Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 2173HU Toyota High Impact Copolymer Polypropylene DescriptionPolyfort® PP 2173HU Toyota is a high flow, UV stabilized, high impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 2173HU Toyota High Impact Copolymer Polypropylene DescriptionPolyfort® PP 2173HU Toyota is a high flow, UV stabilized, high impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 7001 Information provided by A. Schulman. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ISO 1183 |
Total PPC 12642 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 12642 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 70 g/10 min and good mechanical properties.Polypropylene PPC 10641 has been developed for high s.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ISO 1183 |
Total PPC 3666 Polypropylene, Heterophasic Copolymer, Extrusion Polypropylene PPC 3666 is a heterophasic copolymer with a Melt Flow index of 1.5 g/10 min. This resin offers an outstanding processability in combination with good melt strength and excellent mecha.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D1505 |
Total PPC 5720WZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 5720WZ is a nucleated impact copolymer with a Melt Flow index of 20 g/10 min.TOTAL Polypropylene 5720WZ is characterized by good stiffness, creep resistance, very .. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ISO 1183 |
Total PPC 9612 Polypropylene, Heterophasic Copolymer, Injection Molding This product is a Total Ecosolutions grade.Polypropylene PPC 9612 has been developed specifically for the injection molding of crates and is characterized by a high Melt Flow index of 20 g/10 min. .. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ISO 1183 |
Total PPH 11012 Polypropylene Homopolymer, Injection Molding Polypropylene PPH 11012 is a nucleated controlled-rheology antistatic homopolymer with a high melt flow index of 55 g/10 min.Polypropylene PPH 11012 is characterized by high fluidity for high speed .. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D1505 |
Total PPH 3575CC Polypropylene Homopolymer, Film Grade Low Residuals TOTAL Polypropylene 3575CC utilizes the new TOTAL Polypropylene proprietary process technology to provide extremely low residuals for improved color stability and clarity.Slip/Antiblo.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D1505 |
Total PPH 3866 Polypropylene, Controlled Rheology Grade Homopolymer for Spunbond Nonwoven Fabrics, Multifilament Yarns, and Extrusion Coating Process Stability TOTAL Petrochemicals Polypropylene 3866 features excellent processability and gas fade resistance.FDA. 3866 complies with all applicable FDA regulations for food contact applicat.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ISO 1183 |
Total PPH 4026 Polypropylene Homopolymer, Sheet Extrusion and Thermoforming This grade belongs to the Total Ecosolution line.Polypropylene PPH 4026 is a polypropylene homopolymer specifically developed to offer outstanding processability for sheet extrusion and thermoformin.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ISO 1183 |
Total PPH 4069 Polypropylene Homopolymer, Fiber Polypropylene PPH 4069 is a homopolymer polypropylene with a Melt Flow index of 4 g/10 min.Polypropylene PPH 4069 is intended for extrusion of high tenacity staple fibers for non-woven applications... |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ISO 1183 |
Total PPH 4070 Polypropylene Homopolymer Polypropylene PPH 4070 is a homopolymer polypropylene with a Melt Flow index of 3 g/10 min.Polypropylene PPH 4070 has been designed for the production of BOPP film with the tenter frame process and .. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ISO 1183 |
Total PPH 6080 Polypropylene Homopolymer, Cast Film Polypropylene PPH 6080 is a homopolymer polypropylene with a Melt Flow index of 9 g/10 min for the cast extrusion of film with excellent optical properties and good sterilizability.Polypropylene PPH.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ISO 1183 |
Total PPM H350 Polypropylene, Homopolymer Medical Grade Polypropylene PPM H350 is a homopolymer with a Melt Flow Index of 35 g/10 min recommended for the manufacture of medical packaging and medical devices, to the exclusion of implants.Polypropylene PPM.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ISO 1183 |
Total PPS 15080 S01 Polypropylene, Homopolymer Fiber Grade Polypropylene PPS 15080 S01 is a high melt flow rate homopolymer with a very narrow molecular weight distribution.Polypropylene PPS 15080 S01 is intended for the extrusion of fine fibers with the me.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman PP 2175 Polypropylene High Flow Copolymer Polypropylene DescriptionPolypropylene PP 2175 is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman PP 3491 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3491 is a low water carry over homopolymer polypropylene, designed for high speed extrusion.Information provided by A. Schulman. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman PP 3491 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3491 is a low water carry over homopolymer polypropylene, designed for high speed extrusion.Information provided by A. Schulman. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ISO 1183 |
Total PPC 11812 S01 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 11812 S01 has been developed for high speed injection molding of thin walled packaging containers requiring top level impact resistance at cold temperature (-20°C). It is charact.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ISO 1183 |
Total PPC 1640 Polypropylene, Heterophasic Copolymer, Non-pressure Pipes Polypropylene PPC 1640 is a nucleated heterophasic (block) copolymer with a Melt Flow index of 0.3 g/10 min. This resin has a long-term heat stabilization package. It exhibits high stiffness in co.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D1505 |
Total PPC 4720XWZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 4720XWZ is a nucleated impact copolymer with a Melt Flow index of 25 g/10 min.TOTAL Polypropylene 4720XWZ is characterized by improved stiffness, creep resistance,.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D1505 |
Total PPC 4820WZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 4820WZ is a nucleated impact copolymer with a Melt Flow index of 35 g/10 min.TOTAL Polypropylene 4820WZ is characterized by improved stiffness, creep resistance, h.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 2173HU Toyota High Impact Copolymer Polypropylene DescriptionPolyfort® PP 2173HU Toyota is a high flow, UV stabilized, high impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 2175HU-31 High Flow Copolymer Polypropylene DescriptionPolyfort® PP 2175HU-31 is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | 60°F |
ConocoPhillips 680 Bearing Oil Description: Conoco Bearing Oil is formulated for the circulating systems that lubricate roll-neck bearings in steel and nonferrous rolling mills. It is suited for systems in which water and corrosi.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
Braskem H 155 Fiber Extrusion Polypropylene Homopolymer Meltblown nonwoven applications for hygienic, medical and hospital disposable devices; Filters and oil adsorbents.Information provided by Braskem. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
Braskem H 216 Fiber Extrusion Polypropylene Homopolymer Staple fibers and continuous filaments with high tenacity and fine denier; Fibers for asbestos-free roof tiles and concrete reinforcement.Information provided by Braskem. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D1505 |
Total PPC 4170 Polypropylene, Impact Copolymer, Blown Film Grade TOTAL Petrochemicals Polypropylene 4170 is a polypropylene impact copolymer grade with good melt strength for use in the extrusion of blown films.Benefits. 4170 forms tough films with high dart imp.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 3045 Information provided by A. Schulman. |