Total PPH 3575CC Polypropylene Homopolymer, Film Grade

Category Polymer , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Total Atofina
Trade Name PPH
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPH 3575CC Polypropylene Homopolymer, Film Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Low Residuals TOTAL Polypropylene 3575CC utilizes the new TOTAL Polypropylene proprietary process technology to provide extremely low residuals for improved color stability and clarity.Slip/Antiblock. 3575CC contains an optimized level of slip and antiblock additives.FDA. 3575CC complies with all applicable FDA regulations for food contact applications.Recommended Applications. TOTAL Polypropylene 3575CC is recommended for use in non-oriented cast film processes for manufacture of packaging films.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.905 g/cc
0.905 g/cc
ASTM D1505
Water Vapor Transmission 10.9 g/m²/day

@Temperature 37.8 °C
0.700 g/100 in²/day

@Temperature 100 °F
90% RH; ASTM F1249-90
Melt Flow 9.0 g/10 min

@Temperature 230 °C
9.0 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 48.3 MPa
7000 psi
ASTM D882
Elongation at Break 600 %
600 %
ASTM D882
Secant Modulus 0.483 GPa
70.0 ksi
0.01; ASTM D882
Dart Drop 0.787 g/micron
20.0 g/mil
F50; ASTM D1709
Thermal Properties Metric English Comments
Melting Point 163 °C
325 °F
DSC
Optical Properties Metric English Comments
Haze 2.5 %
2.5 %
ASTM D1003
Gloss 80 %
80 %
at 45°; ASTM D2457
Processing Properties Metric English Comments
Melt Temperature 204 - 260 °C
400 - 500 °F
Film Extrusion