A high purity, ultrafine, wet ground natural calcium carbonate available in dry or slurry form.Applications: Plastic applications such as rigid PVC and flexible PVC. Paint applications such as water.. |
|||
Specific Gravity | 1.90 - 2.00 g/cc | 1.90 - 2.00 g/cc | |
P & P Technology Conductive Elastomer Nickel Graphite particlesInformation provided by P & P Technology |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group 2572 AMC Glass fiber reinforced Polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, good abrasion stability, high flame retardance in combin.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group 3535 Epoxy Glass fiber-reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties adn dimensional stability even at high temperatures. Form: Low dust granulate pack.. |
|||
Specific Gravity | 1.90 - 2.00 g/cc | 1.90 - 2.00 g/cc | ISO 1183 |
Raschig Group 4552 Silicone Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to +/- 300°C continuously, excellent electrical properties, good mechanical strength, very good dimensional stabi.. |
|||
Specific Gravity | 1.90 - 2.00 g/cc | 1.90 - 2.00 g/cc | ISO 1183 |
Raschig Group EPOXIDUR® 3582 EP Epoxy Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Moldi.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group RALUPOL® 4806 UP Glass-fiber reinforced polyester molding compound. Very low mold shrinkage and post-shrinkage, very good mechanical strength, very good electrical values, better performance values compared to UP 80.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group RALUPOL® 804 UP Polyester Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy m.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group RALUPOL® 8602 UP Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic molding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical streng.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group SURAPLAST 54 UPA Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for.. |
|||
Specific Gravity | 1.90 - 2.00 g/cc | 1.90 - 2.00 g/cc | ASTM D792 |
Mar-Bal MB1000-10 Thermoset Polyester Composite Molding Compound A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ASTM D792 |
Mar-Bal MB1000-PC Thermoset Polyester Composite Molding Compound A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro.. |
|||
Specific Gravity | 1.90 g/cc | 1.90 g/cc | ASTM D297 |
Greene Tweed FPD Blueâ„¢ 707 Fluoroelastomer Specifically developed for flat panel display CVD and dry plasma etch equipment where seal reliability and minimal contamination are essential, FPD Blueâ„¢ 707 fluoroelastomer provides excellent .. |
|||
Specific Gravity | 1.90 g/cc | 1.90 g/cc | |
Lord Adhesives Thermosetâ„¢ ME-542 Underfill Encapsulant LORD Thermosetâ„¢ ME-542 encapsulant is an anhydridefree, thermally conductive, semiconductor grade epoxy underfill product developed for the encapsulation of densely populated area array flip ch.. |
|||
Specific Gravity | 1.90 g/cc | 1.90 g/cc | ASTM D-792 |
Glastic T-160 Fiberglass-Reinforced Polyester Laminate Grade T-160 is a new, high-strength, heat-resistant laminate. This highly creep-resistant material is excellent for applications where electrically insulating materials are subject to physical load.. |
|||
Specific Gravity | 1.90 g/cc | 1.90 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP 2F006 ETFE LNP* THERMOCOMP* 2F006 is a compound based on ETFE containing 30% Glass Fiber. |
|||
Specific Gravity | 1.90 - 1.98 g/cc | 1.90 - 1.98 g/cc | ASTM D792 |
Adamas Adalon® 403 PTFE, 15% Polyimide Information provided by Adamas, HPM |
|||
Specific Gravity | 1.90 g/cc | 1.90 g/cc | |
BYK Cloisite® 10A Nanoclay Cloisite® 10A is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.
Information provided by Southern Clay ProductsSouthern Clay P.. |
|||
Specific Gravity | 1.90 - 1.96 g/cc | 1.90 - 1.96 g/cc | |
3M Dyneon™ Dynamar™ FX 5911 Polymer Processing Additive Dynamar FX 5911 is a free-flowing fluoropolymer processing aid that is designed for use at very low levels (typically 250-1000 ppm) necessary to improve processing, it does not alter or detract from.. |
|||
Specific Gravity | 1.90 - 1.96 g/cc | 1.90 - 1.96 g/cc | |
3M Dyneon™ FX 5912 Dynamar™ Polymer Processing Additive Dynamar FX 5912 is a free-flowing fluorothermoplastic processing aid that is designed for use at very low levels to improve the processing of thermoplastics. Typical use levels of 200 to 1000 ppm ha.. |
|||
Specific Gravity | 1.90 g/cc | 1.90 g/cc | |
Bulk Molding Compounds BMC 5209 Mineral Filled, Glass Reinforced Polyester BMC 5209 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ex.. |
|||
Specific Gravity | 1.90 - 1.93 g/cc | 1.90 - 1.93 g/cc | ASTM D792 |
Adamas Adalon® 410 PTFE+ PEEK Information provided by Adamas, HPM |
|||
Specific Gravity | 1.90 g/cc | 1.90 g/cc | |
BCC Products Kwik Kast BC 8650 Urethane Casting BC 8650 is an advanced fast cast polyurethane tooling system. BC 8650 features low viscosity, low exotherm and minimal shrinkage. Kwik Kast Blue cures hard, yet more durable resulting in less brittl.. |
|||
Specific Gravity | 1.90 g/cc | 1.90 g/cc | |
Aremco AREMCOLOX™ 502-1600 (94%) Machinable Boron Nitride 94% Hot-pressed 94% boron nitride. High thermal conductivity. Easily machined. Non-reactive in molten salts, aluminum and other metals. Plates from 1/4" to 1" thick; rods from 1/4" to 3" diameter; b.. |
|||
Specific Gravity | 1.90 g/cc | 1.90 g/cc | |
Aremco Corr-Paint™ CP2060 High Temperature Protective Coating Novolac-Epoxy, Silicon Carbide Filled This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho.. |
|||
Specific Gravity | 1.90 - 2.00 g/cc | 1.90 - 2.00 g/cc | |
Bulk Molding Compounds BMC 700 Thermoset Polyester, High Arc Quench Electrical Grade BMC 700 is a general purpose, mineral filled, glass fiber-reinforced polyester compound that was initially designed for molding arc chutes. It has superior arc quench properties. As with all other B.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group 5567 DAP Diallyl Phthalate (DAP), Cast, Mineral Filler Glass-fiber reinforced diallyl phthalate molding compound free from halogens. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exc.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group RALUPOL® 8605 UP Polyester Glass fiber reinforced polyester molding compound. Resistant to hydrolysis. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU dire.. |
|||
Specific Gravity | 1.90 g/cc | 1.90 g/cc | |
Parker Chomerics CHO-BOND 2166 Part B Silicone Information provided by Chomerics |